Shear Strength Enhancement Mechanisms of Steel Fiber-Reinforced Concrete Slender Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength Enhancement Mechanisms of Steel Fiber-Reinforced Concrete Slender Beams

Author(s): Mohammad Reza Zarrinpour and Shih-Ho Chao

Publication: Structural Journal

Volume: 114

Issue: 3

Appears on pages(s): 729-742

Keywords: dowel action; hooked-end steel fiber; shear strength; steel fiber-reinforced concrete

DOI: 10.14359/51689449

Date: 5/1/2017

Abstract:
An experimental study was conducted to identify the shear-enhancement and failure mechanisms behind the ultimate shear strength of steel fiber-reinforced concrete (SFRC) slender beams by using the full field-deformation-measuring capability of digital image correlation (DIC) technology. A total of 12 large-scale simply supported SFRC and RC beams with an overall height from 12 to 48 in. (305 to 1220 mm) were tested under monotonic point load up to failure. The greater shear strength in SFRC beams originates from the ability of the fiber bridging effect that delays the propagation of the cracks into the compression zone, whose shear strength is enhanced by the compressive stresses induced by the higher load. The slow progression of the cracks keeps the compression zone depth large, thereby enabling it to contribute to a higher shear resistance. In contrast with the traditional assumption for either plain concrete or SFRC beams, where the shear contribution resulting from dowel action is completely neglected, this research clearly shows that the dowel action has an appreciable effect on the ultimate shear strength. Its contribution varies from 10 to 30% when the beam depth increases from 12 to 48 in. (305 to 1220 mm). On the other hand, the compression zone’s contribution decreases from 69 to 36% with the increase in beam depth. In addition, the shear contribution from the fiber bridging effect along the critical shear crack stays approximately unchanged at 20%, irrespective of the beam depth. In this study, the minimum shear strength obtained was in the range of 5√fc′ psi (0.42√fc′ MPa) for the beams with the greatest depth. This indicates that the maximum allowed shear stress limit of 1.5√fc′ psi (0.125√fc′ MPa) specified in ACI 318-14 is on the very conservative side.

Related References:

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 519 pp.

Baumann, H., 1968, “Tests to Study the Dowel Action of the Bending Tension Reinforcement of Reinforced Concrete Beams,” Bericht Nr. 77, Munich Technischen Hochschule.

Bresler, B., and Pister, K. S., 1958, “Strength of Concrete under Combined Stresses,” ACI Journal Proceedings, V. 55, No. 9, Sept., pp. 321-345.

Choi, K. K.; Park, H. G.; and Wight, J. K., 2007, “Shear Strength of Steel Fiber-Reinforced Concrete Beams without Web Reinforcement,” ACI Structural Journal, V. 104, No. 1, Jan.-Feb., pp. 12-21.

Dinh, H. H.; Parra-Montesinos, G. J.; and Wight, J. K., 2010, “Shear Behavior of Steel Fiber Reinforced Concrete Beams without Stirrup Reinforcement,” ACI Structural Journal, V. 107, No. 5, Sept.-Oct., pp. 597-606.

Dinh, H. H.; Parra-Montesinos, G. J.; and Wight, J. K., 2011, “Shear Strength Model for Steel Fiber Reinforced Concrete Beams without Stirrup Reinforcement,” Journal of Structural Engineering, ASCE, V. 137, No. 10, pp. 1039-1051. doi: 10.1061/(ASCE)ST.1943-541X.0000362

Fenwick, R. C., and Paulay, T., 1968, “Mechanisms of Shear Resistance of Concrete Beams,” Journal of the Structural Division, ASCE, V. 94, No. 10, pp. 2325-2350.

Ferguson, P. M.; Breen, J. E.; and Jirsa, J. O., 1988, Reinforced Concrete Fundamentals, fifth edition, John Wiley & Sons, Inc., New York, 768 pp.

Houde, J., and Mirza, M. S., 1974, “A Finite Element Analysis of Shear Strength of Reinforced Concrete Beams,” Shear in Reinforced Concrete, SP-42, American Concrete Institute, Farmington Hills, MI, pp. 103-128.

Joint ASCE-ACI Committee 426, 1973, “The Shear Strength of Reinforced Concrete Members,” Journal of the Structural Division, V. 99, No. 6, pp. 1091-1187.

Kani, M. W.; Huggins, M. W.; and Wittkopp, R. R., 1979, Kani on Shear in Reinforced Concrete, University of Toronto Press, Toronto, ON, Canada, 225 pp.

Kotsovos, M. D., 1988, “Compressive Force Path Concept: Basis for Reinforced Concrete Ultimate Limit State Design,” ACI Structural Journal, V. 85, No. 1, Jan.-Feb., pp. 68-85.

Kotsovos, M. D., and Pavlović, M. N., 1998, Ultimate Limit-State Design of Concrete Structures: A New Approach, Thomas Telford, London, UK, 208 pp.

Lubell, A.; Sherwood, T.; Bentz, E. C.; and Collins, M. P., 2004, “Safe Shear Design of Large, Wide Beams,” Concrete International, V. 26, No. 1, Jan., pp. 66-78.

Minelli, F.; Conforti, A.; Cuenca, E.; and Plizzari, G., 2014, “Are Steel Fibres Able to Mitigate or Eliminate Size Effect in Shear?” Materials and Structures, V. 47, No. 3, pp. 459-473. doi: 10.1617/s11527-013-0072-y

Mobasher, B., 2012, Mechanics of Fiber and Textile Reinforced Cement Composites, CRC Press, Boca Raton, FL, 473 pp.

Muttoni, A., and Fernández Ruiz, M., 2008, “Shear Strength of Members without Transverse Reinforcement as a Function of the Critical Shear Crack Width,” ACI Structural Journal, V. 105, No. 2, Mar.-Apr., pp. 163-172.

Naaman, A. E., 2002, “Toughness, Ductility, Surface Energy and Deflection-Hardening FRC Composites,” Proceedings of the JCI International Workshop on Ductile Fiber Reinforced Cementitious Composites (DRFCC)—Application and Evaluation (DFRCC-2002), Japan Concrete Institute, Tokyo, Japan, pp. 33-57.

Naaman, A. E., and Reinhardt, H. W., 2003, “High Performance Fiber-Reinforced Cement Composites: HPFRCC 4,” RILEM Proceedings Pro 30, RILEM Publications S.A.R.L., pp. 95-113.

Park, P., and Paulay, T., 1975, Reinforced Concrete Structures, John Wiley & Sons, Inc., New York, 769 pp.

Parra-Montesinos, G. J., 2006, “Shear Strength of Beams with Deformed Steel Fibers,” Concrete International, V. 28, No. 11, Nov., pp. 57-66.

Reinhardt, H. W., and Walraven, J. C., 1982, “Cracks in Concrete Subject to Shear,” Journal of the Structural Division, V. 108, pp. 207-224.

Sherwood, E. G., 2008, “One-Way Shear Behavior of Large, Lightly-Reinforced Concrete Beams and Slabs,” PhD dissertation, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 547 pp.

Shoaib, A.; Lubell, A. S.; and Bindiganavile, V. S., 2014, “Size Effect in Shear for Steel Fiber-Reinforced Concrete Members without Stirrups,” ACI Structural Journal, V. 111, No. 5, Sept.-Oct., pp. 1081-1090. doi: 10.14359/51686813

Sneed, L. H., and Ramirez, J. A., 2010, “Influence of Effective Depth on Shear Strength of Concrete Beams: Experimental Study,” ACI Structural Journal, V. 107, No. 5, Sept.-Oct., pp. 554-562.

Untrauer, R. E., and Henry, R. L., 1965, “Influence of Normal Pressure on Bond Strength,” ACI Journal Proceedings, V. 62, No. 5, May, pp. 577-586.

Vecchio, F. J., and Collins, M. P., 1986, “The Modified Compression Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr., pp. 219-231.

Walraven, J. C., 1981, “Fundamental Analysis of Aggregate Interlock,” Journal of the Structural Division, ASCE, V. 108, pp. 2245-2270.

Wight, J. K., and MacGregor, J. G., 2012, Reinforced Concrete: Mechanics and Design, sixth edition, Prentice Hall, Upper Saddle River, NJ, 1168 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal