Sustainable production using precast concrete: Precast Concrete & the Challenge of Carbon Footprinting

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Sustainable production using precast concrete: Precast Concrete & the Challenge of Carbon Footprinting

Author(s): Andrew Minson and Hafiz Elhag

Publication: Institute of Concrete Technology

Volume:

Issue:

Appears on pages(s): 6 pages

Keywords:

DOI:

Date: 1/1/2017

Abstract:
Since the Precast Sustainability Charter scheme was introduced in 2007, the precast sector has come a long way in addressing its embodied environmental impacts and emissions. There has been a recent policy shift in the UK and Europe towards construction products’ environmental footprinting and embodied carbon; this will require the precast sector to look again at how it can address the future challenges of its own footprint. This paper reports on the progress made with the Precast Sustainability Charter between 2008 and 2014 and then reports on the main challenges associated with the carbon footprint of precast concrete.


Institute of Concrete Technology, International Partner Access

View Resource »