Pure Mechanics Crack Model for Shear Stress Transfer in Cracked Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pure Mechanics Crack Model for Shear Stress Transfer in Cracked Reinforced Concrete

Author(s): Paolo M. Calvi, Evan C. Bentz, and Michael P. Collins

Publication: Structural Journal

Volume: 114

Issue: 2

Appears on pages(s): 545-554

Keywords: aggregate interlock modeling; crack behavior; cyclic loading; nonlinear response; reinforced concrete; shear strength; structural assessment

DOI: 10.14359/51689460

Date: 3/1/2017

Abstract:
An analytical model is presented that is capable of predicting or assessing the response of cracks in reinforced concrete elements subjected to monotonic, cyclic, or reversed cyclic in-plane shear and normal stresses. The model is formulated in terms of global and local equilibrium, compatibility, and stress-strain relationships. The small number of required empirical parameters are determined from the test results of 14 pre-cracked reinforced concrete panels under uniform shear and uniaxial tensile stresses. The proposed model is shown to capture the important aspects of the response of cracks subjected to complex loading conditions, resulting in improved simulations of crack behavior. In addition, it is shown that the model can be employed to conduct crack-based structural assessments that estimate the stress state of a structure based on crack displacement information collected as part of site-monitoring activities.

Related References:

1. Sherwood, E. G.; Bentz, E. C.; and Collins, M. P., “Effect of Aggregate Size on Beam-Shear Strength of Thick Slabs,” ACI Structural Journal, V. 104, No. 2, Mar.-Apr. 2007, pp. 180-190.

2. Vecchio, F. J., and Collins, M. P., “The Modified Compression Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr. 1986, pp. 219-231.

3. Vecchio, F. J., “Disturbed Stress Field Model for Reinforced Concrete: Formulation,” Journal of Structural Engineering, ASCE, V. 126, No. 9, 2000, pp. 1070-1077. doi: 10.1061/(ASCE)0733-9445(2000)126:9(1070)

4. Calvi, P., M., “A Theory for the Shear Behaviour of Cracks Providing the Basis for the Assessment of Cracked Reinforced Concrete Structures,” PhD dissertation, University of Toronto, Toronto, ON, Canada, 2015, 346 pp.

5. Mattock, A. H., and Hawkins, N. M., “Shear Transfer in Reinforced Concrete—Recent Research,” PCI Journal, V. 17, No. 2, 1972, pp. 55-75. doi: 10.15554/pcij.03011972.55.75

6. Laible, J. P., “An Experimental Investigation of Interface Shear Transfer and Applications in the Dynamic Analysis of Nuclear Containment Vessels,” PhD thesis, Cornell University, Ithaca, NY, 1973, 686 pp.

7. Paulay, T., and Loeber, P. J., “Shear Transfer by Aggregate Interlock,” Shear in Reinforced Concrete, SP-42, American Concrete Institute, Farmington Hills, MI, 1974, pp. 1-15.

8. Bažant, Z. P., and Gambarova, P., “Rough Cracks in Reinforced Concrete,” Journal of the Structural Division, ASCE, V. 106, No. 4, 1979, pp. 819-842.

9. Walraven, J. C., and Reinhardt, H. W., “Theory and Experiments on the Mechanical Behavior of Cracks in Plain and Reinforced Concrete Subjected to Shear Loading,” Heron, V. 26, No. 1A, 1981, 68 pp.

10. Li, B.; Maekawa, K.; and Okamura, H., “Contact Density Model for Stress Transfer Across Cracks in Concrete,” Journal of the Faculty of Engineering, University of Tokyo, V. 40, No. 1, 1989, pp. 9-52.

11. Bujadham, B., and Maekawa, K., “The Universal Model for Stress Transfer Across Cracks in Concrete,” Proceedings of JSCE, V. 17, No. 451, 1992, pp. 277-287.

12. Nagle, T. J., and Kuchma, D. A., “Shear Transfer Resistance in High-Strength Concrete Girders,” Magazine of Concrete Research, V. 59, No. 8, 2007, pp. 611-620. doi: 10.1680/macr.2007.59.8.611

13. Gebreyouhannes, E.; Kishi, T.; and Maekawa, K., “Shear Fatigue Response of Cracked Concrete Interface,” Journal of Advanced Concrete Technology, V. 6, No. 2, 2008, pp. 365-376. doi: 10.3151/jact.6.365

14. Sagaseta, J., and Vollum, R. L., “Influence of Aggregate Fracture on Shear Transfer through Cracks in Reinforced Concrete,” Magazine of Reinforced Concrete Research, V. 63, No. 2, 2011, pp. 119-137. doi: 10.1680/macr.9.00191

15. Calvi, P. M.; Bentz, E. C.; and Collins, M. P., “Reversed Cyclic Experiments on Shear Stress Transfer across Cracks in Reinforced Concrete Elements,” ACI Structural Journal, V. 113, No. 4, July-Aug. 2016, pp. 851-859. doi: 10.14359/51688926

16. Walraven, J. C., “Fundamental Analysis of Aggregate Interlock,” Proceedings, ASCE, V. 107, No. 11, 1981, pp. 2245-2270.


ALSO AVAILABLE IN:

Electronic Structural Journal