Ionically Conductive Mortar for Electrical Heating

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ionically Conductive Mortar for Electrical Heating

Author(s): Ruohong Zhao, Christopher Y. Tuan, Daobo Fan, An Xu, and Bao Luo

Publication: Materials Journal

Volume: 114

Issue: 6

Appears on pages(s): 923-933

Keywords: electrical conductive concrete; ice and snow melting; ionic conduction; radiant heating

DOI: 10.14359/51700897

Date: 11/1/2017

Abstract:
An innovative conductive composite, ionically conductive mortar, is developed in this study. The directional migration of ions under external voltage makes the mortar conductive. The electrical resistance of the mortar causes the mortar to generate heat, which is used for deicing. To ensure conductivity, the number of free ions and the moisture content in the mortar must stay relatively high. The specimens were soaked in electrolyte solutions for 96 hours to saturation and coated with epoxy resin. Subsequent electrical heating tests showed that the specimens could achieve a heating rate of 19.7°C (35.5°F) in 120 minutes under 30 V AC. This heating performance would improve with increasing applied voltage.

Related References:

1. Mu, X. Y., “Electrothermal Test of Carbon Black Cement Mortar Slabs and Analysis of Heat Transfer,” Wuhan University of Technology, Wuhan, China, 2008, pp. 5-6.

2. Lu, Z. H., and Fu, H. L., “Performance Research on Carbon Fibre-Slag Electrically Conductive Concrete,” Advanced Materials Research, V. 512-515, 2012, pp. 2891-2894. doi: 10.4028/www.scientific.net/AMR.512-515.2891

3. Tuan, C. Y., “Roca Spur Bridge: The Implementation of an Innovative Deicing Technology,” Journal of Cold Regions Engineering, ASCCE, V. 22, No. 1, 2008, pp. 1-15. doi: 10.1061/(ASCE)0887-381X(2008)22:1(1)

4. Zuo, Z.; Yang, J.; Hu, Y.; and Wang, Y., “Numerical Computing Method of Conductive Concrete Applied in Construction Heating Engineering,” Journal of Civil, Architectural & Environmental Engineering, V. 35, No. 4, 2013, pp. 139-144.

5. Sun, M. Q.; Liu, Q. P.; Li, Z. Q.; and Hu, Y., “A Study of Piezoelectric Properties of Carbon Fiber Reinforced Concrete Plain Cement Paste during Dynamic Loading,” Cement and Concrete Research, V. 30, No. 10, 2000, pp. 1593-1595. doi: 10.1016/S0008-8846(00)00338-0

6. Yehia, S.; Qaddoumi, N.; Hassan, M.; and Swaked, B., “Conductive Concrete for Electromagnetic Shielding Applications,” Advances in Civil Engineering Materials, V. 3, No. 1, 2014, pp. 270-290. doi: 10.1520/ACEM20130107

7. Zhao, H. M.; Wu, Z. M.; Wang, S. G.; Zheng, J.; and Che, G., “Concrete Pavement Deicing with Carbon Fiber Heating Wires,” Cold Regions Science and Technology, V. 65, No. 3, 2011, pp. 413-420. doi: 10.1016/j.coldregions.2010.10.010

8. Wu, J. M.; Liu, J. G.; and Yang, F., “Three-Phase Composite Conductive Concrete for Pavement Deicing,” Construction and Building Materials, V. 75, 2015, pp. 129-135. doi: 10.1016/j.conbuildmat.2014.11.004

9. Ding, Y.; Chen, Z. P.; Han, Z. B.; Zhang, Y.; and Pacheco-Torgal, F., “Nano-Carbon Black and Carbon Fiber as Conductive Materials for the Diagnosing of the Damage of Concrete Beam,” Construction and Building Materials, V. 43, 2013, pp. 233-241. doi: 10.1016/j.conbuildmat.2013.02.010

10. Pérez, A.; Climent, M. A.; and Garces, P., “Electrochemical Extraction of Chlorides from Reinforced Concrete Using a Conductive Cement Paste as the Anode,” Corrosion Science, V. 52, No. 5, 2010, pp. 1576-1581. doi: 10.1016/j.corsci.2010.01.016

11. Hou, Z. F.; Li, Z. Q.; and Wang, J. J., “Electrically Conductive Concrete for Heating Using Steel Bars as Electrodes,” Journal of Wuhan University of Technology, V. 25, No. 3, 2010, pp. 523-526. doi: (Materials Science Edition)10.1007/s11595-010-0035-x

12. Chung, D. D. L., “Cement-Matrix Composites for Thermal Engineering,” Applied Thermal Engineering, V. 21, No. 16, 2001, pp. 1607-1619. doi: 10.1016/S1359-4311(01)00043-6

13. Yehia, S. A., and Tuan, C. Y., “An Implementation of Using a Conductive Concrete Overlay for Bridge Deck Deicing at Roca,” Transportation Research Circular E-C063: Snow Removal and Ice Control Technology, University of Nebraska, Omaha, Omaha, NE, 2004, pp. 58-60.

14. Reza, F.; Batson, G. B.; and Yamamuro, J. A., “Volume Electrical Resistivity of Carbon Fiber Cement Composites,” ACI Materials Journal, V. 98, No. 1, Jan.-Feb. 2001, pp. 25-35.

15. Whittington, H. W.; McCarter, J.; and Forde, M. C., “The Conduction of Electricity through Concrete,” Magazine of Concrete Research, V. 33, No. 114, 1981, pp. 48-60. doi: 10.1680/macr.1981.33.114.48

16. McGrath, P. F., and Hooton, R. D., “Influence of Voltage on Chloride Diffusion Coefficients from Chloride Migration Tests,” Cement and Concrete Research, V. 26, No. 8, 1996, pp. 1239-1244. doi: 10.1016/0008-8846(96)00094-4

17. Lay, S.; Liebl, S.; Hilbig, H.; and Schießl, P., “New Method to Measure the Rapid Chloride Migration Coefficient of Chloride-Contaminated Concrete,” Cement and Concrete Research, V. 34, No. 3, 2004, pp. 421-427. doi: 10.1016/j.cemconres.2003.08.022

18. Spiesz, P., and Brouwers, H. J. H., “Influence of the Applied Voltage on the Rapid Chloride Migration (RCM) Test,” Cement and Concrete Research, V. 42, No. 8, 2012, pp. 1072-1082. doi: 10.1016/j.cemconres.2012.04.007

19. ASTM C1202-12, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2012, 8 pp.

20. Wu, X. M., and Fan, Y. M., “Structure and Performance of Steam-cured Fly-ash Aerated Concrete with Light Weight Aggregate,” Journal of South China University of Technology, V. 31, No. 9, 2003, pp. 57-61.

21. “Method of Testing Cements—Determination of Strength (ISO 679:1989),” National Standard Publishing House, 1999, pp. 4-5.

22. “Standard for Test Method of Performance on Building Mortar (JGJ/T70-2009),” National Standard Publishing House, 2009, pp 10-18.

23. Cook, R. A., and Hover, K. C., “Mercury Porosity of Hardened Cement Pastes,” Cement and Concrete Research, V. 29, No. 6, 1999, pp. 933-943. doi: 10.1016/S0008-8846(99)00083-6

24. Fan, D. B.; Zhao, R. H.; and Xu, A. et al., “Optimization Research on Manufacture of Ion Conductive Mortar Based on Penetration Test,” China Concrete and Cement Products, V. 10, 2016, pp. 9-13.

25. Neville, A. M., Properties of Concrete, Building Industry Press, Beijing, China, 2008, pp. 23-25.

26. He, Z. M.; Long, G. C.; and Xie, Y. J., “Influence of Subsequent Curing on Water Sorptivity and Pore Structure of Steam-Cured Concrete,” Journal of Central South University, V. 19, No. 4, 2012, pp. 1155-1162. doi: 10.1007/s11771-012-1122-2

27. Li, D., Electrochemical Principle, Beijing University of Aeronautics and Astronautics Press, Beijing, China, 2008, pp.1-11.

28. He, Z. X.; Shi, C. J.; Hu, X.; and Zhang, J., “Development on Migration Characteristic and Interactions of Chloride Ion in Cement-Based Materials under Applied Voltages,” Journal of the Chinese Ceramic Society, V. 43, No. 8, 2015, pp. 1111-1119.

29. Heymsfield, E.; Osweiler, A.; Selvam, P.; and Kuss, M., “Developing Anti-icing Airfield Runways Using Conductive Concrete with Renewable Energy,” Journal of Cold Regions Engineering, ASCE, V. 28, No. 2, 2014, pp. 979-986. doi: 10.1061/(ASCE)CR.1943-5495.0000064

30. Xiao-Chun, X. U.; Song, J. C.; and Feng, J. Y., “Development of Steel Slag-Carbon Fiber Heating Concrete Floor,” Concrete (London), No. 2, 2008, pp. 122-124.


ALSO AVAILABLE IN:

Electronic Materials Journal