Title: Products & Practice Spotlight: Rehabbing Aging Infrastructure

Author(s):

Publication: Concrete International

Volume: 39

Issue: 5

Appears on pages(s): 54-55

Keywords: concrete, wastewater, crack, repair

DOI: 10.14359/51700751

Date: 5/1/2017

Abstract:
Polyurea coatings and liners can provide strong, flexible, damage-resistant dampproofing in wastewater infrastructure rehabilitation projects. With the proper crack repair and surface preparation, coatings can be applied directly to the concrete over a wide temperature range. Rapid curing helps to minimize facility downtime.