Using Particle Packing and Statistical Approach to Optimize Eco-Efficient Ultra-High-Performance Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Using Particle Packing and Statistical Approach to Optimize Eco-Efficient Ultra-High-Performance Concrete

Author(s): Nancy A. Soliman and Arezki Tagnit-Hamou

Publication: Materials Journal

Volume: 114

Issue: 6

Appears on pages(s): 847-858

Keywords: design; packing density; statistical design approach; ultra-high-performance concrete (UHPC)

DOI: 10.14359/51701001

Date: 11/1/2017

Abstract:
Ultra-high-performance concrete (UHPC) is characterized by a dense microstructure that yields ultra-high strength and durability properties. This paper presents an innovative method to produce eco-efficient mixtures of UHPC using locally available materials based on optimization using the packing density and a statistical mixture design approach. The results showed an optimal packing density of 0.79% for a combination of all granular materials (quartz sand, quartz powder, cement, and silica fume). The study presents experimentally based models with high coefficients of correlation in predicting the workability and strength of UHPC as a function of mixture design parameters (water-binder ratio [w/b] and highrange water-reducing admixture [HRWRA] dosage). Contour diagrams to facilitate the use of the models were established. In this research, UHPC mixtures with a slump flow between 130 and 300 mm (5.1 and 11.8 in.) and compressive strength between 135 and 225 MPa (19.6 and 32.6 ksi) were produced; such concretes are required for different industrial applications.

Related References:

1. Gupta, P. R., and Shiu, K. N., “Effective Repair and Maintenance Strategies for Parking Structures,” Concrete Repair Bulletin, V. 27, No. 4, July-Aug. 2014, pp. 30-34.

2. U.S. Department of Homeland Security (DHS) Science and Technology, “UHPC Ultra-High Performance Concrete,” Technical Report, Washington, DC, 23 pp, https://www.dhs.gov/xlibrary/assets/uhpc-pathway-to-commercialization.pdf. (last accessed Nov. 3, 2017)

3. Richard, P., and Cheyrezy, M., “Reactive Powder Concretes with High Ductility and 200-800 MPa Compressive Strength,” Concrete Technology: Paste, Present, & Future, SP-144, P. K. Mehta, ed., American Concrete Institute, Farmington Hills, MI, 1994, pp. 507-518.

4. Richard, P., and Cheyrezy, M., “Composition of Reactive Powder Concretes,” Cement and Concrete Research, V. 25, No. 7, 1995, pp. 1501-1511. doi: 10.1016/0008-8846(95)00144-2

5. Dugat, J.; Roux, N.; and Bernier, G., “Mechanical Properties of Reactive Powder Concretes,” Materials and Structures, V. 29, No. 4, 1996, pp. 233-240. doi: 10.1007/BF02485945

6. Roux, N.; Andrade, C.; and Sanjuan, M., “Experimental Study of Durability of Reactive Powder Concretes,” Journal of Materials in Civil Engineering, ASCE, V. 8, No. 1, 1996, pp. 1-6. doi: 10.1061/(ASCE)0899-1561(1996)8:1(1)

7. Bonneau, O.; Lachemi, M.; Dallaire, E.; Dugat, J.; and Aïtcin, P.-C., “Mechanical Properties and Durability of Two Industrial Reactive Powder Concretes,” ACI Materials Journal, V. 94, No. 4, July-Aug. 1997, pp. 286-290.

8. Schmidt, M., and Fehling, E., “Ultra-High-Performance Concrete: Research, Development and Application in Europe,” Serviceability of Concrete: A Symposium Honoring Dr. Edward G. Nawy, SP-225, R. Frosch, H. Nassif, and A. Scanlon, eds., American Concrete Institute, Farmington Hills, MI, 2005, pp. 51-77.

9. Aïtcin, P.-C.; Lachemi, M.; Adeline, R.; and Richard, P., “The Sherbrooke Reactive Powder Concrete Footbridge,” Structural Engineering International, V. 8, No. 2, 1998, pp. 140-144. doi: 10.2749/101686698780489243

10. Klemens, T., “Flexible Concrete Offers New Solutions,” Concrete Construction, V. 49, No. 12, 2004, p. 72.

11. Racky, P., “Cost-Effectiveness and Sustainability of UHPC,” Proceedings of the International Symposium on UHPC, Kassel, Germany, 2004, pp. 797-805.

12. Aïtcin, P.-C., “Cements of Yesterday and Today—Concrete of Tomorrow,” Cement and Concrete Research, V. 30, No. 9, 2000, pp. 1349-1359. doi: 10.1016/S0008-8846(00)00365-3

13. Graybeal, B. A., “Material Property Characterization of Ultra-High Performance Concrete,” Publication No. FHWA-HRT-06-103, Federal Highway Administration, Washington, DC, 2006.

14. de Larrard, F., and Sedran, T., “Optimization of Ultra-High-Performance Concrete by the Use of a Packing Model,” Cement and Concrete Research, V. 24, No. 6, 1994, pp. 997-1009. doi: 10.1016/0008-8846(94)90022-1

15. de Larrard, F., Concrete Mixture Proportioning: A Scientific Approach, E&FN Spon, London, UK, 1999.

16. Teichmann, T., and Schmidt, M., “Influence of the Packing Density of Fine Particles on Structure, Strength and Durability of UHPC,” International Symposium on UHPC, Kassel, Germany, 2004.

17. Talebinejad, I.; Bassam, S. A.; Iranmanesh, A.; and Shekarchizadeh, M., “Optimizing Mix Proportions of Normal Weight Reactive Powder Concrete with Strengths of 200-350 MPa,” International Symposium on UHPC, Kassel, Germany, 2004.

18. Habel, K.; Charron, J.-P.; Braike, S.; Hooton, R. D.; Gauvreau, P.; and Massicotte, B., “Ultra-High Performance Fiber Reinforced Concrete Mix Design in Central Canada,” Canadian Journal of Civil Engineering, V. 35, No. 2, 2008, pp. 217-224. doi: 10.1139/L07-114

19. Rossi, P.; Arca, A.; Parant, E.; and Fakhri, P., “Bending and Compressive Behaviors of New Cement Composite,” Cement and Concrete Research, V. 35, No. 1, 2005, pp. 27-33. doi: 10.1016/j.cemconres.2004.05.043

20. Park, J.; Kang, S. T.; Taek, K. K.; and Wook, K. S., “Influence of the Ingredients on the Compressive Strength of UHPC as a Fundamental Study to Optimize the Mixing Proportion,” International Symposium on UHPC, Kassel, Germany, 2008, pp. 105-112.

21. Wille, K.; Naaman, A. E.; and Montesinos, G. J. P., “Ultra-High Performance Concrete with Compressive Strength Exceeding 150 MPa (22 ksi),” ACI Materials Journal, V. 108, No. 1, Jan.-Feb. 2011, pp. 46-54.

22. Wang, C.; Yang, C.; Liu, F.; Wan, C.; and Pu, X., “Preparation of Ultra-High Performance Concrete with Common Technology and Materials,” Cement and Concrete Composites, V. 34, No. 4, 2012, pp. 538-544. doi: 10.1016/j.cemconcomp.2011.11.005

23. Ghafari, E.; Costa, H.; and Julio, E., “Statistical Mixture Design Approach for Eco-Efficient UHPC,” Cement and Concrete Composites, V. 55, 2015, pp. 17-25. doi: 10.1016/j.cemconcomp.2014.07.016

24. Kumar, S. V., and Santhanam, M., “Particle Packing Theories and Their Application in Concrete Mixture Proportioning,” Indian Concrete Journal, V. 77, No. 9, 2003, pp. 1324-1331.

25. Powers, T. C., The Properties of Fresh Concrete, John Wiley and Sons, New York, 1968.

26. Fennis, S. A. A. M.; Walraven, J. C.; and Nijland, T., “Measuring the Packing Density to Lower the Cement Content in Concrete,” Tailor Made Concrete Structures: New Solutions for Our Society, J. C. Walraven and D. Stoelhorst, eds., Taylor and Francis Group, London, UK, 2008, pp. 419-424.

27. Lange, F.; Mörtel, H.; and Rudert, V., “Dense Packing of Cement Pastes and Resulting Consequences on Mortar Properties,” Cement and Concrete Research, V. 27, No. 10, 1997, pp. 1481-1488. doi: 10.1016/S0008-8846(97)00189-0

28. Neville, A. M., Properties of Concrete, Longman, Harlow, UK, 1995.

29. Fuller, W. B., and Thompson, S. E., “The Laws of Proportioning Concrete,” Transactions of the American Society of Civil Engineers, V. 59, No. 2, 1907, pp. 67-143.

30. Funk, J. E., and Dinger, D. R., Predictive Process Control of Crowded Particulate Suspensions Applied to Ceramic Manufacturing, Kluwer Academic Publishers, Boston, MA, 1994.

31. Stroeven, P., and Stroeven, M., “Assessment of Packing Characteristics by Computer Simulation,” Cement and Concrete Research, V. 29, No. 8, 1999, pp. 1201-1206. doi: 10.1016/S0008-8846(99)00020-4

32. Kolonko, M.; Raschdorf, S.; and Wasch, D., “A Hierarchical Approach to Estimate the Space Filling of Particle Mixtures with Broad Size Distributions,” Bio-resourse, V. 9, No. 3, 2008, p. 28.

33. Fennis-Huijben, S. A. A. M., “Design of Ecological Concrete by Particle Packing Optimization,” PhD disseration, Delft University of Technology, Delft, the Netherlands, 2010, 277 pp.

34. Dewar, J. D., Computer Modelling of Concrete Mixtures, E&FN Spon, London, UK, 1999.

35. Montgomery, D. C., Design and Analysis of Experiments, sixth edition, John Wiley & Sons, New York, 2005.

36. Omran, A. F.; Khayat, K. H.; and Elaguab, Y. M., “Effect of SCC Mixture Composition on Thixotropy and Formwork Pressure,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 7, 2012, pp. 876-888. doi: 10.1061/(ASCE)MT.1943-5533.0000463

37. Mueller, F. V.; Wallevik, O. H.; and Khayat, K. H., “Linking Solid Particle Packing of Eco-SCC to Material Performance,” Cement and Concrete Composites, V. 54, 2014, pp. 117-125. doi: 10.1016/j.cemconcomp.2014.04.001

38. Bigas, J. P., and Gallias, J. L., “Effect of Fine Mineral Additions on Granular Packing of Cement Mixtures,” Magazine of Concrete Research, V. 54, No. 3, 2002, pp. 155-164. doi: 10.1680/macr.2002.54.3.155

39. Johansen, V., and Andersen, P. J., “Particle Packing and Concrete Properties,” Material Science of Concrete 2, J. Skalny and S. Mindess, eds., American Ceramic Society, Westerville, OH, 1991.

40. Marland, G.; and Boden, T., “Global CO2 Emissions from Fossil-Fuel Burning, Cement Manufacture, and Gas Flaring,” Carbon Dioxide Information Analysis Center, Oak Ridge National Laboratory, Oak Ridge, TN, 2003, pp. 1751-2000.

41. Herold, G., and Müller, H. S., “Measurement of Porosity of Ultra High Strength Fibre Reinforced Concrete,” Proceedings of the International Symposium on UHPC, Kassel, Germany, Sept. 13-15, 2004, pp. 685-694.

42. Ghafari, E.; Costa, H.; Júlio, E.; Portugal, A.; and Durães, L., “The Effect of Nanosilica Addition on Flowability, Strength and Transport Properties of Ultra-High Performance Concrete,” Materials & Design, V. 59, 2014, pp. 1-9. doi: 10.1016/j.matdes.2014.02.051

43. Soutsos, M. N.; Millar, S. G.; and Karaiskos, K., “Mix Design, Mechanical Properties, and Impact Resistance of Reactive Powder Concrete (RPC),” International RILEM Workshop on High Performance Fiber Reinforced Cementitious Composites in Structural Applications, Honolulu, HI, May 2005.

44. Habel, K.; Viviani, M.; Denarié, E.; and Brühwiler, E., “Development of the Mechanical Properties of an Ultra-High Performance Fiber Reinforced Concrete (UHPFRC),” Cement and Concrete Research, V. 36, No. 7, 2006, pp. 1362-1370. doi: 10.1016/j.cemconres.2006.03.009

45. Corinaldesi, V., and Moriconi, G., “Mechanical and Thermal Evaluation of Ultra High Performance Fiber Reinforced Concretes for Engineering Applications,” Construction and Building Materials, V. 26, No. 1, 2012, pp. 289-294. doi: 10.1016/j.conbuildmat.2011.06.023


ALSO AVAILABLE IN:

Electronic Materials Journal