Generic Model Stress-Strain Relationship for Concrete in Compression at Elevated Temperatures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Generic Model Stress-Strain Relationship for Concrete in Compression at Elevated Temperatures

Author(s): Martin Neuenschwander, Markus Knobloch, and Mario Fontana

Publication: Materials Journal

Volume: 114

Issue: 1

Appears on pages(s): 3-14

Keywords: constitutive modeling; cyclic compression tests at elevated temperatures; elastic stiffness degradation; fire resistance; high temperature properties; mechanical properties

DOI: 10.14359/51689468

Date: 1/1/2017

Abstract:
This paper presents a generic uniaxial constitutive model of the complete stress-strain curve of concrete in compression, adaptable to elevated temperatures solely by temperature-dependent material parameters. The pre-peak regime is divided into an initial linear part until the point of first yielding and a subsequent nonlinear part, starting with a tangent slope equal to the elastic modulus. The post-peak regime is split into two parts by the inflection point of the descending branch and ends at a predefined degree of softening. Additionally, elastic stiffness degradation is considered in the post-peak regime. First, analytical expressions for the different parts are derived and then the model is validated against experimental data of normal-strength concrete and self-consolidating concrete at elevated temperatures, including data from specimens heated under sustained loading. Finally, the model performance is discussed with respect to existing models in the literature and to the available design code models.

Related References:

1. Schneider, U., “Concrete at High Temperatures—A General Review,” Fire Safety Journal, V. 13, No. 1, 1988, pp. 55-68. doi: 10.1016/0379-7112(88)90033-1

2. Khoury, G. A., “Compressive Strength of Concrete at High Temperatures: A Reassessment,” Magazine of Concrete Research, V. 44, No. 161, Dec. 1992, pp. 291-309. doi: 10.1680/macr.1992.44.161.291

3. Schneider, U., and Haksever, A., “Determination of the Equivalent Fire Duration of Statically Determined Reinforced Concrete Beams in Natural Fires,” Bericht des Instituts für Baustoffkunde und Stahlbetonbau der Technischen Universität Braunschweig, Germany, 1976. (in German)

4. RILEM Technical Committee 44-PHT, “Properties of Materials at High Temperatures: Concrete,” U. Schneider, ed., Department of Civil Engineering, Kassel, Germany, 1985, pp. 97-98.

5. ASCE, “Structural Fire Protection,” ASCE Manuals and Reports on Engineering Practice No. 78, T. T. Lie, ed., ASCE Committee on Fire Protection, Structural Division, American Society of Civil Engineers, New York, 1992, pp. 199-201.

6. EN 1992-1-2, “Eurocode 2: Design of Concrete Structures. Part 1-2: General Rules—Structural Fire Design,” CEN European Committee for Standardization, Brussels, Belgium, 2008.

7. Anderberg, Y., and Thelandersson, S., “Stress and Deformation Characteristics of Concrete at High Temperatures—2. Experimental Investigation and Material Behaviour Model,” Division of Structural Mechanics and Concrete Construction, Bulletin 54, Lund Institute of Technology, Lund, Sweden, 1976.

8. Khennane, A., and Baker, G., “Uniaxial Model for Concrete under Variable Temperature and Stress,” Journal of Engineering Mechanics, ASCE, V. 119, No. 8, 1993, pp. 1507-1525. doi: 10.1061/(ASCE)0733-9399(1993)119:8(1507)

9. Terro, M. J., “Numerical Modeling of the Behavior of Concrete Structures in Fire,” ACI Structural Journal, V. 95, No. 2, Mar.-Apr. 1998, pp. 183-192.

10. Youssef, M. A., and Moftah, M., “General Stress-Strain Relationship for Concrete at Elevated Temperatures,” Engineering Structures, V. 29, No. 10, 2007, pp. 2618-2634. doi: 10.1016/j.engstruct.2007.01.002

11. Lin, F. B.; Bažant, Z. P.; Chern, J. C.; and Marchertas, A. H., “Concrete Model with Normality and Sequential Identification,” Computers & Structures, V. 26, No. 6, 1987, pp. 1011-1025. doi: 10.1016/0045-7949(87)90118-0

12. Neuenschwander, M.; Knobloch, M.; and Fontana, M., “Suitability of the Damage-Plasticity Modelling Concept for Concrete at Elevated Temperatures: Experimental Validation with Uniaxial Cyclic Compression Tests,” Cement and Concrete Research, V. 79, 2016, pp. 57-75. doi: 10.1016/j.cemconres.2015.07.013

13. Bamonte, P., and Gambarova, P. G., “A Study on the Mechanical Properties of Self-Compacting Concrete at High Temperature and after Cooling,” Materials and Structures, V. 45, No. 9, 2012, pp. 1375-1387. doi: 10.1617/s11527-012-9839-9

14. Schneider, U., and Kordina, K., “On the Behaviour of Normal Concrete under Steady State and Transient Temperature Conditions,” 3rd International Conference on Structural Mechanics in Reactor Technology, V. 3, Paper 1/6, Part H, London, UK, Sept. 1-5, 1975.

15. Neuenschwander, M.; Knobloch, M.; and Fontana, M., “ISO Standard Fire Tests of Concrete-Filled Steel Tube Columns with Solid Steel Core,” Journal of Structural Engineering, ASCE, doi:10.1061/(ASCE)ST.1943-541X.0001695.

16. Lie, T. T.; Lin, T. D.; Allen, D. E.; and Abrams, M. S., “Fire Resistance of Reinforced Concrete Columns,” NRC No. 23065, NRC Institute for Research in Construction, National Research Council Canada, Ottawa, ON, Canada, 1984.

17. ASTM E119, “Standard Methods of Fire Tests of Building Construction and Materials,” ASTM International, West Conshohocken, PA, 1985.

18. ISO 834-1, “Fire Resistance Test—Elements of Building Construction – Part 1: General Requirements,” International Organization for Standardization, Geneva, Switzerland, 1999.

19. RILEM Technical Committee 200-HTC, “Recommendation of RILEM TC 200-HTC: Mechanical Concrete Properties at High Temperatures—Modelling and Applications, Part 2: Stress-Strain Relation,” Materials and Structures, V. 40, No. 9, 2007, pp. 855-864. doi: 10.1617/s11527-007-9286-1

20. RILEM Technical Committee 200-HTC, “Recommendation of RILEM TC 200-HTC: Mechanical Concrete Properties at High Temperatures—Modelling and Applications, Part 1: Introduction—General Presentation,” Materials and Structures, V. 40, No. 9, 2007, pp. 841-853. doi: 10.1617/s11527-007-9285-2

21. Popovics, S., “A Numerical Approach to the Complete Stress-Strain Curve of Concrete,” Cement and Concrete Research, V. 3, No. 5, 1973, pp. 583-599. doi: 10.1016/0008-8846(73)90096-3

22. Becker, J. M., and Bresler, B., “Fire-RC-A Computer Program for the Fire Response of Structural-Reinforced Concrete Frames,” Report No. UCB FRG 74-3, Department of Civil Engineering, University of California, Berkeley, Berkeley, CA, 1974.

23. van Mier, J. G. M., Fracture Processes of Concrete: Assessment of Material Parameters for Fracture Models, CRC Press, Boca Raton, FL, 1997, pp. 68-80.

24. Lankard, D. R.; Birkimer, D. L.; Fondriest, F. F.; and Snyder, M. J., “Effects of Moisture Content on the Structural Properties of Portland Cement Concrete Exposed to Temperatures up to 500°F,” Temperature and Concrete, SP-25, American Concrete Institute, Farmington Hills, MI, 1971, pp. 59-102.


ALSO AVAILABLE IN:

Electronic Materials Journal