Compliance of Self-Consolidating Concrete for Prestressed Applications

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compliance of Self-Consolidating Concrete for Prestressed Applications

Author(s): Anton K. Schindler, Robert W. Barnes, Jonas Kammoe Kamgang, and Bryan Kavanaugh

Publication: Materials Journal

Volume: 114

Issue: 2

Appears on pages(s): 273-283

Keywords: accelerated curing; creep; loading ages; prediction methods; shrinkage

DOI: 10.14359/51689594

Date: 3/1/2017

Abstract:
Estimating the time-dependent behavior of self-consolidating concrete (SCC) is essential for its successful use in prestressed concrete applications. Compliance is the total load-induced strain (elastic and creep strain) at any age per unit stress caused by a sustained applied load. Compliance of SCC is compared to that of conventional-slump concrete (CSC). Four SCC and one CSC mixtures were made under controlled laboratory conditions and tested under sustained load applied at either 18 hours, 2 days, 7 days, 28 days, or 90 days. All SCC mixtures cured under elevated or standard laboratory temperatures exhibited compliance values less than or similar to the CSC mixture. The accuracy of six compliance prediction methods was also investigated. The compliance prediction accuracy achieved for SCC is similar to that for CSC. The CEB 2010 model was the most accurate compliance prediction method regardless of concrete type or curing condition.

Related References:

1. ACI Committee 237, “Self-Consolidating Concrete (ACI 237R-07),” American Concrete Institute, Farmington Hills, MI, 2007, 30 pp.

2. ACI Committee 209, “Guide for Modeling and Calculating Shrinkage and Creep in Hardened Concrete (ACI 209.2R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 44 pp.

3. Schindler, A. K.; Barnes, R. W.; Roberts, J. B.; and Rodriguez, S., “Properties of Self-Consolidating Concrete for Prestressed Members,” ACI Materials Journal, V. 104, No. 1, Jan.-Feb. 2007, pp. 53-61.

4. Neville, A. M., Properties of Concrete, fourth edition, John Wiley & Sons, Inc., New York, 1996, 844 pp.

5. Mindess, S.; Young, J. F.; and Darwin, D., Concrete, second edition, Prentice Hall, Upper Saddle River, NJ, 2003, 644 pp.

6. Long, W. J., and Khayat, K. H., “Creep of Prestressed Self-Consolidating Concrete,” ACI Materials Journal, V. 108, No. 5, Sept.-Oct. 2011, pp. 476-484.

7. Kim, Y. H.; Trejo, D.; Hueste, M. B. D.; and Kim, J. J., “Experimental Study on Creep and Durability of High-Early-Strength Self-Consolidating Concrete for Precast Elements,” ACI Materials Journal, V. 108, No. 2, Mar.-Apr. 2011, pp. 128-138.

8. AASHTO, “AASHTO LRFD Bridge Design Specifications,” sixth edition, American Association of State Highway and Transportation Officials, Washington, DC, 2012, 1672 pp.

9. Khayat, H. K., and Mitchell, D., “Self-Consolidating Concrete for Precast, Prestressed Concrete Bridge Elements,” NCHRP Report 628, Washington, DC, 2009, 99 pp.

10. fib, “Creep and Shrinkage,” Model Code 2010: First Complete Draft, fédération internationale du béton (fib), Lausanne, Switzerland, 2010, 292 pp.

11. ASTM C1074, “Standard Practice for Estimating Concrete Strength by the Maturity Method,” ASTM International, West Conshohocken, PA, 2011, 8 pp.

12. Bažant, Z. P., and Baweja, S., “Description of Model B3 and Prediction Procedure,” The Adam Neville Symposium: Creep and Shrinkage— Structural Design Effects, SP-194, A. Al-Manaseer, ed., American Concrete Institute, Farmington Hills, MI, 2000, pp. 1-100.

13. Kavanaugh, B. P., “Creep Behavior of Self-Consolidating Concrete,” MS thesis, Auburn University, Auburn, AL, 2008, 209 pp.

14. AASHTO M 43, “Sizes of Aggregate for Road and Bridge Construction,” American Association of State Highway and Transportation Officials, Washington, DC, 2003, 3 pp.

15. ASTM C1611, “Standard Test Method for Slump Flow of Self-Consolidating Concrete,” ASTM International, West Conshohocken, PA, 2006, 6 pp.

16. AASHTO T 126, “Making and Curing Concrete Test Specimens in the Laboratory,” American Association of State Highway and Transportation Officials, Washington, DC, 2003, 13 pp.

17. ASTM C512, “Standard Test for Creep in Concrete in Compression,” ASTM International, West Conshohocken, PA, 2006, 5 pp.

18. Gardner, N. J., and Lockman, M. J., “Design Provisions for Drying Shrinkage and Creep of Normal-Strength Concrete,” ACI Materials Journal, V. 98, No. 2, Mar.-Apr. 2001, pp. 159-167.

19. McCuen, R. H., Statistical Methods for Engineers, Prentice Hall, Inc., Lebanon, IN, 1985, 439 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal