Concrete Damage under Fatigue Loading in Uniaxial Compression

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Damage under Fatigue Loading in Uniaxial Compression

Author(s): Benard Isojeh, Maria El-Zeghayar, and Frank J. Vecchio

Publication: Materials Journal

Volume: 114

Issue: 2

Appears on pages(s): 225-235

Keywords: compressive strength; damage; fatigue; fatigue secant modulus; residual concrete strength; strain evolution; variable loading

DOI: 10.14359/51689477

Date: 3/1/2017

Abstract:
Despite rigorous efforts in the derivation of various fatigue damage models for concrete, damage predictions of sufficient accuracy are still limited to loading conditions similar to those of the experiments used for developing the models. Most models are void of salient factors affecting the fatigue behavior of concrete such as frequency, stress ratio, and loading waveform, and the approaches used in developing such models tend to be rudimentary. Therefore, further investigation is required. In this study, damage models are expressed for residual concrete strength and fatigue secant modulus using experimental data from tested cylindrical specimens, a damage function, and a stress-life model in the literature. The number of cycles leading to failure, required for normalizing the fatigue cycles for each specimen, is obtained using a proposed secondary strain rate model. The aforementioned influencing factors incorporated into the damage function result in robust models that account for variations in loading parameters.

Related References:

1. Shah, S. P., “Predictions of Cumulative Damage for Concrete and Reinforced Concrete,” Materiales de Construcción, V. 17, No. 1, 1984, pp. 65-68. doi: 10.1007/BF02474059

2. Torrenti, J. M.; Pijaudier-Cabot, G.; and Reynouard, J.-M., eds., Mechanical Behaviour of Concrete, John Wiley & Sons, Inc., 2010, pp. 185-223.

3. Papa, E., and Taliercio, A., “Anisotropic Damage Model for the Multiaxial Static and Fatigue Behaviour of Plain Concrete,” Engineering Fracture Mechanics, V. 55, No. 2, 1996, pp. 163-179. doi: 10.1016/0013-7944(96)00004-5

4. Vega, I. M.; Bhatti, M. A.; and Nixon, W. A., “A Nonlinear Fatigue Damage Model for Concrete in Tension,” International Journal of Damage Mechanics, V. 4, No. 4, 1995, pp. 362-379. doi: 10.1177/105678959500400404

5. Taliercio, A. L. F., and Gobbi, E., “Experimental Investigation on the Triaxial Fatigue Behaviour of Plain Concrete,” Magazine of Concrete Research, V. 48, No. 176, 1996, pp. 157-172. doi: 10.1680/macr.1996.48.176.157

6. Song, Y.-P.; Cao, W.; and Meng, X., “Fatigue Properties of Plain Concrete under Triaxial Constant-Amplitude Tension-Compression Cyclic Loading,” Journal of Shanghai University, V. 9, No. 2, 2005, pp. 127-133. doi: 10.1007/s11741-005-0064-4

7. Tamulenas, V.; Gelazius, V.; and Ramanauskas, R., “Calculation Technique for Stress-Strain Analysis of RC Elements Subjected to High-Cyclic Compression,” Civil and Transport Engineering, Aviation Technologies, V. 6, No. 5, 2014, pp. 468-473. doi: 10.3846/mla.2014.687

8. Aas-Jacobsen, K., “Fatigue of Concrete Beams and Columns,” Bulletin No. 70-1, Institutt for Betonkonstruksjoner, Trondheim, Norway, 1970, 148 pp.

9. Murdock, J. W., and Kesler, C. E., “Effects of Range of Stress on Fatigue Strength of Plain Concrete Beams,” ACI Journal Proceedings, V. 55, No. 2, 1955, pp. 221-231.

10. Hilsdorf, H. K., and Kesler, C. E., “Fatigue Strength of Concrete under Varying Flexural Stresses,” ACI Journal Proceedings, V. 63, No. 10, Oct. 1966, pp. 1059-1076.

11. Awad, M. E., and Hilsdorf, H. K., “Strength and Deformation Characteristics of Plain Concrete Subjected to High Repeated and Sustained Loads,” Civil Engineering Studies, Structural Research Series No. 372, University of Illinois, Champaign, IL, 1971.

12. Oh, B. H., “Cumulative Damage Theory of Concrete under Variable-Amplitude Fatigue Loadings,” ACI Materials Journal, V. 88, No. 2, Mar.-Apr. 1991, pp. 122-128.

13. Ople, F. S., and Hulsbos, C. L., “Probable Fatigue Life of Plain Concrete with Stress Gradient,” ACI Journal Proceedings, V. 63, No. 1, Jan. 1966, pp. 59-82.

14. Graf, O., and Brenner, E., “Experiments for Investigating the Resistance of Concrete under often Repeated Compressive Loads 2,” Bulletin No. 83, Deutscher Ausschuss fur Eisenbeton, 1936.

15. Sparks, P. R., and Menzies, J. B., “The Effect of Rate of Loading upon the Static and Fatigue Strength of Plain Concrete in Compression,” Magazine of Concrete Research, V. 25, No. 83, 1973, pp. 73-80. doi: 10.1680/macr.1973.25.83.73

16. Raithby, K. D., and Galloway, J. W., “Effect of Moisture Condition, Age, and Rate of Loading on Fatigue of Plain Concrete,” Fatigue of Concrete, SP-41, American Concrete Institute, Farmington Hills, MI, 1974, pp. 15-34.

17. Holmen, J. O., “Fatigue of Concrete by Constant and Variable Amplitude Loading,” Fatigue of Concrete Structures, SP-75, American Concrete Institute, Farmington Hills, MI, 1982, pp. 71-110.

18. Naik, T. R.; Singh, S. S.; and Ye, C., “Fatigue Behaviour of Plain Concrete Made with or without Fly Ash,” Centre for By-Products Utilization, Department of Civil Engineering & Mechanics, University of Wisconsin-Milwaukee, Milwaukee, WI, 1993.

19. Zhang, B.; Phillips, D. V.; and Wu, K., “Effects of Loading Frequency and Stress Reversal on Fatigue Life of Plain Concrete,” Magazine of Concrete Research, V. 48, No. 177, 1996, pp. 361-375. doi: 10.1680/macr.1996.48.177.361

20. Takhar, S. S.; Jordaan, I. J.; and Gamble, B. R., “Fatigue of Concrete under Lateral Confining Pressure,” Fatigue of Concrete, SP-41, American Concrete Institute, Farmington Hills, MI, 1974, pp. 59-70.

21. RILEM COMMITTEE 36-RDL, “Long Term Random Dynamic Loading of Concrete Structures,” Materials and Structures, V. 17, 1984, pp. 1-28.

22. Hsu, T. C., “Fatigue and Micro-Cracking of Concrete,” Materiales de Construcción, V. 17, No. 1, 1984, pp. 51-54. doi: 10.1007/BF02474056

23. Hooi, T., “Effects of Passive Confinement on Fatigue Properties of Concrete,” Magazine of Concrete Research, V. 52, No. 1, 2000, pp. 7-15. doi: 10.1680/macr.2000.52.1.7

24. Lee, M. K., and Barr, B. I. G., “An Overview of the Fatigue Behaviour of Plain and Fibre Reinforced Concrete,” Cement and Concrete Composites, V. 26, No. 4, 2004, pp. 299-305. doi: 10.1016/S0958-9465(02)00139-7

25. Gebreyouhannes, E.; Kishi, T.; and Maekawa, K., “Shear Fatigue Response of Cracked Concrete Interface,” Journal of Advanced Concrete Technology, V. 6, No. 2, 2008, pp. 365-376. doi: 10.3151/jact.6.365

26. Cook, D. J., and Chindaprasirt, P., “Influence of Loading History upon the Compressive Properties of Concrete,” Magazine of Concrete Research, V. 32, No. 111, 1980, pp. 89-100. doi: 10.1680/macr.1980.32.111.89

27. Cook, D. J., and Chindaprasirt, P., “Influence of Loading History upon the Tensile Properties of Concrete,” Magazine of Concrete Research, V. 33, No. 116, 1981, pp. 154-160. doi: 10.1680/macr.1981.33.116.154

28. Cornelissen, H. A. W., and Reinhardt, H. W., “Effect of Static and Fatigue Preloading on Residual Strength and Stiffness of Plain Concrete,” Fracture Control of Engineering Structures (ECF 6), 1987.

