Failure Envelope of Circular Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars and Spirals

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Failure Envelope of Circular Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars and Spirals

Author(s): Abdeldayem Hadhood, Hamdy M. Mohamed, and Brahim Benmokrane

Publication: Structural Journal

Volume: 114

Issue: 6

Appears on pages(s): 1417-1428

Keywords: circular; column; eccentricity; fiber-reinforced polymer; interaction diagram

DOI: 10.14359/51689498

Date: 11/1/2017

Abstract:
This paper presents the results of an experimental investigation on the eccentric behavior of 10 circular concrete columns reinforced with glass fiber-reinforced polymer (GFRP) bars and spirals. The columns measured 1500 mm (60 in.) in length and 305 mm (12 in.) in diameter. The test variables were the eccentricity-to-diameter ratio and the longitudinal reinforcement ratio. The columns were subjected to predesigned different levels of eccentricities to develop the failure envelope (axial load-moment interaction diagram). Compression failure due to concrete crushing controlled the ultimate capacity of specimens tested under low eccentric loading. Flexural-tension failure initiated in specimens tested under high eccentric loading, however, resulted from large axial and lateral deformations and cracks on the tension side until a secondary compression failure occurred due to the strain limitations in concrete and degradation of the concrete compressive block. The axial force-moment interaction diagrams were predicted based on the principles of strain compatibility and internal force equilibrium, and following the recommendations of the available design standards/guidelines and recent research work on GFRP-reinforced concrete (RC) columns. The analysis results revealed that ignoring the contribution of GFRP bars in compression conservatively underestimated the axial flexural capacity of test specimens.