Disc. 113-M15/From the March-April 2016 ACI Materials Journal, p. 151

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Disc. 113-M15/From the March-April 2016 ACI Materials Journal, p. 151

Author(s): Chao Jiang and Xiang-Lin Gu

Publication: Materials Journal

Volume: 114

Issue: 1

Appears on pages(s): 185-186

Keywords:

DOI:

Date: 1/1/2017

Abstract:
Disc. 113-M15/From the March-April 2016 ACI Materials Journal, p. 151 Analysis of Compressive Strength Development and Carbonation Depth of High-Volume Fly Ash Cement Pastes. Paper by Xiao-Yong Wang and Ki-Bong Park