Title: Magneto-Electric Active Control of Scaled-Down Reinforced Concrete Columns

Author(s): Omid Rezaifar, Iman Abavisani, and Ali Kheyroddin

Publication: Structural Journal

Volume: 114

Issue: 5

Appears on pages(s): 1351-1362

Keywords: alternating current (AC) electricity; alternating magnetic field (AMF); compressive strength; current intensity; real-time behavior controlling

DOI: 10.14359/51700790

Date: 9/1/2017

Abstract:
An exploratory investigation was conducted into the feasibility of improving compressive behavior of reinforced concrete (RC) columns and controlling their structural behavior in real time through interaction between alternating magnetic field (AMF) and alternating current (AC) electricity as actuating systems. For this purpose, some compression experiments were performed on scaled-down RC columns, where AMF of power 0.5 tesla (T) and with frequency of 50 Hz was externally applied to RC columns and/or AC of current intensities up to 36 ampere (A) was run through the reinforcing web. Hence, a specialized test setup comprising magnetic and electric circuits was devised, capable of applying AMF, AC, and uniaxial compression to the specimen simultaneously. For better understanding and discussion about the effect of AMF, some cube specimens of plain concrete (PC) were also prepared, magnetized, and tested. Then the test data for these specimens and those of RC columns were correlated. It was observed that exposing fresh RC column to AMF upon placement facilitates compaction of concrete through vibrating the reinforcing bars, besides a marginal effect on its compressive behavior in the solid phase. But applying AMF to a hardened RC column enhanced the compressive strength by more than 11%, while causing more brittle behavior. On the other hand, employing AC proved to reduce the RC column’s load-bearing capacity but improving ductility. Moreover, the load-bearing capacity and the strength degradation rate in the descending branch of the stress-strain curve of RC columns were experimentally derived as functions of current intensity. Finally, it was found this technique can be a base for real-time compressive behavior controlling of RC members and managing their failure mods through interaction between AMF and AC.

Related References:

1. Maalej, M.; Karasaridis, A.; Pantazopoulou, S.; and Hatzinakos, D., “Structural Health Monitoring of Smart Structures,” Smart Materials and Structures, V. 11, No. 4, July 2002, pp. 581-589.

2. Leung, C. K. Y.; Wan, K. T.; Inaudi, D.; Bao, X.; Habel, W.; Zhou, Z.; Ou, J.; Ghandehari, M.; Wu, H. C.; and Imai, M., “Review: Optical Fiber Sensors for Civil Engineering Applications,” Materials and Structures, V. 48, No. 4, Apr. 2015, pp. 871-906.

3. Uva, G.; Porco, F.; Fiore, A.; and Porco, G., “Structural Monitoring Using Fiber Optic Sensors of a Pre-Stressed Concrete Viaduct during Construction Phases,” Case Studies in Nondestructive Testing and Evaluation, V. 2, Oct. 2014, pp. 27-37.

4. Perry, M.; Yan, Z.; Sun, Z.; Zhang, L.; Niewczas, P.; and Johnston, M., “High Stress Monitoring of Prestressing Tendons in Nuclear Concrete Vessels Using Fibre-Optic Sensors,” Nuclear Engineering and Design, V. 268, Mar. 2014, pp. 35-40.

5. Karayannis, C. G.; Chalioris, C. E.; Angeli, G. M.; Papadopoulos, N. A.; Fawata, M. J.; and Providakis, C. P., “Experimental Damage Evaluation of Reinforced Concrete Steel Bars Using Piezoelectric Sensors,” Construction and Building Materials, V. 105, Feb. 2016, pp. 227-244.

6. Dong, B.; Liu, Y.; Qin, L.; Wang, Y.; Fang, Y.; Xing, F.; and Chen, X., “In Situ Stress Monitoring of the Concrete Beam under Static Loading with Cement-Based Piezoelectric Sensors,” Nondestructive Testing and Evaluation, V. 30, No. 4, 2015, pp. 312-326.

7. Xu, D.; Banerjee, S.; Wang, Y.; Huang, S.; and Cheng, X., “Temperature and Loading Effects of Embedded Smart Piezoelectric Sensor for Health Monitoring of Concrete Structures,” Construction and Building Materials, V. 76, Feb. 2015, pp. 187-193.

8. Jingzhou, L.; Congya, S.; Qingbin, L.; Fengli, L.; and Fengda, W., “Theoretical Investigation on Natural Frequency of Electrorheological Material Based Adaptive Mortar Beam Structures Using Concentrated Compliance Method,” Journal of Basic Science and Engineering, V. 4, 2009, pp. 558-565.

9. Soleymani, M. M.; Hajabasi, M. A.; and Elahi Mahani, S., “Free Vibrations Analysis of a Sandwich Rectangular Plate with Electrorheological Fluid Core,” Journal of Computational and Applied Research in Mechanical Engineering, V. 5, No. 1, 2015, pp. 71-81.

10. Lim, S. H.; Prusty, B. G.; Pearce, G.; Kelly, D.; and Thomson, R. S., “Study of Magnetorheological Fluids Towards Smart Energy Absorption of Composite Structures for Crashworthiness,” Mechanics of Advanced Materials and Structures, V. 23, No. 5, 2016, pp. 538-544.

11. Xu, Z. D.; Shen, Y. P.; and Guo, Y. Q., “Semi-Active Control of Structures Incorporated with Magnetorheological Dampers Using Neural Networks,” Smart Materials and Structures, V. 12, No. 1, Jan. 2003, pp. 80-87.

12. Jani, J. M.; Leary, M.; Subic, A.; and Gibson, M. A., “A Review of Shape Memory Alloy Research, Applications and Opportunities,” Materials & Design, V. 56, Apr. 2014, pp. 1078-1113.

13. Chen, Q., and Andrawe, B., “Monotonic and Cyclic Experimental Testing of Concrete Confined with Shape Memory Alloy Spirals,” Proceedings of 10th US National Conference on Earthquake Engineering, July 21-25, 2014, Anchorage, AK.

14. Sheta, E. F.; Moses, R. W.; and Huttsell, L. J., “Active Smart Material Control System for Buffet Alleviation,” Journal of Sound and Vibration, V. 292, No. 3-5, May 2006, pp. 854-868.

15. Li, Z., and Bainum, P. M., “Vibration Control of Flexible Spacecraft Integrating a Momentum Exchange Controller and a Distributed Piezoelectric Actuator,” Journal of Sound and Vibration, V. 177, No. 4, Nov. 1994, pp. 539-553.

16. Feng, Q.; Kong, Q.; and Song, G., “Damage Detection of Concrete Piles Subject to Typical Damage Types Based on Stress Wave Measurement Using Embedded Smart Aggregates Transducers,” Measurement, V. 88, June 2016, pp. 345-352.

17. Ai, D.; Zhu, H.; and Luo, H., “Sensitivity of Embedded Active PZT Sensors for Concrete Structural Impact Damage Detection,” Journal of Construction and Building Materials, V. 111, May 2016, pp. 348-357.

18. Agrawal, B. N.; Elshafei, M. A.; and Song, G., “Adaptive Antenna Shape Control Using Piezoelectric Actuators,” Acta Astronautica, V. 40, No. 11, June 1997, pp. 821-826.

19. Baier, H., “Approaches and Technologies for Optimal Control-Structure-Interaction in Smart Structures,” Transactions on the Built Environment, V. 19, 1996, pp. 323-335.

20. Messineo, A.; Alaimo, A.; Denaro, M.; and Ticali, D., “Piezoelectric Bender Transducers for Energy Harvesting Applications,” Energy Procedia, V. 14, 2012, pp. 39-44.

21. Zhou, L.; Sun, J.; Zheng, X. J.; Deng, S. F.; Zhao, J. H.; Peng, S. T.; Zhang, Y.; Wang, X. Y.; and Cheng, H. B., “A Model for the Energy Harvesting Performance of Shear Mode Piezoelectric Cantilever,” Sensors and Actuators. A, Physical, V. 179, June 2012, pp. 185-192.

22. Mayer, D.; Atzrodt, H.; Herold, S.; and Thomaier, M., “An Approach for the Model Based Monitoring of Piezoelectric Actuators,” Computers & Structures, V. 86, No. 3-5, Feb. 2008, pp. 314-321.

23. Wu, Z.; Qing, X. P.; and Chang, F. K., “Damage Detection for Composite Laminate Plates with a Distributed Hybrid PZT/FBG Sensor Network,” Journal of Intelligent Material Systems and Structures, V. 20, No. 9, June 2009, pp. 1069-1077.

24. Ray, M. C., and Balaji, R., “Active Structural-Acoustic Control of Laminated Cylindrical Panels Using Smart Damping Treatment,” International Journal of Mechanical Sciences, V. 49, No. 9, Sept. 2007, pp. 1001-1017.

25. Choi, S. C.; Park, J. S.; and Kim, J. H., “Active Damping of Rotating Composite Thin-Walled Beams Using MFC Actuators and PVDF Sensors,” Composite Structures, V. 76, No. 4, Dec. 2006, pp. 362-374.

26. Goldfeld, Y.; Rabinovitch, O.; Quadflieg, T.; and Gries, T., “Integrated Monitoring of TRC Using Carbon Fibers,” Proceedings of the 11th International Symposium on Ferrocement and 3rd ICTRC International Conference on Textile Reinforced Concrete, Aachen, Germany, June 2015, pp. 327-334.

27. Afshin, H.; Gholizadeh, M.; and Khorshidi, N., “Improving Mechanical Properties of High Strength Concrete by Magnetic Water Technology,” Journal of Scientia Iranica Transaction A,” Civil Engineering (New York, N.Y.), V. 17, No. 1, Feb. 2010, pp. 74-79.

28. Reddy, B. S. K.; Ghorpade, V. G.; and Rao, H. S., “Effect of Magnetic Field Exposure Time on Workability and Compressive Strength of Magnetic Water Concrete,” International Journal of Advances in Engineering and Technology, V. 4, No. 3, July-Sept. 2013, pp. 120-122.

29. Soltani Todeshki, A. R.; Raeisi Vanani, H.; Shayannejad, M.; and Ostad Ali Askari, K., “Effects of Magnetized Municipal Effluent on Some Chemical Properties of Soil in Furrow Irrigation,” International Journal of Agriculture and Crop Sciences, V. 8, No. 3, 2015, pp. 482-489.

30. Cai, R.; Yang, H.; He, J.; and Zhu, W., “The Effects of Magnetic Fields on Water Molecular Hydrogen Bonds,” Journal of Molecular Structure, V. 938, No. 1-3, Dec. 2009, pp. 15-19.

31. Khorshidi, N.; Ansari, M.; and Bayat, M., “An Investigation of Water Magnetization and its Influence on Some Concrete Specificities Like Fluidity and Compressive Strength,” Computers and Concrete, V. 13, No. 5, May 2014, pp. 649-657.

32. Tawfic, Y. R., and Abdelmoez, W., “The Influence of “Water Magnetization” on Fresh and Hardened Concrete Properties,” International Journal of Civil Engineering and Technology, V. 4, No. 6, Nov.-Dec. 2013, pp. 31-43. (IJCIET)

33. Ahmed, S. M., “Effect of Magnetic Water on Engineering Properties of Concrete,” Journal of Al-Rafidain Engineering, V. 7, No. 1, Feb. 2009, pp. 71-82.

34. Su, N.; Wu, Y.-H.; and Mar, C.-Y., “Effect of Magnetic Water on the Engineering Properties of Concrete Containing Granulated Blast-Furnace Slag,” Cement and Concrete Research, V. 30, No. 4, Apr. 2000, pp. 599-605.

35. Su, N., and Wu, C.-F., “Effect of Magnetic Field Treated Water on Mortar and Concrete Containing Fly Ash,” Cement and Concrete Composites, V. 25, No. 7, Oct. 2003, pp. 681-688.

36. Gholizadeh, M., and Arabshahi, H., “The Effect of Magnetic Water on Strength Parameters of Concrete,” Journal of Engineering and Technology Research, V. 3, No. 3, Mar. 2011, pp. 77-81.

37. Reddy, B. S. K.; Ghorpade, V. G.; and Rao, H. S., “Influence of Magnetic Water on Strength Properties of Concrete,” Indian Journal of Science and Technology, V. 7, No. 1, Jan. 2014, pp. 14-18.

38. Nair, S. D., and Ferron, R. D., “Set-on-Demand Concrete,” Cement and Concrete Research, V. 57, Mar. 2014, pp. 13-27.

39. Soto-Bernal, J. J.; Gonzalez-Mota, R.; Rosales, I.; and Ortiz-Lozano, J. A., “Effects of Static Magnetic Fields on the Physical, Mechanical, and Microstructural Properties of Cement Pastes,” Advances in Materials Science and Engineering, V. 2015, Apr. 2015, pp. 1-9.

40. Abavisani, I.; Rezaifar, O.; and Kheyroddin, A., “Magneto-Electric Control of Scaled-Down Reinforced Concrete Beams,” ACI Structural Journal, V. 114, No. 1, Jan.-Feb. 2017, pp. 233-244. doi: 10.14359/51689452

41. Bakshi, U. A., and Bakshi, M. V., “Magnetic Circuits,” Magnetic Circuits and Transformers, Technical Publications, India, 2008, pp. 1-48.

42. Askeland, D. R., and Wright, W. J., The Science and Engineering of Materials, seventh edition, Cengage Learning, Boston, MA, 2015, 960 pp.

43. ASTM C109/C109M-02, “Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. or [50-mm] Cube Specimens),” ASTM International, West Conshohocken, PA, 2002, 6 pp.

44. ASTM C39/C39M-03, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2003, 5 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal