Influence of Alkali-Silica Reaction Reactivity on Corrosion in Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Alkali-Silica Reaction Reactivity on Corrosion in Reinforced Concrete

Author(s): David Trejo, Vandad Mazarei, Jason H. Ideker, and O. Burkan Isgor

Publication: Materials Journal

Volume: 114

Issue: 5

Appears on pages(s): 723-731

Keywords: alkali-silica reaction (ASR); ASR gel; corrosion; critical chloride threshold; diffusivity; interfacial transition zone

DOI: 10.14359/51689895

Date: 9/1/2017

Abstract:
Alkali-silica reaction (ASR) and reinforcement corrosion are wellknown deterioration mechanisms in concrete structures. This research investigates how ASR affects corrosion in reinforced concrete specimens. Concrete specimens containing aggregate susceptible to ASR (reactive) and aggregate not susceptible to ASR (nonreactive) were cast. Expansion of the specimens, corrosion potential, macrocell current, and chloride diffusivity were measured for each specimen until the embedded reinforcement began to actively corrode. Scanning electron microscopy (SEM) results indicate that ASR gel can fill the interfacial transition zone (ITZ) and cracks, which can reduce the transport of the chlorides in concrete. The presence of ASR gel at the HCP-steel interface likely reduces the pH at the interface, which can reduce the critical chloride threshold level (CT). The results indicate that ASR expansion does not significantly influence the time to corrosion initiation of reinforced concrete systems for laboratory specimens exposed to wetting/drying cycles at 100°F (38°C).

Related References:

1. Swamy, S. N., The Alkali-Silica Reaction in Concrete, Blackie and Son Ltd, 2002, 336 pp.

2. Stanton, T. E., “Expansion of Concrete through Reaction between Cement and Aggregate,” Proceedings of the American Society of Civil Engineers, V. 66, 1940, pp. 1781-1811.

3. Wang, H., and Gillott, J. E., “Mechanism of Alkali-Silica Reaction and the Significance of Calcium Hydroxide,” Cement and Concrete Research, V. 21, No. 4, 1991, pp. 647-654. doi: 10.1016/0008-8846(91)90115-X

4. Bérubé, M. A.; Fournier, B.; and Durand, B., “Chemistry and Other Characteristics of ASR Gels,” 11th International Conference on Alkali Aggregate Reactions in Concrete, QC, Canada, 2000, pp. 31-40.

5. Kawamura, M.; Arano, N.; and Terashima, T., “Composition of ASR Gels and Expansion of Mortars,” Sidney Diamond Symposium, 1998, pp. 261-276.

6. Thaulow, N.; Jakobsen, U. H.; and Clark, B., “Composition of Alkali Silica Gel and Ettringite in Concrete Railroad Ties: SEM-EDX and X-Ray Diffraction Analyses,” Cement and Concrete Research, V. 26, No. 2, 1996, pp. 309-318. doi: 10.1016/0008-8846(95)00219-7

7. Pourbaix, M., Atlas of Electrochemical Equilibria in Aqueous Solutions, second edition, NACE International, Houston, TX, 1974, 664 pp.

8. Pillai, R. G., and Trejo, D., “Surface Condition Effects on Critical Chloride Threshold of Steel Reinforcement,” ACI Materials Journal, V. 102, No. 2, Mar.-Apr. 2005, pp. 103-109.

9. Trejo, D., and Pillai, R. G., “Accelerated Chloride Threshold Testing: Part I—ASTM A 615 and A 706 Reinforcement,” ACI Materials Journal, V. 100, No. 6, Nov.-Dec. 2003, pp. 519-527.

10. Alonso, C.; Andrade, C.; Castellote, M.; and Castro, P., “Chloride Threshold Values to Depassivate Reinforcing Bars Embedded in a Standardized OPC Mortar,” Cement and Concrete Research, V. 30, No. 7, 2000, pp. 1047-1055. doi: 10.1016/S0008-8846(00)00265-9

11. Hansson, C. M., and Sorensen, B., “Threshold Concentration of Chloride in Concrete for the Initiation of Reinforcement Corrosion,” ASTM Special Technical Publication, No. 1065, 1990, pp. 3-16.

12. Angst, U.; Elsener, B.; Larsen, C. K.; and Vennesland, Ø., “Critical Chloride Content in Reinforced Concrete—A Review,” Cement and Concrete Research, V. 39, No. 12, 2009, pp. 1122-1138. doi: 10.1016/j.cemconres.2009.08.006

13. Scrivener, K. L., and Gartner, E. M., “Microstructural Gradients in Cement Paste around Aggregate Particles,” Symposium R – Bonding in Cementitious Composites, V. 114, 1987, pp. 77-86.

14. Leemann, A.; Münch, B.; Gasser, P.; and Holzer, L., “Influence of Compaction on the Interfacial Transition Zone and the Permeability of Concrete,” Cement and Concrete Research, V. 36, No. 8, 2006, pp. 1425-1433. doi: 10.1016/j.cemconres.2006.02.010

15. Zheng, J.; Wong, H. S.; and Buenfeld, N. R., “Assessing the Influence of ITZ on the Steady-State Chloride Diffusivity of Concrete Using a Numerical Model,” Cement and Concrete Research, V. 39, No. 9, 2009, pp. 805-813. doi: 10.1016/j.cemconres.2009.06.002

16. Ollivier, J. P.; Maso, J. C.; and Bourdette, B., “Interfacial Transition Zone in Concrete,” Advanced Cement Based Materials, V. 2, No. 1, 1995, pp. 30-38. doi: 10.1016/1065-7355(95)90037-3

17. Oh, B. H., and Jang, S. Y., “Prediction of Diffusivity of Concrete Based on Simple Analytic Equations,” Cement and Concrete Research, V. 34, No. 3, 2004, pp. 463-480. doi: 10.1016/j.cemconres.2003.08.026

18. Caré, S., and Hervé, E., “Application of a n-Phase Model to the Diffusion Coefficient of Chloride in Mortar,” Transport in Porous Media, V. 56, No. 2, 2004, pp. 119-135. doi: 10.1023/B:TIPM.0000021730.34756.40

19. Yang, C. C., “Effect of the Interfacial Transition Zone on the Transport and the Elastic Properties of Mortar,” Magazine of Concrete Research, V. 55, No. 4, 2003, pp. 305-312. doi: 10.1680/macr.2003.55.4.305

20. Delagrave, A.; Bigas, J. P.; Ollivier, J. P.; Marchand, J.; and Pigeon, M., “Influence of the Interfacial Zone on the Chloride Diffusivity of Mortars,” Advanced Cement Based Materials, V. 5, No. 3-4, 1997, pp. 86-92. doi: 10.1016/S1065-7355(96)00008-9

21. Wang, L.; Soda, M.; and Ueda, T., “Simulation of Chloride Diffusivity for Cracked Concrete Based on RBSM and Truss Network Model,” Journal of Advanced Concrete Technology, V. 6, No. 1, 2008, pp. 143-155. doi: 10.3151/jact.6.143

22. Winslow, D. N.; Cohen, M. D.; Bentz, D. P.; Snyder, K. A.; and Garboczi, E. J., “Percolation and Pore Structure in Mortars and Concrete,” Cement and Concrete Research, V. 24, No. 1, 1994, pp. 25-37. doi: 10.1016/0008-8846(94)90079-5

23. François, R., and Arliguie, G., “Influence of Service Cracking on Reinforcement Steel Corrosion,” Journal of Materials in Civil Engineering, ASCE, V. 10, No. 1, 1998, pp. 14-20. doi: 10.1061/(ASCE)0899-1561(1998)10:1(14)

24. Otieno, M. B.; Alexander, M. G.; and Beushausen, H. D., “Corrosion in Cracked and Uncracked Concrete—Influence of Crack Width, Concrete Quality and Crack Reopening,” Magazine of Concrete Research, V. 62, No. 6, 2010, pp. 393-404. doi: 10.1680/macr.2010.62.6.393

25. Yu, L.; François, R.; Dang, V. H.; L’Hostis, V.; and Gagné, R., “Development of Chloride-Induced Corrosion in Pre-cracked RC Beams under Sustained Loading: Effect of Load-Induced Cracks, Concrete Cover, and Exposure Conditions,” Cement and Concrete Research, V. 67, 2015, pp. 246-258. doi: 10.1016/j.cemconres.2014.10.007

26. Picket, G., “Effect of Gypsum Content and Other Factors on Shrinkage of Concrete Prism,” ACI Journal Proceedings, V. 44, No. 10, Oct. 1947, pp. 149-176.


ALSO AVAILABLE IN:

Electronic Materials Journal