Title: Closure Strip Strategies

Author(s): Andre Brault, Neil Hoult, Tom Greenough, Ian Trudeau, and Barry Charnish

Publication: Concrete International

Volume: 39

Issue: 7

Appears on pages(s): 29-35

Keywords: slab, shrinkage, model, displacement

DOI: 10.14359/51700883

Date: 7/1/2017

Abstract:
Closure strips are temporary gaps in reinforced concrete floor slabs. They are provided to allow sections on either side to undergo shrinkage independently; however, only limited guidance is available for their design. This article summarizes currently available design approaches, presents a case study of closure strip monitoring, and compares the obtained field data with predictions from the available design approaches.

Related References:

1. “Industry Data,” Bureau of Economic Analysis, Washington, DC, www.bea.gov/iTable/iTable.cfm?ReqID=51&step=1#reqid=51&step=51&isuri=1&5114=a&5102=1. (last accessed July 19, 2016)

2. Suprenant, B., “Shrinkage and Temperature Reinforcement,” Concrete International, V. 24, No. 9, Sept. 2002, pp. 72-76.

3. Eskildsen, S.; Jones, M.; and Richardson, J., “No More Pour Strips,” Concrete International, V. 31, No. 10, Oct. 2009, pp. 42-47.

4. Kim, H., and Cho, S., “Shrinkage Stress Analysis of Concrete Slabs with Shrinkage Strips in a Multistory Building,” Computers & Structures, V. 82, No. 15-16, June 2004, pp. 1143-1152.

5. Fintel, M., Handbook of Concrete Engineering, second edition, Van Nostrand Reinhold, New York, 1985, 892 pp.

6. “Detailing Corner: Closure Strips and Lapped Reinforcement,” Concrete International, V. 33, No. 4, Apr. 2011, pp. 49-53.

7. “Expansion Joints in Buildings,” Technical Report No. 65, Federal Construction Council, National Academy of Sciences National Research Council, Washington, DC, 1974, 52 pp.

8. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

9. ACI Committee 209, “Guide for Modeling and Calculating Shrinkage and Creep in Hardened Concrete (ACI 209.2R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 46 pp.

10. “Ottawa, ON: Monthly Calendar,” Weather Network, www.theweathernetwork.com/monthly/canada/ontario/ottawa?year=2014&month=10&dispt=calendar-container-monthly. (last accessed Nov. 30, 2014)

11. Faria, R.; Azenha, M.; and Figueiras, J., “Modelling of Concrete at Early Ages: Application to an Externally Restrained Slab,” Cement and Concrete Composites, V. 28, No 6, July 2006, pp. 572-585.

12. ACI Committee 209, “Prediction of Creep, Shrinkage, and Temperature Effects in Concrete Structures,” (ACI 209R-92) (Reapproved 2008),” American Concrete Institute, Farmington Hills, MI, 1992, 47 pp.

13. Computers & Structures, Inc., CSI Analysis Reference Manual, 2016, 534 pp.