29. Zhang, B., and Wu, K., “Residual Fatigue Strength and Stiffness of Ordinary Concrete under Bending,” Cement and Concrete Research, V. 27, No. 1, 1997, pp. 115-126. doi: 10.1016/S0008-8846(96)00183-4

30. CEB, “Fatigue of Concrete Structures—State of-the-Art-Report,” Bulletin No. 188, International Federation for Structural Concrete (fib), Lausanne, Switzerland, 1988, 312 pp.

31. fib Model Code, 2010, “fib Model Code for Concrete Structures,” John Wiley & Sons, 2013, 434 pp.

32. Lohaus, L.; Oneschkow, N.; and Wefer, M., “Design Model for the Fatigue Behaviour of Normal-Strength, High-Strength and Ultra-High-Strength Concrete,” Structural Concrete, V. 13, No. 3, 2012, pp. 182-192. doi: 10.1002/suco.201100054

33. Schaff, J. R., and Davidson, B. D., “Life Prediction Methodology for Composite Structures. Part 1- Constant Amplitude and Two-Stress Level Fatigue,” Journal of Composite Materials, V. 31, No. 2, 1997, pp. 128-157. doi: 10.1177/002199839703100202

34. Zhu, H., and Li, X., “Experimental Research on Residual Strength of Recycled Aggregate Concrete under Compressive Fatigue Loading,” Advanced Materials Research, V. 150-151, 2010, pp. 1379-1382. doi: 10.4028/www.scientific.net/AMR.150-151.1379

35. Van Paepegem, W., and Degrieck, J., “A New Coupled Approach of Residual Stiffness and Strength for Fatigue of Fibre-Reinforced Composites,” International Journal of Fatigue, V. 24, No. 7, 2002, pp. 747-762. doi: 10.1016/S0142-1123(01)00194-3

36. Shah, S. P., and Chandra, S., “Fracture of Concrete Subjected to Cyclic and Sustained Loading,” ACI Journal Proceedings, V. 67, No. 10, Oct. 1970, pp. 816-827.

37. Gao, L., and Hsu, T. T. C., “Fatigue of Concrete Under Uniaxial Compression Cyclic Loading,” ACI Materials Journal, V. 95, No. 5, Sept.-Oct. 1998, pp. 575-580.

38. Zhang, B.; Phillips, D. V.; and Green, D. R., “Sustained Loading Effect on the Fatigue Life of Plain Concrete,” Magazine of Concrete Research, V. 50, No. 3, 1998, pp. 263-278. doi: 10.1680/macr.1998.50.3.263

39. Oneschkow, N., “Influence of Loading Frequency on the Fatigue Behaviour of High-Strength Concrete,” Proceedings of the 9th fib International PhD Symposium in Civil Engineering, Karlsruhe, Germany, 2012.

40. Edalatmanesh, R., and Newhook, J. P., “Residual Strength of Precast Steel-Free Panels,” ACI Structural Journal, V. 110, No. 5, Sept.-Oct. 2013, pp. 715-722.

41. Miner, M. A., “Cumulative Damage in Fatigue,” Journal of Applied Mechanics, V. 12, No. 3, 1945, pp. A159-A164.

42. Palmgren, A., “Die Lebensdauer von Kugellagern,” Zeitschrift des Vereines Deutcher Ingenieure, V. 68, 1924, pp. 339-341. (VDI Zeitschrift)

43. Thun, H.; Ohlsson, U.; and Elfgren, L., “A Deformation Criterion for Fatigue of Concrete in Tension,” Structural Concrete, V. 12, No. 3, 2011, pp. 187-197. doi: 10.1002/suco.201100013


ALSO AVAILABLE IN: