Formwork Pressure of Self-Consolidating Concrete Containing Recycled Coarse Aggregates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Formwork Pressure of Self-Consolidating Concrete Containing Recycled Coarse Aggregates

Author(s): Joseph J. Assaad and Jacques Harb

Publication: Materials Journal

Volume: 114

Issue: 3

Appears on pages(s): 491-500

Keywords: formwork pressure; recycled aggregates; self-consolidating concrete (SCC); thixotropy

DOI: 10.14359/51689494

Date: 5/1/2017

Abstract:
The successful use of highly flowable self-consolidating concrete (SCC) containing recycled concrete aggregate (RCA) in structural applications entails proper assessment of lateral pressure developed on vertical formworks. Three series of relatively low to high stable SCC mixtures were considered in this paper; the virgin aggregates were substituted by 25, 50, 75, and 100% RCA. Regardless of SCC composition, test results have shown that mixtures prepared with increased RCA replacement levels led to reduced initial pressure measured after placement, as well as accelerated rates of pressure drop over time. The former phenomenon was related to higher RCA surface roughness that increases internal friction, while the latter was attributed to higher water absorption that improves concrete stability. A series of regression models based on thixotropy and relative water absorption of aggregates were developed to predict the effect of RCA on SCC formwork pressure.

Related References:

1. Etxeberria, M.; Mari, A. R.; and Vazquez, A. E., “Recycled Aggregate Concrete as Structural Material,” Materials and Structures, V. 40, No. 5, 2007, pp. 529-541. doi: 10.1617/s11527-006-9161-5

2. Ajdukiewicz, A. B., and Kliszczewicz, A. T., “Comparative Tests of Beams and Columns Made of Recycled Aggregate Concrete and Natural Aggregate Concrete,” Journal of Advanced Concrete Technology, V. 5, No. 2, 2007, pp. 259-273. doi: 10.3151/jact.5.259

3. Fathifazl, G.; Razaqpur, A. G.; Isgor, O. B.; Abbas, A.; Fournier, B.; and Foo, S., “Shear Capacity Evaluation of Steel Reinforced Recycled Concrete (RRC) Beams,” Engineering Structures, V. 33, No. 3, 2011, pp. 1025-1033. doi: 10.1016/j.engstruct.2010.12.025

4. Assaad, J. J., and Daou, Y., “Behavior of Structural Polymer-Modified Concrete Containing Recycled Aggregates,” Journal of Adhesion Science and Technology, V. 31, No. 8, 2017, doi: 10.1080/01694243.2016.1235750

5. Fakitsas, C. G.; Papakonstantinou, P. E. A.; Kiousis, P. D.; and Savva, A., “Effects of Recycled Concrete Aggregates on the Compressive and Shear Strength of High-Strength Self-Consolidating Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 4, 2012, pp. 356-361. doi: 10.1061/(ASCE)MT.1943-5533.0000397

6. Grdic, Z. J.; Curcic, G. A.; Despotovic, I. M.; and Ristic, N. S., “Properties of Self-Compacting Concrete Prepared with Coarse Recycled Concrete Aggregate,” Construction and Building Materials, V. 24, No. 7, 2010, pp. 1129-1133. doi: 10.1016/j.conbuildmat.2009.12.029

7. Yang, K. H.; Chung, H. S.; and Ashour, A. F., “Influence of Type and Replacement Level of Recycled Aggregates on Concrete Properties,” ACI Materials Journal, V. 105, No. 3, May-June 2008, pp. 289-296.

8. Poon, C. S.; Kou, C. S.; and Lam, L., “Influence of Recycled Aggregate on Slump and Bleeding of Fresh Concrete,” Materials and Structures, V. 40, No. 9, 2007, pp. 981-988. doi: 10.1617/s11527-006-9192-y

9. Assaad, J. J., and Khayat, K. H., “Effect of Coarse Aggregate Characteristics on Lateral Pressure Exerted by Self-Consolidating Concrete,” ACI Materials Journal, V. 102, No. 3, May-June 2005, pp. 145-153.

