Bond Strength in Multilayer Casting of Self-Consolidating Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bond Strength in Multilayer Casting of Self-Consolidating Concrete

Author(s): Wael A. Megid and Kamal H. Khayat

Publication: Materials Journal

Volume: 114

Issue: 3

Appears on pages(s): 467-476

Keywords: bond strength; fold lines; lift lines; multilayer casting; rheology; self-consolidating concrete; structural buildup at rest; thixotropy

DOI: 10.14359/51689597

Date: 5/1/2017

Abstract:
Multilayer casting of self-consolidating concrete (SCC) can be critical in situations involving casting of successive lifts. The increase in structural buildup at rest of freshly cast SCC material prior to the placement of a successive layer can result in lift lines and loss in interlayer bond strength. Delay in the casting of successive lifts without mechanical consolidation can further reduce bond. Eight SCC mixtures designed to develop different levels of structural buildup at rest were investigated. The structural buildup at rest was determined by multiplying the values of initial slump flow, T50, or J-ring flow by average rates of change in these properties with rest time. Bond between successive layers was determined using composite specimens cast with two lifts of SCC after rest periods of 17 to 52 minutes, which corresponds to 25 to 60 minutes of concrete age. Bond strength was determined using the slant shear and direct shear test setups. Compared to monolithically cast samples, composite specimens had residual bond strengths of 15 to 100%. The critical delay time to secure at least a 90% residual bond strength was found to vary between 5 and 55 minutes, depending on the structural buildup at rest of the concrete in the existing layer. Statistical models for predicting residual bond strength between successive lifts were established and account for the structural buildup at rest of the first lift and delay period between successive lifts. Based on the level of structural buildup at rest, three categories of SCC are proposed. Category III SCC with relatively low structural buildup at rest can develop high residual interlayer bond. Such concrete should have maximum slump flow filling ability index of 800 mm.mm/min (31.5 in.in./min), T50 viscosity index of 0.08 sec.sec/min, and J-ring passing ability index of 600 mm.mm/min (23.6 in.in./min).

Related References:

1. Assaad, J.; Khayat, K. H.; and Mesbah, H., “Influence of Thixotropy on Formwork Pressure of Flowable and Self-Consolidating Concrete—Laboratory Tests,” ACI Materials Journal, V. 100, No. 1, Jan.-Feb. 2003, pp. 29-37.

2. Assaad, J., and Khayat, K. H., “Variations of Lateral and Pore Water Pressure of Self-Consolidating Concrete at Early Age,” ACI Materials Journal, V. 101, No. 4, July-Aug. 2004, pp. 310-317.

3. Khayat, K. H.; Saric-Coric, M.; and Liotta, F., “Influence of Thixotropy on Stability Characteristics of Cement Grout and Concrete,” ACI Materials Journal, V. 99, No. 3, May-June 2002, pp. 234-241.

4. Billberg, P. H.; Roussel, N.; Amziane, S.; Beitzel, M.; Charitou, G.; Freund, B.; Gardner, J. N.; Grampeix, G.; Graubner, C.-A.; Keller, L.; Khayat, K. H.; Lange, D. A.; Omran, A. F.; Perrot, A.; Proske, T.; Quattrociocchi, R.; and Vanhove, Y., “Field Evaluation of Models for Predicting Lateral Form Pressure Exerted by SCC,” Cement and Concrete Composites, V. 54, Nov. 2014, pp. 70-79. doi: 10.1016/j.cemconcomp.2014.02.003

5. Assaad, J., and Khayat, K. H., “Effect of Viscosity-Enhancing Admixtures on Formwork Pressure and Thixotropy of Self-Consolidating Concrete,” ACI Materials Journal, V. 103, No. 4, July-Aug. 2006, pp. 280-287.

6. Roussel, N., “A Thixotropic Model for Fresh Fluid Concretes: Theory, Validation and Applications,” Cement and Concrete Research, V. 36, No. 10, 2006, pp. 1797-1806. doi: 10.1016/j.cemconres.2006.05.025

7. Roussel, N., and Cussigh, F., “Distinct-Layer Casting of SCC: The Mechanical Consequences of Thixotropy,” Cement and Concrete Research, V. 38, No. 5, 2008, pp. 624-632. doi: 10.1016/j.cemconres.2007.09.023

8. Khayat, K. H.; Omran, A.; and Megid, W. A., “Evaluation of Thixotropy of Self-Consolidating Concrete and Influence on Concrete Performance,” 3rd Iberian Congress on Self-Compacting Concrete, Progress and Opportunities, Dec. 3-4, 2012, Madrid, Spain.

9. Vikan, H., “Quality of Concrete Surfaces: State of the Art,” SINTEF Building and Infrastructure, SINTEF Report, Sept. 2007, Norway.

10. Momayz, A., Ramezanianpour, A., Rajaie, H., and Ehsani, M., “Bi-Surface Shear Test for Evaluation Bond between Existing and New Concrete,” ACI Materials Journal, V. 101, No. 2, Mar.-Apr. 2004, pp. 99-106.

11. Trejo, D.; Hueste, M. B.; Kim, Y. H.; and Atahan, H., “Characterization of Self-Consolidating Concrete for Design of Precast, Prestressed Bridge Girders,” Report No. FHWA/TX-09/0-5134-2, Texas Transportation Institute, The Texas A&M University System, College Station, TX, Dec. 2008.

12. ASTM C882-99, “Standard Test Method for Bond Strength of Epoxy Resin Systems Used with Concrete by Slant Shear,” ASTM International, West Conshohocken, PA, 1999, 4 pp.

13. BS 6319-3, “Testing of Resin and Polymer/Cement Compositions for Use in Construction. Methods for Measurement of Modulus of Elasticity in Flexure and Flexural strength,” British Standards Institution, London,UK, Dec. 1990.

14. Lange, D., “Roadware 10-Minute Concrete Mender: Evaluation of Bond Strength,” Department of Civil Engineering, University of Illinois at Urbana-Champaign, Urbana, IL, Dec. 2001.

15. Bao, W.; Chen, X.; Wang, H.; and Zhou, C., “Shear Strength and Shear Failure of Layered Machinable Ti3AlC2 Ceramics,” Journal of the European Ceramic Society, V. 24, No. 5, 2004, pp. 855-860. doi: 10.1016/S0955-2219(03)00328-5

16. Fehervari, S.; Galos, M.; and Nehme, G., “Determination of KIIC Stress Intensity Factor of New Shape Concrete Specimens,” Concrete Structure, Annual Technical Journal, V. 11, 2010, pp. 53-60.

17. Aysha, H.; Ramsundar, K. R.; Arun, M.; and Velrajkumar, G., “An Overview of Interface Behavior between Concrete to Concrete,” International Journal of Advanced Structures and Geotechnical Engineering, V. 3, No. 02, Apr. 2014.

18. Khayat, K. H.; Omran, A.; Naji, S.; Billberg, P.; and Yahia, A., “Field-Oriented Test Methods to Evaluate Structural Build-up at Rest of Flowable Mortar and Concrete,” Materials and Structures Journal, V. 45, No. 10, 2012, pp. 1547-1564. doi: 10.1617/s11527-012-9856-8

19. Omran, A. F.; Naji, S.; and Khayat, K. H., “Portable Vane Test to Assess Structural Build-up at Rest of Self-Consolidating Concrete,” ACI Materials Journal, V. 108, No. 6, Nov.-Dec. 2011, pp. 628-637.

20. Khayat, K. H.; Omran, A. F.; and Pavate, T. V., “Inclined Plane Test Method to Determine Structural Build-Up at Rest of Self-Consolidating Concrete,” ACI Materials Journal, V. 107, No. 5, Sept.-Oct. 2010, pp. 515-522.


ALSO AVAILABLE IN:

Electronic Materials Journal