Title: Performance of SCC Made with Limestone Fillers

Author(s): Kamal H. Khayat

Publication: Web Session

Volume: ws_2017_0123_Khayat_PSCCMLF.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 11/10/2015

Abstract:
This session will introduce the new document developed by ACI Subcommittee 211-N, “Guide to Proportioning Concrete Mixtures with Ground Limestone and Other Mineral Fillers,” and provide case studies for ground limestone and mineral filler.