Shear Design Considering Interaction between Steel Stirrups and Carbon Fiber-Reinforced Polymer Strips

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Design Considering Interaction between Steel Stirrups and Carbon Fiber-Reinforced Polymer Strips

Author(s): Yungon Kim, Wassim M. Ghannoum, and James O. Jirsa

Publication: Structural Journal

Volume: 114

Issue: 4

Appears on pages(s): 803-813

Keywords: carbon fiber-reinforced polymer (CFRP); interaction of steel and CFRP; modification factors; shear design; strengthening

DOI: 10.14359/51689867

Date: 7/1/2017

Abstract:
Conventional shear-strength relations provide conservative estimates for the design strength of new members. However, when members are strengthened with carbon fiber-reinforced polymer (CFRP) vertical strips, the traditional approach of independently summing the concrete, steel, and CFRP contributions to shear strength was found to overestimate the strength increase due to the CFRP material. Thus, modification factors ksF and kfS are proposed to modify the shear-strength equations in ACI 440.2R and account for the interaction between steel and CFRP transverse reinforcement. The proposed factors provide more accurate and less conservative estimates of shear strength of concrete beams, with improved estimates of the strength increase when CFRP materials are added.

Related References:

1. Joint ACI-ASCE Committee 445, “Recent Approaches to Shear Design of Structural Concrete,” Journal of Structural Engineering, ASCE, V. 124, No. 12, 1998, pp. 1375-1417.

2. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

3. AASHTO, “AASHTO LRFD Bridge Design Specifications,” fourth edition, Washington, DC, 2007.

4. Kim, Y., “Shear Behavior of Reinforced Concrete T-Beams Strengthened with Carbon Fiber Reinforced Polymer Sheets and CFRP Anchors,” PhD dissertation, Department of Civil, Environmental and Architectural Engineering, University of Texas at Austin, Austin, TX, 2011.

5. Kim, Y.; Quinn, K.; Satrom, N.; Garcia, Jo.; Sun, W.; Ghannoum, W. M.; and Jirsa, J. O., “Shear Strengthening of Large Reinforced and Prestressed Concrete Elements Using Carbon Fiber Reinforced Polymer (CFRP) Sheets and CFRP Anchors,” Center for Transportation Research (CTR) Report 0-6306-1, 2012, 296 pp.

6. Kim, Y.; Quinn, K.; Ghannoum, W. M.; and Jirsa, J. O., “Strengthening of Reinforced Concrete T-Beams Using Anchored CFRP Materials,” ACI Structural Journal, V. 111, No. 5, Sept.-Oct. 2014, pp. 1027-1036.

7. Kim, Y.; Ghannoum, W. M.; and Jirsa, J. O., “Shear Behavior of Full-Scale Reinforced Concrete T-Beams Strengthened with CFRP Strips and Anchors,” Construction and Building Materials, V. 94, 2015, pp. 1-9.

8. Chen, G. M.; Teng, J. G.; Chen, J. F.; and Rosenboom, O. A., “Interaction between Steel Stirrups and Shear-Strengthening FRP Strips in RC Beams,” Journal of Composites for Construction, ASCE, V. 14, No. 5, 2010, pp. 498-509.

9. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 76 pp.

10. Chaallal, O.; Shahawy, M.; and Hassan, M., “Performance of Reinforced Concrete T-Girders Strengthened in Shear with Carbon Fiber-Reinforced Polymer Fabric,” ACI Structural Journal, V. 99, No. 3, May-June 2002, pp. 335-343.

11. Bousselham, A., and Chaallal, O., “Behavior of Reinforced Concrete T-Beams Strengthened in Shear with Carbon Fiber Reinforced Polymer—An Experimental Study,” ACI Structural Journal, V. 103, No. 3, May-June 2006, pp. 339-347.

12. Bousselham, A., and Chaallal, O., “Mechanisms of Shear Resistance of Concrete Beams Strengthened in Shear with Externally Bonded FRP,” Journal of Composites for Construction, ASCE, V. 12, No. 5, 2008, pp. 499-512.

