Title: Self-Consolidating Concrete in Virginia Department of Transportation’s Bridge Structures

Author(s): Gail M. Moruza and H. Celik Ozyildirim

Publication: Materials Journal

Volume: 114

Issue: 1

Appears on pages(s): 57-64

Keywords: consolidation; lightweight self-consolidating concrete; permeability; placement; self-consolidating concrete (SCC); shrinkage; slump flow; strength

DOI: 10.14359/51689480

Date: 1/1/2017

Abstract:
The Virginia Department of Transportation (VDOT) incorporates innovative materials into its concrete structures to ensure durable and cost-effective infrastructure. However, poor consolidation can reduce the durability of VDOT concrete structures because it leads to unacceptable amounts of voids in hardened concrete that increase its permeability and reduces its strength. Self-consolidating concrete (SCC) that has high flow rates and the ability to move through congested reinforcement is a new addition to VDOT concretes; it facilitates placement, minimizes consolidation problems, and improves structure longevity. This paper summarizes VDOT’s use of SCC in bridge structures both in precast and castin-place applications. In precast applications, beams were fabricated with normalweight and lightweight SCC. In cast-in-place applications, drilled shafts, pier caps, and substructure repairs were cast with normalweight SCC. Summaries of field applications by VDOT as well as lessons learned through implementation are included in the paper.

Related References:

1. ACI Committee 309, “Guide for Consolidation of Concrete (ACI 309R-05),” American Concrete Institute, Farmington Hills, MI, 2005, 36 pp.

2. Ozyildirim, C., “Lightweight High-Performance Concrete Bulb-T Beams with Self-Consolidating Concrete in a Bridge Structure,” VCTIR 14-R15, Virginia Center for Transportation Innovation and Research, Charlottesville, VA, 2014.

3. Ozyildirim, C., “Consolidation Concerns Continue,” Concrete International, V. 29, No. 9, Sept. 2005, pp. 43-45.

4. Ozyildirim, C., and Moruza, G., “Using Self-Consolidating Concrete for Bridge Repairs,” Concrete International, V. 37, No. 4, Apr. 2015, pp. 42-46.

5. Lane, S., “Evaluation of Consolidation in Concrete Pavements,” Technical Assistance Report, Virginia Transportation Research Council, Charlottesville, VA, 1994.

6. ACI Committee 237, “Self-Consolidating Concrete (ACI 237R-07), American Concrete Institute, Farmington Hills, MI, 2007, 30 pp.

7. NDOT, “Evaluation of Self-Consolidating Concrete (SCC) for Use in North Dakota Transportation Projects,” June 2010.

8. Okamura, H., and Ouchi, M., “Self-Compacting Concrete,” Journal of Advanced Concrete Technology, V. 1, No. 1, 2003, pp. 5-15. doi: 10.3151/jact.1.5

9. Ozyildirim, C., “Virginia Department of Transportation Early Experience with Self-Consolidating Concrete,” TRR 1914, Concrete Materials 2005, Transportation Research Board, Washington, DC, 2005, pp. 81-84.

10. Ozyildirim, C., and Sharp, S., “Evaluation of Drilled Shafts with Self-Consolidating Concrete,” TRR 2342, Concrete Materials 2013, Transportation Research Board, Washington, DC, 2013, pp. 35-41.

11. Ozyildirim, C., and Moruza, G., “Redefining High-Performance Concrete,” Concrete International, V. 36, No. 10, Oct. 2014, pp. 37-42.

12. Ozyildirim, C., and Moruza, G., “Bridge Beams and Pier Caps with Self-Consolidating Concrete at Nimmo Parkway,” Virginia Transportation Research Council, Charlottesville, VA, 2016.

13. Ozyildirim, C., “Bulb-T Beams with Self-Consolidating Concrete on the Route 33 Bridge over the Pamunkey River in Virginia,” VTRC 09-R5, Virginia Center for Transportation and Research, Charlottesville, VA, 2008.

14. Ozyildirim, C., and Davis, R. T., “Bulb-T Beams with Self-Consolidating Concrete on Route 33 in Virginia,” Journal of the Transportation Research Board, No. 2020, 2007, pp. 76-82.

15. Dymond, B.; Roberts-Wollman, C.; and Cousins, T., “Shear Strength of a PCBT-53 Girder Fabricated with Lightweight, Self-Consolidating Concrete,” VTRC 09-CR11, Virginia Transportation Research Council, Charlottesville, VA, 2009.

16. ASTM C1202-12, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2012, 8 pp.

17. Ozyildirim, C., “Permeability Specifications for High-Performance Concrete Decks,” Journal of the Transportation Research Board, No. 1610, 1998, pp. 1-5.


ALSO AVAILABLE IN:

Electronic Materials Journal