Title: Long-Term Multipliers and Deformability of Fiber-Reinforced Polymer Prestressed Concrete

Author(s): Yail J. Kim and Raymon W. Nickle

Publication: Structural Journal

Volume: 115

Issue: 1

Appears on pages(s): 223-234

Keywords: bridge; deformability; fiber-reinforced polymer (FRP); longterm multiplier; minimum reinforcement; prestress

DOI: 10.14359/51700988

Date: 1/1/2018

Abstract:
This paper presents the flexural characteristics of highway bridge girders prestressed with fiber-reinforced polymer (FRP) tendons. Of interest are the technical challenges identified by ACI Subcommittee 440-I (FRP-Prestressed Concrete): long-term multipliers, deformability, and minimum reinforcement. Aramid and carbon FRP (AFRP and CFRP, respectively) composites are used to prestress concrete girders. Based on analytical models, new design expressions are proposed for the aforementioned items, followed by an assessment using laboratory test data and full-scale benchmark bridges. The long-term multipliers calibrated per reliability theory are mostly different from the empirical multipliers adopted in ACI 440.4R-04. The girders prestressed with AFRP/CFRP sufficiently deform in flexure, even though their moment-curvature responses are not comparable with those of steel-prestressed girders. The new deformability index specifies design requirements for AFRP/CFRP-prestressed members with either compression-controlled or tensioned-controlled sections. The importance of a potential change in FRP modulus during the service life of prestressed concrete girders is examined. A factored ultimate-tocracking moment ratio of ϕMn/Mcr = 1.2 is suggested for girders prestressed with AFRP/CFRP, which aligns with the articles of existing design manuals and specifications dedicated to prestressed concrete.

Related References:

1. Abdelrahman, A. A.; Tadros, G.; and Rizkalla, S. H., “Test Model for the First Canadian Smart Highway Bridge,” ACI Structural Journal, V. 92, No. 4, July-Aug. 1995, pp. 451-458.

2. Fam, A. Z.; Rizkalla, S. H.; and Tadros, G., “Behavior of CFRP for Prestressing and Shear Reinforcements of Concrete Highway Bridges,” ACI Structural Journal, V. 94, No. 1, Jan.-Feb. 1997, pp. 77-86.

3. ACI Committee 440, “Prestressing Concrete Structures with FRP Tendons (ACI 440.4R-04),” American Concrete Institute, Farmington Hills, MI, 2004, 35 pp.

4. Youakim, S. A., and Karbhari, V. M., “An Approach to Determine Long-Term Behavior of Concrete Members Prestressed with FRP Tendons,” Construction and Building Materials, V. 21, No. 5, 2007, pp. 1052-1060. doi: 10.1016/j.conbuildmat.2006.02.006

5. Nanni, A., and Tanigaki, M., “Pretensionded Prestressed Concrete Members with Bonded Fiber Reinforced Plastic Tendons: Development and Flexural Bond Lengths (Static),” ACI Structural Journal, V. 89, No. 4, July-Aug. 1992, pp. 433-441.

6. Grace, N. F., and Abdel-Sayed, G., “Behavior of Carbon Fiber-Reinforced Prestressed Concrete Skew Bridges,” ACI Structural Journal, V. 97, No. 1, Jan.-Feb. 2000, pp. 26-35.

7. Dolan, C. W., and Swanson, D., “Development of Flexural Capacity of an FRP Prestressed Beam with Vertically Distributed Tendons,” Composites. Part B, Engineering, V. 33, No. 1, 2002, pp. 1-6. doi: 10.1016/S1359-8368(01)00053-1

8. Saiedi, R.; Fam, A.; and Green, M. F., “Behavior of CFRP-Prestressed Concrete Beams under High-Cycle Fatigue at Low Temperature,” Journal of Composites for Construction, ASCE, V. 15, No. 4, 2011, pp. 482-489. doi: 10.1061/(ASCE)CC.1943-5614.0000190

9. Zhang, K.; Fang, Z.; and Nanni, A., “Behavior of Tendons with Multiple CFRP Rods,” Journal of Structural Engineering, ASCE, V. 142, No. 10, 2016, p. 04016065. doi: 10.1061/(ASCE)ST.1943-541X.0001535

10. Soudki, K. A., “FRP Reinforcement for Prestressed Concrete Structures,” Progress in Structural Engineering and Materials, V. 1, No. 2, 1998, pp. 135-142. doi: 10.1002/pse.2260010205

11. Lees, J. M., “Fibre-Reinforced Polymers in Reinforced and Prestressed Concrete Applications: Moving Forward,” Progress in Structural Engineering and Materials, V. 3, No. 2, 2001, pp. 122-131. doi: 10.1002/pse.60

12. Martin, L. D., “A Rational Method for Estimating Camber and Deflection of Precast Prestressed Members,” PCI Journal, V. 22, No. 1, 1977, pp. 100-108.

13. Zou, P. X. W., “Flexural Behavior and Deformability of Fiber Reinforced Polymer Prestressed Concrete Beams,” Journal of Composites for Construction, ASCE, V. 7, No. 4, 2003, pp. 275-284. doi: 10.1061/(ASCE)1090-0268(2003)7:4(275)

14. Au, F. T. K., and Du, J. S., “Deformability of Concrete Beams with Unbonded FRP Tendons,” Engineering Structures, V. 30, No. 12, 2008, pp. 3764-3770. doi: 10.1016/j.engstruct.2008.07.003

15. AASHTO, “AASHTO LRFD Bridge Design Specifications,” seventh edition with interim revisions, American Association of State Highway and Transportation Officials, Washington, DC, 2016.

16. Kim, Y. J., and Nickle, R. W., “Strength Reduction Factors for Fiber-Reinforced Polymer Prestressed Concrete Bridges in Flexure,” ACI Structural Journal, V. 113, No. 5, Sept.-Oct. 2016, pp. 1043-1052. doi: 10.14359/51689028

17. ACI Committee 318, “Building Code Requirements for Reinforced Concrete (ACI 318-71),” American Concrete Institute, Farmington Hills, MI, 1971, 78 pp.

18. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

19. ACI Committee 209, “Prediction of Creep, Shrinkage, and Temperature Effects in Concrete Structures,” Designing for Effects of Creep, Shrinkage and Temperature in Concrete Structures, SP-27, American Concrete Institute, Farmington Hills, MI, 1971, pp. 51-93.

20. Skogman, B. C.; Tadros, M. K.; and Grasmick, R., “Ductility of Reinforced and Prestressed Concrete Flexural Members,” PCI Journal, V. 33, No. 6, 1988, pp. 94-107. doi: 10.15554/pcij.11011988.94.107

21. PCI, PCI Bridge Design Manual, Precast/Prestressed Concrete Institute, Chicago, IL, 2003.

22. Karbhari, V. M., “Durability Data for FRP Rehabilitation Systems,” Report No. CA09-0248, California Department of Transportation, Sacramento, CA, 2009.

23. Lees, J. M.; Toumpanaki, E.; Barbezat, M.; and Terrasi, G. P., “Mechanical and Durability Screening Test Methods for Cylindrical CFRP Prestressing Tendons,” Journal of Composites for Construction, ASCE, V. 21, No. 2, 2017, p. 04016080 doi: 10.1061/(ASCE)CC.1943-5614.0000727

24. Guedes, R. M., “Time-Dependent Failure Criteria for Polymer Matrix Composites: A Review,” Journal of Reinforced Plastics and Composites, V. 29, No. 20, 2010, pp. 3041-3047. doi: 10.1177/0731684410370067

25. PCI, PCI Design Handbook, seventh edition, Precast/Prestressed Concrete Institute, Chicago, IL, 2010.

26. Kwon, O.-S.; Kim, E.; Orton, S.; Salim, H.; and Hazlett, T., “Calibration of the Live Load Factor in LRFD Design Guidelines,” Final Report No. OR11-003, Missouri Department of Transportation, Jefferson City, MO, 2011.

27. Atadero, R. A., and Karbhari, V. M., “Calibration of Resistance Factors for Reliability-Based Design of Externally-Bonded FRP Composites,” Composites. Part B, Engineering, V. 39, No. 4, 2008, pp. 665-679. doi: 10.1016/j.compositesb.2007.06.004

28. Sanchez-Heres, L. F.; Ringsberg, J. W.; and Johnson, E., “Influence of Mechanical and Probabilistic Models on the Reliability Estimates of Fibre-Reinforced Cross-Ply Laminates,” Structural Safety, V. 51, 2014, pp. 35-46. doi: 10.1016/j.strusafe.2014.06.001

29. Okeil, A.; El-Tawil, S.; and Shahawy, M., “Flexural Reliability of Reinforced Concrete Bridge Girders Strengthened with Carbon Fiber-Reinforced Polymer Laminates,” Journal of Bridge Engineering, ASCE, V. 7, No. 5, 2002, pp. 290-299. doi: 10.1061/(ASCE)1084-0702(2002)7:5(290)

30. Grace, N. F., and Singh, S. B., “Design Approach for Carbon Fiber-Reinforced Polymer Prestressed Concrete Bridge Beams,” ACI Structural Journal, V. 100, No. 3, May-June 2003, pp. 365-376.

31. Stoll, F.; Saliba, J. E.; and Casper, L. E., “Experimental Study of CFRP-Prestressed High-Strength Concrete Bridge Beams,” Composite Structures, V. 49, 2000, pp. 191-200. doi: 10.1016/S0263-8223(99)00134-8

32. Toutanji, H., and Saafi, M., “Performance of Concrete Beams Prestressed with Aramid Fiber-Reinforced Polymer Tendons,” Composite Structures, V. 44, No. 1, 1999, pp. 63-70. doi: 10.1016/S0263-8223(98)00126-3

33. McKay, K. S., and Erki, M. A., “Flexural Behaviour of Concrete Beams Pretensioned with Aramid Fibre Reinforced Plastic Tendons,” Canadian Journal of Civil Engineering, V. 20, No. 4, 1993, pp. 688-695. doi: 10.1139/l93-085

34. Niitani, K.; Tezuka, M.; and Tamura, T., “Flexural Behavior of Prestressed Concrete Beams Using AFRP Pre-Tensioning Tendons,” Proceedings of the 3rd International Symposium on Non-Metallic (FRP) Reinforcement for Concrete Structures, 1997, pp. 663-670.

35. Taerwe, L., and Matthys, S., “Structural Behavior of Concrete Slabs Prestressed with AFRP Bars,” Proceedings of the 2nd International Symposium on Non-Metallic (FRP) Reinforcement for Concrete Structures, 1995, pp. 421-429.


ALSO AVAILABLE IN:

Electronic Structural Journal