10. Roussel, N., “Rheology of Fresh Concrete: From Measurements to Predictions of Casting Processes,” Materials and Structures, V. 40, No. 10, 2007, pp. 1001-1012. doi: 10.1617/s11527-007-9313-2

11. Gallego, E.; Fuentes, J. M.; Ramírez, A.; and Ayuga, F., “Computer Simulation of Complex-Shaped Formworks Using Three-Dimensional Numerical Models,” Automation in Construction, V. 20, No. 7, 2011, pp. 830-836. doi: 10.1016/j.autcon.2011.03.001

12. Assaad, J. J., “Correlating Thixotropy of Self-Consolidating Concrete to Stability, Formwork Pressure, and Multilayer Casting,” Journal of Materials in Civil Engineering, ASCE, V. 28, No. 10, 2016, 10.1061/(ASCE)MT.1943-5533.0001624

13. Assaad, J. J., and Khayat, K. H., “Kinetics of Formwork Pressure Drop of Self-Consolidating Concrete Containing Various Types and Contents of Binder,” Cement and Concrete Research, V. 35, No. 8, 2005, pp. 1522-1530. doi: 10.1016/j.cemconres.2004.12.005

14. Assaad, J. J., and Khayat, K. H., “Effect of Viscosity-Enhancing Admixtures on Formwork Pressure and Thixotropy of Self-Consolidating Concrete,” ACI Materials Journal, V. 103, No. 4, July-Aug. 2006, pp. 280-287.

15. Wallevik, J. E., “Rheological Properties of Cement Paste: Thixotropic Behavior and Structural Breakdown,” Cement and Concrete Research, V. 39, No. 1, 2009, pp. 14-29. doi: 10.1016/j.cemconres.2008.10.001

16. Abbas, A.; Fathifazl, G.; Isgor, O. B.; Razaqpur, A.; Fournier, B.; and Foo, S., “Proposed Method for Determining the Residual Mortar Content of Recycled Concrete Aggregates,” Journal of ASTM International, V. 5, 2008, pp. 1-10.

17. BS 812-110, “Testing Aggregates,” British Standards Institute, London, UK, 1990, 18 pp.

18. Khayat, K. H.; Assaad, J. J.; and Daczko, J., “Comparison of Field-Oriented Test Methods to Assess Dynamic Stability of Self-Consolidating Concrete,” ACI Materials Journal, V. 101, No. 2, Mar.-Apr. 2004, pp. 168-176.

19. EPG, “The European Guidelines for Self-Compacting Concrete Specification Production and Use,” May 2005, http://www.efnarc.org/pdf/SCCGuidelinesMay2005.pdf.

20. Nguyen, Q. D., and Boger, D. V., “Direct Yield Stress Measurement with the Vane Method,” Journal of Rheology, V. 29, No. 3, 1985, pp. 335-347. doi: 10.1122/1.549794

21. Assaad, J. J.; Harb, J.; and Maalouf, Y., “Effect of Vane Configuration on Yield Stress Measurements of Cement Pastes,” Journal of Non-Newtonian Fluid Mechanics, V. 230, 2016, pp. 31-42. doi: 10.1016/j.jnnfm.2016.01.002

22. Gardner, N. J., “Pressure of Concrete on Formwork—A Review,” Journal Proceedings of Civil Engineering (New York, N.Y.), V. 82, No. 1, 1985, pp. 744-753.

23. Khayat, K. H., and Assaad, J. J., “Measurement Systems for Determining Formwork Pressure of Highly Flowable Concrete,” Materials and Structures, V. 41, No. 1, 2007, pp. 37-46. doi: 10.1617/s11527-006-9216-7


ALSO AVAILABLE IN:

Electronic Materials Journal