Method to Calculate Cement Content in Hardened Concrete Based on Theory of Carbonization

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Method to Calculate Cement Content in Hardened Concrete Based on Theory of Carbonization

Author(s): Yue Li, Wei Guo, and Hong Li

Publication: Materials Journal

Volume: 114

Issue: 2

Appears on pages(s): 245-251

Keywords: carbonation depth; carbonation model; cement content; hardened concrete

DOI: 10.14359/51689491

Date: 3/1/2017

Abstract:
Once concrete is set and hardened, it is very hard to evaluate its primitive composition once again. Currently, the conditions required for testing of original cement content in the hardened concrete are severe; the test is complicated, and the test precision is hard to be guaranteed. To explore a convenient and easy method to calculate the cement content in the hardened concrete, in this test, concrete of different mixture proportions was prepared and the carbonation depth of concrete at different curing ages was tested. Based on formulas in references and experimental results, a method to determinate the cement content in hardened concrete via carbonization depth was put forward, in which many influences such as CO2 concentration are taken into consideration. The result shows that the feasibility of this method is good, which can provide a certain reference for practical engineering.

Related References:

1. Haha, M. B.; De Weerdt, K.; and Lothenbach, B., “Quantification of the Degree of Reaction of Fly Ash,” Cement and Concrete Research, V. 40, No. 11, 2010, pp. 1620-1629. doi: 10.1016/j.cemconres.2010.07.004

2. Kocaba, V.; Gallucci, E.; and Scrivener, K., “Methods for Determination of Degree of Reaction of Slag in Blended Cement Pastes,” Cement and Concrete Research, V. 42, No. 3, 2012, pp. 511-525. doi: 10.1016/j.cemconres.2011.11.010

3. Linares, L.; López-Atalaya, M.; and Chinchón, S., “Cement Content Determination through Selective Stain in Hardened Concrete,” Cement and Concrete Research, V. 39, No. 11, 2009, pp. 1105-1109. doi: 10.1016/j.cemconres.2009.07.016

4. Wong, H. S.; Matter, K.; and Buenfeld, N. R., “Estimating the Original Cement Content and Water-Cement Ratio of Portland Cement Concrete and Mortar using Backscattered Electron Microscopy,” Magazine of Concrete Research, V. 65, No. 11, 2013, pp. 693-706. doi: 10.1680/macr.12.00201

5. Wong, H. S., and Buenfeld, N. R., “Determining the Water-Cement Ratio, Cement Content, Water Content and Degree of Hydration of Hardened Cement Paste: Method Development and Validation on Paste Samples,” Cement and Concrete Research, V. 39, No. 10, 2009, pp. 957-965. doi: 10.1016/j.cemconres.2009.06.013

6. NDIS 3422:2002, “Detection of Unit Cement Content in Hardened Concrete by Sodium Gluconate,” Japanese Society for Non-Destructive Inspection, Tokyo, Japan. (in Japanese)

7. ASTM C1084-02, “Standard Test Method for Portland Cement Content of Hardened Hydraulic-Cement,” ASTM International, West Conshohocken, PA, 2002, 6 pp.

8. BS 1881-124:1988, “Testing Concrete. Methods for Analysis of Hardened Concrete,” British Standards Institution, London, UK, 24 pp.

9. Huang, H.; Qian, C.; Zhao, F.; Qu, J.; Guo, J.; and Danzinger, M., “Improvement on Microstructure of Concrete by Polycarboxylate Superplasticizer (PCE) and its Influence on Durability of Concrete,” Construction and Building Materials, V. 110, No. 9, 2016, pp. 293-299. doi: 10.1016/j.conbuildmat.2016.02.041

10. Harrison, T., “Durability and Sustainable Concrete,” Magazine of Concrete Research, V. 68, No. 9, 2016, pp. 433-434. doi: 10.1680/jmacr.2016.68.9.433

11. Ramezanianpour, A. M.; Esmaeili, K.; Ghahari, S. A.; and Ramezanianpour, A. A., “Influence of Initial Steam Curing and Different Types of Mineral Additives on Mechanical and Durability Properties of Self-Compacting Concrete,” Construction and Building Materials, V. 73, 2014, pp. 187-194. doi: 10.1016/j.conbuildmat.2014.09.072

12. Gesoglu, M.; Guneyisi, E.; Nahhab, A. H.; and Yazıcı, H., “The Effect of Aggregates with High Gypsum Content on the Performance of Ultra-High Strength Concretes and Portland Cement Mortars,” Construction and Building Materials, V. 110, 2016, pp. 346-354. doi: 10.1016/j.conbuildmat.2016.02.045

13. Jiang, L., and Zhang, Y., “Concrete Carbonation Depth Calculation and Test Research,” Ready-Mixed Concrete, V. 4, 1996, pp. 12-18. (in Chinese)


ALSO AVAILABLE IN: