Acid-soluble and Water-soluble Chloride – Testing Proficiency and Specification

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Acid-soluble and Water-soluble Chloride – Testing Proficiency and Specification

Author(s): W. South, W.A. Thomas, V. Sirivivatnanon

Publication: CCAA

Volume:

Issue:

Appears on pages(s): 502–513

Keywords: Acid-soluble, water-soluble, chloride, performance limit Rights: (c) 2015 the authors

DOI:

Date: 8/31/2015

Abstract:
The importance of limiting the chloride ion content in concrete has always been recognised and specified in structural concrete specifications. The Australian Standard test method for acid-soluble chloride has been revised and published as AS 1012.20.1. At the same time, a newly developed water-soluble chloride test method has been published as a parallel Australian Standard AS 1012.20.2. The paper reviews and report the proficiency of the two test methods and the relationship between acid- and water-soluble chloride based on research and proficiency testing program conducted by Cement Concrete and Aggregates Australia (CCAA). Performance limits specified in international concrete standards are reviewed and recommended to be specified in relevant Australian standards and specifications.


Cement Concrete & Aggregates Australia, International Partner Access

View Resource »