Performance-Based Damage States of Shape Memory Alloy (SMA) Reinforced Concrete Bridge Piers

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Performance-Based Damage States of Shape Memory Alloy (SMA) Reinforced Concrete Bridge Piers

Author(s): Shahria Alam

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/18/2016

Abstract:
ACI Committee 341, “Earthquake-Resistant Concrete Bridges,” will be sponsoring a session on the seismic performance evaluation, design, and retrofitting of concrete bridges by using advanced materials such as shape memory alloy (SMA) in the form of reinforcing bar, wire, or strand; ultra-high-strength metals; ultra-high-performance cement composites; and nanosilica. The main objective of this session is to present results from recent research studies (experimental/numerical/analytical) and practical examples of application of advanced materials in reinforced concrete (RC) bridge piers, bents, or full bridges. This session is for practitioners, educators, and researchers.