Structural Responses of External Post-Tensioned Tendons to Increasing Localized Damage

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Structural Responses of External Post-Tensioned Tendons to Increasing Localized Damage

Author(s): Jun Ki Lee

Publication: Structural Journal

Volume: 114

Issue: 5

Appears on pages(s): 1155-1166

Keywords: bridges; corrosion; damage; post-tensioning; stress redistribution; tendon

DOI: 10.14359/51689679

Date: 9/1/2017

Abstract:
This paper presents an experimental investigation of the structural effect of moderate to severe levels of localized damage in external post-tensioned tendons. Eight large-scale specimens with multiple seven-wire strands were fabricated, and the wires in the strands were consecutively fractured until a severe level of damage was identified using three controlled methods: accelerated galvanic corrosion, fatigue loading, and direct exposure to an acid solution. During this process, the structural effects induced by the applied damage were monitored based on visual inspection, acoustic sensors, transverse displacement, and vibration signals, depending on the experimental conditions. Experimental results showed that the behaviors of the damaged specimens were continuously governed by the residual tensile force, which was appreciably redistributed after wire fracture(s) in the strands, especially when the level of damage was moderate. As a result, the rate of decrement in the structural response became larger as the level of damage increased; however, they were not as sensitively influenced relative to the level of applied damage.

Related References:

1. Virlogeux, M. P., “External Prestressing: From Construction History to Modern Technique and Technology,” External Prestressing in Bridges, SP-120, American Concrete Institute, Farmington Hills, MI, 1990, pp. 1-60.

2. Bruggeling, A. S. G., “External Prestressing: A State of the Art,” External Prestressing in Bridges, SP-120, American Concrete Institute, Farmington Hills, MI, 1990, pp. 61-82.

3. Poston, R. W.; Frank, K. H.; and West, J. S., “Enduring Strength,” Civil Engineering (New York, N.Y.), V. 73, No. 9, Sept. 2003, pp. 58-63.

4. Podolny, W., “Corrosion of Prestressing Steels and Its Mitigation,” PCI Journal, V. 37, No. 5, 1992, pp. 34-55. doi: 10.15554/pcij.09011992.34.55

5. Woodard, R. J., “Collapse of a Segmental Post-Tensioned Concrete Bridge,” Transportation Research Record 1211, Transportation Research Board, National Research Council, Washington, DC, 1989, pp. 38-59.

6. ACI Committee 222, “Corrosion of Prestressing Steels (ACI 222.2R-01),” American Concrete Institute, Farmington Hills, MI, 2001, 42 pp.

7. Corven Engineering, “Mid-Bay Bridge Post-Tensioning Evaluation,” Final Report to Florida Department of Transportation, 2001.

8. Cavell, D. G., and Waldron, P., “A Residual Strength Model for Deteriorating Post-Tensioned Concrete Bridge,” Computers & Structures, V. 79, No. 4, 2001, pp. 361-373. doi: 10.1016/S0045-7949(00)00150-4

9. Coronelli, D.; Castel, A.; Vu, N. A.; and François, R., “Corroded Post-Tensioned Beams with Bonded Tendons and Wire Failure,” Engineering Structures, V. 31, No. 8, 2009, pp. 1687-1697. doi: 10.1016/j.engstruct.2009.02.043

10. Lee, J., “Evaluation of External Post-Tensioned Tendon using Vibration Signatures,” PhD dissertation, University of Texas at Austin, Austin, TX, 2007.

11. McKinstry, C. A., “Frequency Response of Damaged External Post-Tensioned Tendons,” MS thesis, University of Texas at Austin, Austin, TX, 2010.

12. Wood, S. L.; McKinstry, C. A.; and Lee, J., “Residual Tensile Capacity of Grouted, Post-Tensioned Tendons,” ACI Structural Journal, V. 110, No. 6, Nov.-Dec. 2013, pp. 1099-1107.

13. Irvine, M. H., Cable Structures, Dover Publications, Mineola, New York, 1981, pp. 42-46.

14. Fang, Z., and Wang, J., “Practical Formula for Cable Tension Estimation by Vibration Method,” Journal of Bridge Engineering, ASCE, V. 17, No. 1, 2012, pp. 161-164. doi: 10.1061/(ASCE)BE.1943-5592.0000200

15. Zui, H.; Shinke, T.; and Namita, Y., “Practical Formulas for Estimation of Cable Tension by Vibration Method,” Journal of Structural Engineering, ASCE, V. 122, No. 6, 1996, pp. 651-656. doi: 10.1061/(ASCE)0733-9445(1996)122:6(651)

16. ASTM A416/A416M-10, “Standard Specification for Steel Strand, Uncoated Seven-Wire for Prestressed Concrete,” ASTM International, West Conshohocken, PA, 2010, 5 pp.

17. ASTM C942-10, “Standard Test Method for Compressive Strength of Grouts for Preplaced-Aggregate Concrete in the Laboratory,” ASTM International, West Conshohocken, PA, 2010, 3 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal