330.2R-17: Guide for the Design and Construction of Concrete Site Paving for Industrial and Trucking Facilities

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 330.2R-17: Guide for the Design and Construction of Concrete Site Paving for Industrial and Trucking Facilities

Author(s): ACI Committee 330

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 67

Keywords: industrial pavement; joint stability; lift truck; lug anchor; over-the-road truck; pavement support system; sustainable industrial pavement system; unreinforced concrete pavement.

DOI:

Date: 4/27/2017

Abstract:
This guide provides information useful in the design and construction of a successful site-paving project for heavy-duty industrial and trucking facilities. This information assists architects/engineers, contractors, and testing agencies with designing, detailing, constructing, repairing, and inspecting site paving. Engineers use this guide to make recommendations for the pavement support system, concrete mixture, pavement thickness, joint spacing, and load transfer devices. Thickness design tables are including for common over-the-road trucks and industrial lift trucks. Tables are also provided to check the pavement thickness for punching shear and concrete strength for bearing stress applied by loaded trailers that have been disconnected from the tractor. Contractors use this guide to understand proper ways to construct site paving with block or strip placements and avoid common mistakes made during construction. Proper placing, consolidating, and finishing techniques are described to construct a durable pavement that complies with the project documents. Inspectors and testing agencies use this guide to understand the design and be better equipped to monitor the project from stripping and grubbing of the site to concrete pavement curing. Testing and inspection included in this guide should only be done by individuals holding the appropriate certifications.