Title: ACI Concrete Sustainability Forum IX

Author(s): Koji Sakai and Julie K. Buffenbarger

Publication: Concrete International

Volume: 39

Issue: 2

Appears on pages(s): 27-31

Keywords: carbon, cement, building, environment

DOI: 10.14359/51689634

Date: 2/1/2017

Abstract:
ACI Concrete Sustainability Forum IX took place in October 2016 at the ACI Concrete Convention and Exposition. The forum featured presentations from seven experts on sustainability design, sustainability assessment systems, and new material technologies for sustainable buildings and civil engineering structures.

Related References:

1. Sakai, K., and Sordyl, D., “ACI St. Louis Workshop on Sustainability,”Concrete International, V. 31, No. 2, Feb. 2009, pp. 34-38.

2. Sakai, K.; Buffenbarger, J.K.; and Stehly, R.D., “Concrete Sustainability Forum,” Concrete International, V. 32, No. 3, Mar. 2010, pp. 56-59.

3. Sakai, K., and Buffenbarger, J.K., “Concrete Sustainability Forum III,” Concrete International, V. 33, No. 3, Mar. 2011, pp. 37-40.

4. Sakai, K., and Buffenbarger, J.K., “Concrete Sustainability Forum IV,” Concrete International, V. 34, No. 3, Mar. 2012, pp. 41-44.

5. Sakai, K., and Buffenbarger, J.K., “Concrete Sustainability Forum V,” Concrete International, V. 35, No. 4, Apr. 2013, pp. 45-49.

6. Sakai, K., and Buffenbarger, J.K., “Concrete Sustainability Forum VI,” Concrete International, V. 36, No. 3, Mar. 2014, pp. 55-58.

7. Sakai, K., and Buffenbarger, J.K., “Concrete Sustainability Forum VII,” Concrete International, V. 37, No. 3, Mar. 2015, pp. 55-58.

8. Sakai, K., and Buffenbarger, J.K., “Concrete Sustainability Forum VIII,” Concrete International, V. 38, No. 4, Apr. 2016, pp. 72-76.

9. International Federation for Structural Concrete, “fib Model Code for Concrete Structures 2010,” Ernst & Sohn, Berlin, Germany, 2013, 402 pp.

10. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

11. ISO/TC 71/SC 8, “Environmental Management for Concrete and Concrete Structures—Part 1: General Principles (ISO 13315-1:2012),” International Organization for Standardization, Geneva, Switzerland, 2012.

12. ISO/TC 71/SC 8, “Environmental Management for Concrete and Concrete Structures—Part 2: System Boundary and Inventory Data (ISO 13315-2:2014),” International Organization for Standardization, Geneva, Switzerland, 2014.

13. Institute for Sustainable Infrastructure, https://sustainableinfrastructure.org/.

14. Scrivener, K.L; John, V.M.; and Gartner, E.M., Eco-efficient Cements: Potential, Economically Viable Solutions for a Low-CO2, Cement Based Materials Industry, United Nations Environment Program, 2016, 50 pp.

15. The Paris Agreement, http://unfccc.int/paris_agreement/items/9485.php.