Analysis-Oriented Stress-Strain Model for Concrete Confined with Fiber-Reinforced Polymer Spirals

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analysis-Oriented Stress-Strain Model for Concrete Confined with Fiber-Reinforced Polymer Spirals

Author(s): Thomas A. Hales, Chris P. Pantelides, Priyank Sankholkar, and Lawrence D. Reaveley

Publication: Structural Journal

Volume: 114

Issue: 5

Appears on pages(s): 1263-1272

Keywords: axial loads; concrete columns; confinement model; fiber-reinforced polymer; glass fibers; spiral; stress-strain

DOI: 10.14359/51689788

Date: 9/1/2017

Abstract:
Considerable research has been conducted for confinement of reinforced concrete (RC) columns with external fiber-reinforced polymer (FRP) jackets. Research is limited with respect to concrete confinement using internal FRP spirals. Concrete columns internally reinforced with FRP spirals and longitudinal bars have advantages because FRP composite materials are not susceptible to corrosion. This is a desirable alternative for coastal structures and structures subjected to severe environmental conditions, which deteriorate with time due to corrosion of steel reinforcement. Existing models for concrete confined with steel spirals cannot represent the behavior of FRP-confined concrete adequately because they are based on a constant confining stress. FRP composites behave in a linear elastic manner with confining stress increasing continuously until failure. An analytical confinement model has been developed and is proposed for describing the axial strength and stress-strain relationship of FRP-spiral-confined circular columns based on plasticity and the Popovics’ concrete model. FRP spirals have a lower modulus of elasticity compared to steel spirals and, hence, a larger bar diameter and smaller pitch is required for satisfactory performance. The proposed model, developed based on triaxial behavior of concrete, provides an accurate representation of FRP-spiral-confined concrete in axial compression experiments for a wide range of confining stress and could be used in analysis and design.

Related References:

1. Willam, K. J., and Warnke, E. P., “Constitutive Model for the Triaxial Behavior of Concrete,” Proceedings of the Seminar on Concrete Structures Subjected to Triaxial Stresses, 1974, 30 pp. http://doi.org/10.5169/seals-1752610.5169/seals-17526

2. Mander, J. B.; Priestley, J. N.; and Park, R., “Theoretical Stress-Strain Model for Confined Concrete,” Journal of Structural Engineering, ASCE, V. 114, No. 8, 1988, pp. 1804-1826. doi: 10.1061/(ASCE)0733-9445(1988)114:8(1804)

3. Bing, L.; Park, R.; and Tanaka, H., “Stress-Strain Behavior of High-Strength Concrete Confined by Ultra-High-and Normal-Strength Transverse Reinforcements,” ACI Structural Journal, V. 98, No. 3, May-June 2001, pp. 395-406.

4. Yan, Z., and Pantelides, C. P., “Fiber-Reinforced Polymer Jacketed and Shape-Modified Compression Members: II—Model,” ACI Structural Journal, V. 103, No. 6, Nov.-Dec. 2006, pp. 894-903.

5. Afifi, M. Z.; Mohamed, H. M.; and Benmokrane, B., “Theoretical Stress-Strain Model for Circular Concrete Columns Confined by GFRP Spirals and Hoops,” Engineering Structures, V. 102, Nov. 2015, pp. 202-213. doi: 10.1016/j.engstruct.2015.08.020

6. Afifi, M. Z.; Mohamed, H. M.; Chaallal, O.; and Benmokrane, B., “Confinement Model for Concrete Columns Internally Confined with Carbon FRP Spirals and Hoops,” Journal of Structural Engineering, ASCE, V. 141, No. 9, 2015, pp. 1-11. doi: 10.1061/(ASCE)ST.1943-541X.0001197

7. Karim, H.; Sheikh, M. N.; and Hadi, M. N. S., “Axial Load-Axial Deformation Behavior of Circular Concrete Columns Reinforced with GFRP Bars and Helices,” Construction and Building Materials, V. 112, 2016, pp. 1147-1157. doi: 10.1016/j.conbuildmat.2016.02.219

8. Maranan, G. B.; Manalo, A. C.; Benmokrane, B.; Karunasena, W.; and Mendis, P., “Behavior of Concentrically Loaded Geopolymer-Concrete Circular Columns Reinforced Longitudinally and Transversely with GFRP Bars,” Engineering Structures, V. 117, 2016, pp. 422-436. doi: 10.1016/j.engstruct.2016.03.036

9. Chen, W. F., and Han, D. J., Plasticity for Structural Engineering, Springer-Verlag, New York, 1982.

10. Schickert, G., and Winkler, H., “Results of Tests Concerning Strength and Strain of Concrete Subjected to Multiaxial Compressive Stresses,” Deutscher Ausschuss fur Stahlbeton, Heft 277, Berlin, West Germany, 1979.

