Modeling of Inexpensive Strengthening Technique for Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling of Inexpensive Strengthening Technique for Reinforced Concrete Beams

Author(s): Usama Ebead and Huda Saeed

Publication: Structural Journal

Volume: 114

Issue: 2

Appears on pages(s): 451-462

Keywords: beams; cementitious materials; direct tensile test; ferrocement; finite element modeling; reinforced concrete; strengthening

DOI: 10.14359/51689444

Date: 3/1/2017

Abstract:
A noble cause motivated the interest to carry out research work on an inexpensive strengthening technique using ferrocement for reinforced concrete beams applicable in developing countries. Ferrocement as an inexpensive strengthening material is suitable for some developing countries where using such a technique offers an optimum strengthening solution for deteriorated structures. The main experimental component of this research work on strengthening reinforced concrete beams has been already published. This paper primarily presents material characterization and finite element models to study the flexural and interfacial types of behavior of ferrocement-strengthened concrete beams. Twenty-seven (27) ferrocement specimens were tested under direct tension to characterize the behavior of the used ferrocement. Special grip attachments have been designed and manufactured to elude local failure at the specimens’ ends. Based on the direct tension test results, a stress-strain relationship has been developed to describe the uniaxial tensile constitutive relation for ferrocement in the finite element models. The interfacial bond behavior between the ferrocement and the concrete is considered in the models by using interface elements. Moreover, a user-defined subroutine for the microplane constitutive law is integrated into the model for the concrete material. Results of the finite element modeling are presented for the ultimate load-carrying capacities, load-deflection history, and stress distributions at the ferrocement/concrete interface. The finite element modeling results have been validated against the published experimental findings and have shown reasonable agreement.

Related References:

1. Paramasivam, P.; Lim, C. T. E.; and Ong, K. C. G., “Strengthening of RC Beams with Ferrocement Laminates,” Cement and Concrete Composites, V. 20, No. 1, 1998, pp. 53-65. doi: 10.1016/S0958-9465(97)00068-1

2. Shannag, M. J., and Al-Ateek, S. A., “Flexural Behavior of Strengthened Concrete Beams with Corroding Reinforcement,” Construction and Building Materials, V. 20, No. 9, 2006, pp. 834-840. doi: 10.1016/j.conbuildmat.2005.01.059

3. Takiguchi, K., and Abdullah, “Shear Strengthening of Reinforced Concrete Columns Using Ferrocement Jacket,” ACI Structural Journal, V. 98, No. 5, Sept.-Oct. 2001, pp. 696-704.

4. Thanoon, W. A.; Yardim, Y.; Jaafar, M. S.; and Noorzaei, J., “Structural Behaviour of Ferrocement-Brick Composite Floor Slab Panel,” Construction and Building Materials, V. 24, No. 11, 2010, pp. 2224-2230. doi: 10.1016/j.conbuildmat.2010.04.034

5. Liao, H. P., and Fang, S. S., “An Experimental Study on Flexural Behavior of Reinforced Concrete Beams Strengthened with High-Performance Ferrocement,” Advanced Materials Research, V. 163-167, 2010, pp. 3772-3776. doi: 10.4028/www.scientific.net/AMR.163-167.3772

6. Haddad, R. H.; Shannag, M. J.; and Moh’d, A., “Repair of Heat-Damaged RC Shallow Beams Using Advanced Composites,” Materials and Structures, V. 41, No. 2, 2008, pp. 287-299. doi: 10.1617/s11527-007-9238-9

7. Zeng, L. H.; Shang, S. P.; and Peng, H., “Nonlinear Analysis of Reinforced Concrete Beam Strengthened with Ferrocement under Secondary Loading,” Advances in Structural Engineering: Theory and Applications, 2006, pp. 470-476.

8. Fahmy, E. H.; Shaheen, Y. B. I.; Abou Zeid, M. N.; and Gaafar, H. M., “Ferrocement Sandwich and Hollow Core Panels for Floor Construction,” Canadian Journal of Civil Engineering, V. 39, No. 12, 2012, pp. 1297-1310. doi: 10.1139/cjce-2011-0016

9. Cheah, C. B., and Ramli, M., “Load Capacity and Crack Development Characteristics of HCWA-DSF High Strength Mortar Ferrocement Panels in Flexure,” Construction and Building Materials, V. 36, 2012, pp. 348-357. doi: 10.1016/j.conbuildmat.2012.05.034

10. Clarke, R. P., “Study of Full-Scale Elements of a Ferrocement Roof System for Caribbean Application,” Construction and Building Materials, V. 24, No. 3, 2010, pp. 221-229. doi: 10.1016/j.conbuildmat.2009.09.003

11. Ahmad, S. F., “Precast Ferrocement Barrel Shell Planks as Low Cost Roof,” Challenges, Opportunities and Solutions in Structural Engineering and Construction, 2010, pp. 645-649.

12. Alnuaimi, A. S.; Hago, A. W.; Al-Jabri, K. S.; and Al-Saidy, A. H., “Investigation on the Flexural Behaviour of Ferrocement Pipes and Roof Panels Subjected to Bending Moment,” Structural Engineering and Mechanics, V. 33, No. 4, 2009, pp. 503-527. doi: 10.12989/sem.2009.33.4.503

13. Alnuaimi, A. S.; Hago, A.; and Al-Jabri, K. S., “Flexural Behaviour of Ferrocement Roof Panels,” High Performance Structures and Materials III, V. 85, 2006, pp. 93-102. doi: 10.2495/HPSM06010

14. Masood, A.; Arif, M.; Akhtar, S.; and Haquie, M., “Performance of Ferrocement Panels in Different Environments,” Cement and Concrete Research, V. 33, No. 4, 2003, pp. 555-562. doi: 10.1016/S0008-8846(02)01003-7

15. Ibrahim, H. M. H., “Shear Capacity of Ferrocement Plates in Flexure,” Engineering Structures, V. 33, No. 5, 2011, pp. 1680-1686. doi: 10.1016/j.engstruct.2011.02.004

16. Moita, G. F.; de Las Casas, E. B.; Mantilla Carrasco, E. V.; and Bonifácio, S. N., “Experimental and Numerical Analysis of Large Ferrocement Water Tanks,” Cement and Concrete Composites, V. 25, No. 2, 2003, pp. 243-251. doi: 10.1016/S0958-9465(02)00014-8

17. Arif, M.; Pankaj, and Kaushik, S. K., “Mechanical Behaviour of Ferrocement Composites: An Experimental Investigation,” Cement and Concrete Composites, V. 21, No. 4, 1999, pp. 301-312. doi: 10.1016/S0958-9465(99)00011-6

18. Ebead, U., “Inexpensive Strengthening Technique for Partially Loaded Reinforced Concrete Beams: Experimental Study,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 10, 2015, p. 04015002 doi: 10.1061/(ASCE)MT.1943-5533.0001249

19. Neale, K. W.; Ebead, U. A.; Abdel Baky, H. M.; Elsayed, W. E.; and Godat, A., “Analysis of the Load-Deformation Behaviour and Debonding for FRP-strengthened Concrete Structures,” Advances in Structural Engineering, V. 9, No. 6, 2006, pp. 751-763. doi: 10.1260/136943306779369437

20. Baky, H. A.; Ebead, U. A.; and Neale, K. W., “Flexural and Interfacial Behavior of FRP-Strengthened Reinforced Concrete Beams,” Journal of Composites for Construction, ASCE, V. 11, No. 6, 2007, pp. 629-639. doi: 10.1061/(ASCE)1090-0268(2007)11:6(629)

21. Ebead, U., and Neale, K., “Mechanics of Fibre-Reinforced Polymer-Concrete Interfaces,” Canadian Journal of Civil Engineering, V. 34, No. 3, 2007, pp. 367-377. doi: 10.1139/l06-107

22. Elsayed, W.; Ebead, U. A.; and Neale, K. W., “Interfacial Behavior and Debonding Failures in FRP-Strengthened Concrete Slabs,” Journal of Composites for Construction, ASCE, V. 11, No. 6, 2007, pp. 619-628. doi: 10.1061/(ASCE)1090-0268(2007)11:6(619)

23. Kotynia, R.; Abdel Baky, H.; Neale, K. W.; and Ebead, U. A., “Flexural Strengthening of RC Beams with Externally Bonded CFRP Systems: Test Results and 3D Nonlinear FE Analysis,” Journal of Composites for Construction, ASCE, V. 12, No. 2, 2008, pp. 190-201. doi: 10.1061/(ASCE)1090-0268(2008)12:2(190)

24. Rabinovitch, O., and Frostig, Y., “Delamination Failure of RC Beams Strengthened with FRP Strips—A Closed-Form High-Order and Fracture Mechanics Approach,” Journal of Engineering Mechanics, ASCE, V. 127, No. 8, 2001, pp. 852-861. doi: 10.1061/(ASCE)0733-9399(2001)127:8(852)

25. Teng, J. et al., “Recent Research on Intermediate Crack-Induced Debonding in FRP-Strengthened RC Beams,” Proceedings of the 4th International Conference on Advanced Composite Materials in Bridges and Structures, Calgary, AB, Canada, 2004, 8 pp.

26. Ebead, U., and Saeed, H., “Modeling of Reinforced Concrete Slabs Strengthened with Fiber-Reinforced Polymer or Steel Plates,” ACI Structural Journal, V. 107, No. 2, Mar.-Apr. 2010, pp. 218-227.

27. Bažant, Z.; Caner, F. C.; Carol, I.; Adley, M. D.; and Akers, S. A., “Microplane Model M4 for Concrete. I: Formulation with Work-Conjugate Deviatoric Stress,” Journal of Engineering Mechanics, ASCE, V. 126, No. 9, 2000, pp. 944-953. doi: 10.1061/(ASCE)0733-9399(2000)126:9(944)

28. Bathe, K. J., ADINA, ADINA R&D, Inc., Watertown, MA, 2005.

29. Caner, F., and Bažant, Z., “Microplane Model M4 for Concrete. II: Algorithm and Calibration,” Journal of Engineering Mechanics, ASCE, V. 126, No. 9, 2000, pp. 954-961. doi: 10.1061/(ASCE)0733-9399(2000)126:9(954)

30. Ghazi, M.; Attard, M.; and Foster, S., “Modelling Triaxial Compression Using the Microplane Formulation for Low Confinement,” Computers & Structures, V. 80, No. 11, 2002, pp. 919-934. doi: 10.1016/S0045-7949(02)00057-3

31. CSA Group, “Design of Concrete Structures (CSA-A23.3),” Canadian Standards Association, Mississauga, ON, Canada, 2004, 214 pp.

32. ACI Committee 549, “Report on Ferrocement (ACI 549R-97),” American Concrete Institute, Farmington Hills, MI, 1997, 26 pp.

33. Pama, R.; Sutharatnachaiyarorn, C.; and Lee, S., “Rigidities and Strength of Ferrocement,” First Australian Conference on Engineering Materials, University of New South Wales, Sydney, Australia, 1974, pp. 287-308.

34. Kent, D. C., and Park, R., “Flexural Members with Confined Concrete,” Journal of the Structural Division, ASCE, V. 97, No. 7, 1971, pp. 1969-1990.

35. Ombres, L., “Analysis of the Bond between Fabric Reinforced Cementitious Mortar (FRCM) Strengthening Systems and Concrete,” Composites. Part B, Engineering, V. 69, 2015, pp. 418-426. doi: 10.1016/j.compositesb.2014.10.027

36. D’Ambrisi, A.; Feo, L.; and Focacci, F., “Experimental Analysis on Bond between PBO-FRCM Strengthening Materials and Concrete,” Composites. Part B, Engineering, V. 44, No. 1, 2013, pp. 524-532. doi: 10.1016/j.compositesb.2012.03.011

37. Bažant, Z. P., and Oh, B. H., “Crack Band Theory for Fracture of Concrete,” Materials and Structures, V. 16, No. 3, 1983, pp. 155-177.

38. Ebead, U., and Saeed, H., “Numerical Modeling of Shear Strengthened Reinforced Concrete Beams Using Different Systems,” Journal of Composites for Construction, ASCE, V. 18, No. 1, 2014, p. 04013031. doi: 10.1061/(ASCE)CC.1943-5614.0000409

39. Ebead, U., and Saeed, H., “Flexural and Interfacial Behavior of Externally Bonded/Mechanically Fastened Fiber-Reinforced Polymer Strengthened Reinforced Concrete Beams,” ACI Structural Journal, V. 111, No. 4, July-Aug. 2014, pp. 741-752. doi: 10.14359/51686628

40. Elsanadedy, H. M.; Almusallam, T. H.; Alsayed, S. H.; and Al-Salloum, Y. A., “Flexural Strengthening of RC Beams Using Textile Reinforced Mortar—Experimental and Numerical Study,” Composite Structures, V. 97, 2013, pp. 40-55. doi: 10.1016/j.compstruct.2012.09.053


ALSO AVAILABLE IN:

Electronic Structural Journal