343R-95: Analysis and Design of Reinforced Concrete Bridge Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 343R-95: Analysis and Design of Reinforced Concrete Bridge Structures

Author(s): ACI Committee 343

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 162

Keywords: bridges

DOI:

Date: 3/1/1995

Abstract:
This new report provides currently acceptable guidelines for the analysis and design of reinforced, prestressed, and partially prestressed concrete bridges based on the state-of-the-art at this time. The provisions recommended herein apply to pedestrian bridges, highway bridges, railroad bridges, airport taiway bridges, and other special bridge structures.