11. Elwi, A. A., and Murray, D. W., “A 3D Hypoelastic Concrete Constitutive Relationship,” Journal of Engineering Mechanics, V. 105, No. 4, 1979, pp. 623-641.

12. Sankholkar, P. P., “Confinement Model for Concrete Columns Internally Reinforced with Glass Fiber Reinforced Polymer Spirals,” MS thesis, University of Utah, Salt Lake City, UT, 2016.

13. Hadi, M. N. S.; Karim, H.; and Sheikh, M. N., “Experimental Investigations on Circular Concrete Columns Reinforced with GFRP Bars and Helices under Different Loading Conditions,” Journal of Composites for Construction, ASCE, V. 20, No. 4, 2016, pp. 1-12. doi: 10.1061/(ASCE)CC.1943-5614.0000670

14. Lam, L., and Teng, J. G., “Design-Oriented Stress-Strain Model for FRP-Confined Concrete,” Construction and Building Materials, V. 17, No. 6-7, 2003, pp. 471-489. doi: 10.1016/S0950-0618(03)00045-X

15. Smith, S. S., “On Fundamental Aspects of Concrete Behavior,” Structural Research Series No. 87-12, C.E.A.E. Department, University of Colorado, Boulder, CO, 1987.

16. Mizuno, E., and Hatanaka, S., “Compressive Softening Model for Concrete,” Journal of Engineering Mechanics, ASCE, V. 118, No. 8, 1992, pp. 1546-1563. doi: 10.1061/(ASCE)0733-9399(1992)118:8(1546)

17. Imran, I., “Application of Non-Associated Plasticity in Modeling the Mechanical Response of Concrete,” PhD dissertation, University of Toronto, Toronto, ON, Canada, 1994.

18. Pantelides, C. P.; Gibbons, M. E.; and Reaveley, L. D., “Axial Load Behavior of Concrete Columns Confined with GFRP Spirals,” Journal of Composites for Construction, ASCE, V. 17, No. 3, 2013, pp. 305-313. doi: 10.1061/(ASCE)CC.1943-5614.0000357

19. Afifi, M. Z.; Mohamed, H. M.; and Benmokrane, B., “Axial Capacity of Circular Concrete Columns Reinforced with GFRP Bars and Spirals,” Journal of Composites for Construction, ASCE, V. 18, No. 1, 2014, pp. 1-11. doi: 10.1061/(ASCE)CC.1943-5614.0000438

20. Afifi, M. Z.; Mohamed, H. M.; and Benmokrane, B., “Strength and Axial Behavior of Circular Concrete Columns Reinforced with CFRP Bars and Spirals,” Journal of Composites for Construction, ASCE, V. 18, No. 2, 2014, pp. 1-11. doi: 10.1061/(ASCE)CC.1943-5614.0000430

21. Mohamed, H. M.; Afifi, M. Z.; and Benmokrane, B., “Performance Evaluation of Concrete Columns Reinforced Longitudinally with FRP Bars and Confined with FRP Hoops and Spirals under Axial Load,” Journal of Bridge Engineering, ASCE, V. 19, No. 7, 2014, pp. 1-12. doi: 10.1061/(ASCE)BE.1943-5592.0000590

22. Hales, T. A., “Slender Concrete Columns Reinforced with Fiber Reinforced Polymer Spirals,” PhD dissertation, University of Utah, Salt Lake City, UT, 2015.

23. Hales, T. A.; Pantelides, C. P.; and Reaveley, L. D., “Experimental Evaluation of Slender High-Strength Concrete Columns with GFRP and Hybrid Reinforcement,” Journal of Composites for Construction, ASCE, V. 20, No. 6, 2016, pp. 1-10. doi: 10.1061/(ASCE)CC.1943-5614.0000709

24. Popovics, S., “A Numerical Approach to the Complete Stress-Strain Curve of Concrete,” Cement and Concrete Research, V. 3, No. 5, 1973, pp. 583-599. doi: 10.1016/0008-8846(73)90096-3

25. Imran, I., and Pantazopoulou, S. J., “Experimental Study Plan of Plain Concrete under Triaxial Stress,” ACI Materials Journal, V. 93, No. 6, Nov.-Dec. 1996, pp. 589-601.

26. Sheikh, S. A., and Uzumeri, S. M., “Strength and Ductility of Tied Concrete Columns,” Journal of the Structural Division, ASCE, V. 106, No. 5, 1980, pp. 1079-1102.

27. Bažant, Z. P., and Xiang, Y., “Size Effect in Compression Fracture: Splitting Crack Band Propagation,” Journal of Engineering Mechanics, ASCE, V. 123, No. 2, 1997, pp. 162-172. doi: 10.1061/(ASCE)0733-9399(1997)123:2(162)


ALSO AVAILABLE IN:

Electronic Structural Journal