Effects of Fly Ash on Early-Age Properties and Cracking of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Fly Ash on Early-Age Properties and Cracking of Concrete

Author(s): Inamullah Khan, Arnaud Castel, and Raymond Ian Gilbert

Publication: Materials Journal

Volume: 114

Issue: 4

Appears on pages(s): 673-681

Keywords: cracking age; fly ash; shrinkage; tensile creep

DOI: 10.14359/51689898

Date: 7/1/2017

Abstract:
This paper focuses on the effects of fly ash on early-age mechanical and viscoelastic properties of concrete and on early-age cracking. Fly ash is a supplementary cementitious material that is mainly used to increase the durability of concrete. The effect on shrinkage-induced cracking of replacing some ordinary portland cement (OPC) with fly ash has not been studied previously. Material properties such as compressive strength, indirect tensile strength, and elastic modulus were measured with different percentage replacements of OPC with fly ash. Tensile creep and drying shrinkage were also measured on two types of specimens by using two different experimental techniques. The cracking age of plain concrete was observed by using a restrained ring test. Results revealed that the strength evolution of fly-ash-blended concrete is lower than the corresponding OPC concrete and the age at which restrained shrinkage cracking first occurs is also reduced. Slightly higher tensile creep coefficients were observed for fly-ash-blended concrete compared to OPC concrete, but drying shrinkage was not altered to any great extent.

Related References:

1. Naik, T. R., and Singh, S. S., “Influence of Fly Ash on Setting and Hardening Characteristics of Concrete Systems,” ACI Materials Journal, V. 94, No. 5, Sept.-Oct. 1997, pp. 355-360.

2. Sivasundaram, V.; Carette, G. G.; and Malhotra, V. M., “Long-Term Strength Development of High-Volume Fly Ash Concrete,” Cement and Concrete Composites, V. 12, No. 4, 1990, pp. 263-270. doi: 10.1016/0958-9465(90)90005-I

3. Tikalsky, P. J.; Carrasquillo, P. M.; and Carrasquillo, R. L., “Strength and Durability Considerations Affecting Mix Proportioning of Concrete Containing Fly Ash,” ACI Materials Journal, V. 85, No. 6, Nov.-Dec. 1988, pp. 505-511.

4. Day, R. L., “Strength, Durability and Creep of Fly-Ash Concrete. Part II,” Serviceability and Durability of Construction Materials, Proceedings of the 1st Materials Engineering Conference, Denver, CO, 1990, pp. 864-873.

5. Haque, M. N.; Kayyali, O. A.; and Gopalan, M. K., “Fly Ash Reduces Harmful Chloride Ions in Concrete,” ACI Materials Journal, V. 89, No. 3, May-June 1992, pp. 238-241.

6. AS 1012.9:2014, “Methods of Testing Concrete—Compressive Strength Tests – Concrete, Mortar and Grout Specimens,” Standards Australia, Sydney, Australia, 2014.

7. AS 1012.10:2000, “Methods of Testing Concrete – Determination of Indirect Tensile Strength of Concrete Cylinders (‘Brazil’ or Splitting Test),” Standards Australia, Sydney, Australia, 2000.

8. Shah, S. P.; Karaguler, M. E.; and Sarigaphuti, M., “Effects of Shrinkage-Reducing Admixture on Restrained Shrinkage Cracking of Concrete,” ACI Materials Journal, V. 89, No. 3, May-June 1992, pp. 88-90.

9. Weiss, W. J.; Yang, W.; and Shah, S. P., “Influence of Specimen Size and Geometry on Shrinkage Cracking,” Journal of Engineering Mechanics, ASCE, V. 126, No. 1, 2000, pp. 93-101. doi: 10.1061/(ASCE)0733-9399(2000)126:1(93)

10. Grzybowski, M., and Shah, S. P., “Shrinkage Cracking of Fiber Reinforced Concrete,” ACI Materials Journal, V. 87, No. 2, Mar.-Apr. 1990, pp. 138-148.

11. See, H. T.; Attiogbe, E. K.; and Miltenberger, M. A., “Shrinkage Cracking Characteristics of Concrete Using Ring Specimens,” ACI Materials Journal, V. 100, No. 3, May-June 2003, pp. 239-245.

12. Hossain, A. B., and Weiss, J., “Assessing Residual Stress Development and Stress Relaxation in Restrained Concrete Ring Specimens,” Cement and Concrete Composites, V. 26, No. 5, 2004, pp. 531-540. doi: 10.1016/S0958-9465(03)00069-6

13. Dong, W.; Zhou, X. M.; and Wu, Z. M., “Influence of Specimen Thickness on Cracking Behaviour in Restrained Shrinkage Ring Test,” IACSIT International Journal of Engineering and Technology, V. 5, No. 6, 2013, pp. 698-702. doi: 10.7763/IJET.2013.V5.645

14. Trost, H., “Auswirkungen des Superpositionsprinzips auf Kriech- und Relaxations Probleme bei Beton und Spannbeton,” Beton- und Stahlbetonbau, V. 62, 1967, pp. 261-269. (in German)

15. Dilger, W., and Neville, A. M., “Method of Creep Analysis of Structural Members,” Designing for Effects of Creep, Shrinkage and Temperature in Concrete Structures, SP-27, American Concrete Institute, Farmington Hills, MI, 1971, pp. 349-379.

16. Bažant, Z. P., “Prediction of Concrete Creep Effects Using Age-Adjusted Effective Modulus Method,” ACI Journal Proceedings, V. 69, No. 4, Apr. 1972, pp. 212-217.

17. Gilbert, R. I., and Ranzi, G., Time-Dependent Behaviour of Concrete Structures, Spon Press, London, UK, 2010.

18. Tao, Z., and Weizu, Q., “Tensile Creep due to Restraining Stresses in High-Strength Concrete at Early Ages,” Cement and Concrete Research, V. 36, No. 3, 2006, pp. 584-591. doi: 10.1016/j.cemconres.2005.11.017

19. Pane, I., and Hansen, W., “Early Age Creep and Stress Relaxation of Concrete Containing Blended Cements,” Materials and Structures, V. 35, No. 246, 2002, pp. 92-96. doi: 10.1617/13800

20. Akkaya, Y.; Ouyang, C.; and Shah, S. P., “Effect of Supplementary Cementitious Materials on Shrinkage and Crack Development in Concrete,” Cement and Concrete Composites, V. 29, No. 2, 2007, pp. 117-123. doi: 10.1016/j.cemconcomp.2006.10.003

21. Mehta, P. K., and Monteiro, J. M., Concrete: Microstructure, Properties and Materials, third editiion, McGraw-Hill, New York, 2006.

22. Mindess, S.; Young, J. F.; and Darwin, D., Concrete, second edition, Prentice Hall, Upper Saddle River, NJ, 2002.


ALSO AVAILABLE IN:

Electronic Materials Journal