Comparative Study of Concrete Panels’ Fire Resistance

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Comparative Study of Concrete Panels’ Fire Resistance

Author(s): A. Gil, F. Pacheco, R. Christ, F. Bolina, K. H. Khayat, and B. Tutikian

Publication: Materials Journal

Volume: 114

Issue: 5

Appears on pages(s): 755-762

Keywords: concrete panels; concrete spalling; fire safety; polypropylene microfibers; precast concrete panels; prestressed concrete

DOI: 10.14359/51689715

Date: 9/1/2017

Abstract:
There is still a concern regarding concrete structures’ fire safety, mostly due to the occurrence of concrete spalling. Although many tests have already been carried out, there is no clear definition about the parameters of the factors that influence its occurrence. This paper aimed to compare three different types of concrete panels, with dimensions of 300 x 315 x 10 cm (124.0 x 39.4 x 3.9 in.), composed of reinforced concrete (RC), prestressed concrete, and polypropylene microfiber RC. The panels were exposed to the standard fire curve based on ISO 834, aged 28 days, measuring the temperatures in panels’ surfaces. Prestressed concrete panels experienced explosive spalling 18 minutes after the test began. RC panels and the panels with polypropylene microfiber addition maintained their integrity and structural stability for 240 minutes, failing in the thermal insulation criteria at 210 and 140 minutes, respectively. Although polypropylene microfiber concrete panels presented no spalling of concrete, conventional concrete panels attended the standardized criteria for a longer period due to its better thermal insulation.

Related References:

1. International Association of Fire and Rescue Services, “World Fire Statistics,” Center of Fire Statistics, CTIF, No. 20, 2015, 63 pp.

2. Mehta, P. K., and Monteiro, P. J., Concrete: Microstructure, Properties, and Materials, McGraw-Hill Professional Publishing, New York, 2014, 704 pp.

3. Fédération Internationale du Betón, (fib), “Fire Design of Concrete Structures—Materials, Structures and Modeling – State-of-Art Report,” Bulletin d’information No. 38, Lausanne, Switzerland, 2007, 97 pp.

4. Fédération Internationale du Betón (fib), “Fire Design of Concrete Structures—Structural Behavior and Assessment – State-of-Art Report,” Bulletin d’information No. 46, Lausanne, Switzerland, 2008, 209 pp.

5. European Committee for Standardization (CEN), “Eurocode 2: Design of Concrete Structures—Part 1-2: General Rules—Structural Fire Design (EN 1992-1),” Brussels, Belgium, 2004, 100 pp.

6. ACI Committee 216, “Guide for Determining Fire Endurance of Concrete Elements (ACI 216R-89),” American Concrete Institute, Farmington Hills, MI, 1989, 48 pp.

7. Khoury, G. A., “Passive Fire Protection of Concrete Structures,” Proceedings of the Institution of Civil Engineers. Structures and Buildings, V. 161, No. 3, 2008, pp. 135-145. doi: 10.1680/stbu.2008.161.3.135

8. Ren, R., and Naito, C. J., “Precast Concrete Diaphragm Connector Performance Database,” Journal of Structural Engineering, ASCE, V. 139, No. 1, 2013, pp. 15-27. doi: 10.1061/(ASCE)ST.1943-541X.0000598

9. Robinson, G., “Design and Performance of Precast Concrete Structures,” doctoral dissertation, Centre for Innovative and Collaborative Construction Engineering, Loughborough University, Loughborough, UK, 175 pp.

10. International Organization for Standardization (ISO), “Fire-Resistance Tests—Elements of Building Construction—Part 1: General Requirements (ISO 834),” Geneva, Switzerland, 1991, 53 pp.

11. Zago, C. S.; Moreno, A. L. Jr.; and Marin, M. C., “Considerações sobre o desempenho de estruturas de concreto pré-moldado em situação de incêndio,” Ambiente Construído, V. 15, No. 1, 2015, pp. 49-61. doi: 10.1590/S1678-86212015000100006

12. European Committee for Standardization (CEN), “Fire Classification of Construction Products and Building Elements—Classification Using Data from Fire Resistance Tests, Excluding Ventilation Services (EN 13501-2),” Brussels, Belgium, 2004, 84 pp.

13. Gustaferro, A. H., and Martin, L. D., “Design for Fire Resistance of Precast Prestressed Concrete (MNL-124-89),” second edition, Prestressed Concrete Institute, Chicago, IL, 1989, 85 pp.

14. Prestressed Concrete Institute (PCI), “Fire Resistance of Architectural Precast Concrete Envelopes (DN-31),” Chicago, IL, 2011, pp. 46-56.

15. Buchanan, A. H., Structural Design for Fire Safety, Wiley, New York, 2001, 444 pp.

16. Jansson, R., “Fire Spalling of Concrete: Theoretical and Experimental Studies,” doctoral thesis, Vetenskap Och Konst, Stockholm, Sweden, 2013, 134 pp.

17. Zhang, H. L., and Davie, C. T., “A Numerical Investigation of the Influence of Pore Pressure and Thermally Induced Stresses for Spalling of Concrete Exposed to Elevated Temperatures,” Fire Safety Journal, V. 59, 2013, pp. 102-110. doi: 10.1016/j.firesaf.2013.03.019

18. Mindeguia, J. C.; Carré, H.; Pimienta, P.; and Borderie, C. L., “Experimental Discussion on the Mechanisms Behind the Fire Spalling of Concrete,” Fire and Materials, V. 39, No. 7, 2014, pp. 619-635.

19. Ali, F., “Is High Strength Concrete More Susceptible to Explosive Spalling than Normal Strength Concrete in Fire?” Fire and Materials, V. 26, No. 3, 2002, pp. 127-130. doi: 10.1002/fam.791

20. Heo, Y.; Han, C.; and Kim, K., “Combined Fiber Technique for Spalling Protection of Concrete Column, Slab and Beam in Fire,” Materials and Structures, V. 48, No. 10, 2015, pp. 3377-3390. doi: 10.1617/s11527-014-0406-4

21. Kalifa, P.; Chéné, G.; and Galle, C., “High-Temperature Behaviour of HPC with Polypropylene Fibers—From Spalling to Microstructure,” Cement and Concrete Research, V. 31, No. 10, 2001, pp. 1487-1499. doi: 10.1016/S0008-8846(01)00596-8

22. Associação Brasileira de Normas Técnicas (ABNT), “Paredes Divisórias sem Função Estrutural—Determinação da Resistência ao Fogo: Método de Ensaio (NBR 10636),” Rio de Janeiro, Brazil, 1989, 7 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal