Towards a More Sustainable Australian Cement and Concrete Industry

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Towards a More Sustainable Australian Cement and Concrete Industry

Author(s): James Mohammadi, Warren South, Des Chalmers

Publication: CCAA

Volume:

Issue:

Appears on pages(s): 596-603

Keywords: General purpose (GP) cements; Limestone cement; Australian Standard AS 3972; Australian Standard AS 2350; Sulfate expansion; Rapid chloride penetration

DOI:

Date: 1/9/2015

Abstract:
This document provides a summary of results for the comprehensive test program to investigate the properties and performance of General Purpose (Type GP) cement prepared with up to 12% limestone content. An extensive literature review was carried out initially, and then an experimental research program designed. Cement, mortar, and concrete tests were conducted on a variety of mixes to evaluate the effect of introducing higher limestone mineral addition content to cement. The test results showed that there is no significant effect on most concrete properties due to increasing the limestone addition in cement. The result of this research supports the recommendation to increase the allowable limestone content of General Purpose (Type GP) cement to a maximum of 12%


Cement Concrete & Aggregates Australia, International Partner Access

View Resource »