13. Chen, J. F., and Teng, J. G., “Shear Capacity of Fiber-Reinforced Polymer-Strengthened Reinforced Concrete Beams: Fiber Reinforced Polymer Rupture,” Journal of Structural Engineering, ASCE, V. 129, No. 5, 2003, pp. 615-625.

14. Chen, J. F., and Teng, J. G., “Shear Capacity of FRP-Strengthened RC Beams: FRP Debonding,” Construction and Building Materials, V. 17, No. 1, 2003, pp. 27-41.

15. Pellegrino, C., and Modena, C., “Fiber Reinforced Polymer Shear Strengthening of Reinforced Concrete Beams with Transverse Steel Reinforcement,” Journal of Composites for Construction, ASCE, V. 6, No. 2, 2002, pp. 104-111.

16. Pellegrino, C., and Modena, C., “Fiber-Reinforced Polymer Shear Strengthening of Reinforced Concrete Beams: Experimental Study and Analytical Modeling,” ACI Structural Journal, V. 103, No. 5, Sept.-Oct. 2006, pp. 720-728.

17. Grande, E., and Imbimbo, M., “Effect of Transverse Steel on the Response of RC Beams Strengthened in Shear by FRP: Experimental Study,” Journal of Composites for Construction, ASCE, V. 13, No. 5, 2009, pp. 405-414.

18. NCHRP Report 514, “Bonded Repair and Retrofit of Concrete Structures Using FRP Composites—Recommended Construction Specifications and Process Control Manual,” Transportation Research Board, Washington, DC, 2014.

19. NCHRP Report 655, “Recommended Guide Specification for the Design of Externally Bonded FRP Systems for Repair and Strengthening of Concrete Bridge Elements,” Transportation Research Board, Washington, DC, 2010.

20. NCHRP Report 678, “Design of FRP Systems for Strengthening Concrete Girders in Shear,” Transportation Research Board, Washington, DC, 2011.

21. Sas, G.; Täljsten, B.; Barros, J.; and Lima, J., “Are Available Models Reliable for Predicting the FRP Contribution to the Shear Resistance of RC Beams?” Journal of Composites for Construction, ASCE, V. 13, No. 6, 2009, pp. 514-534.

22. Abdeldjelil, B., “Behavior of Full-Scale RC T-Beams Strengthened in Shear with Externally Bonded FRP Sheets,” Construction and Building Materials, V. 32, 2012, pp. 27-40.

23. Colotti, V., “Shear Interaction Effect between Transverse Reinforcements in FRP-Strengthened RC Beams,” Composites. Part B, Engineering, V. 45, No. 1, 2013, pp. 1222-1233.

24. Chen, G., “Shear Strength Model for FRP-Strengthened RC Beams with Adverse FRP-Steel Interaction,” Journal of Composites for Construction, ASCE, V. 17, No. 1, 2013, pp. 50-66.

25. Dias, S., and Barros, J., “Shear Strengthening of RC Beams with NSM CFRP Laminates: Experimental Research and Analytical Formulation,” Composite Structures, V. 99, 2013, pp. 477-490.

26. Deniaud, C., and Cheng, J., “Simplified Shear Design Method for Concrete Beams Strengthened with Fiber Reinforced Polymer Sheets,” Journal of Composites for Construction, ASCE, V. 8, No. 5, 2004, pp. 425-433.

27. Mofidi, A., and Chaallal, O., “Shear Strengthening of RC Beams with EB FRP: Influencing Factors and Conceptual Debonding Model,” Journal of Composites for Construction, ASCE, V. 15, No. 1, 2011, pp. 62-74.

28. Birrcher, D., “Design of Reinforced Concrete Deep Beams for Strength and Serviceability,” PhD dissertation, Univesity of Texas at Austin, Austin, TX, 2009.


ALSO AVAILABLE IN:

Electronic Structural Journal