Title: Guide to Shotcrete

Author(s): Lars Balck

Publication: Concrete International

Volume: 39

Issue: 2

Appears on pages(s): 35-37

Keywords: gunite, specification, strength, testing

DOI: 10.14359/51689631

Date: 2/1/2017

Abstract:
This article is a reprint of a paper that originally appeared in the Summer 2016 issue of Shotcrete. It discusses updates to “Guide to Shotcrete (ACI 506R-16),” including new and expanded sections.

Related References:

1. Rodriquez, L., From Elephants to Swimming Pools: Carl Akeley, Samuel W. Taylor, and the Development of the Cement Gun, Canal History and Technology Press, Easton, PA, 2006, 150 pp.

2. ACI Committee 506, “Specification for Shotcrete (ACI 506.2-13),”American Concrete Institute, Farmington Hills, MI, 2013, 12 pp.

3. ACI Committee 117, “Specification for Tolerances for Concrete Construction and Materials (ACI 117-10) and Commentary (ACI 117R-10) (Reapproved 2015),” American Concrete Institute, Farmington Hills, MI, 2010, 76 pp.

4. ACI Committee 506, “Guide to Shotcrete (ACI 506R-16),” American Concrete Institute, Farmington Hills, MI, 2016, 52 pp.