Plasticity Constitutive Model for Stress-Strain Relationship of Confined Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Plasticity Constitutive Model for Stress-Strain Relationship of Confined Concrete

Author(s): B. Piscesa, M. M. Attard, A. K. Samani, and S. Tangaramvong

Publication: Structural Journal

Volume: 114

Issue: 2

Appears on pages(s): 361-371

Keywords: biaxial compression; confined concrete; plastic dilation rate; plasticity; stress-strain model; triaxial compression

DOI: 10.14359/51689428

Date: 3/1/2017

Abstract:
This paper presents a plasticity constitutive formulation for concrete under uniaxial compression and confinement in triaxial and biaxial compression. The failure surface is derived from a three-parameter loading surface. A new frictional driver is introduced in the loading function to control the failure surface at the peak and residual stress under confinement. In biaxial loading, a procedure to calibrate the out-of-roundness eccentricity is proposed that affects the shape of the failure surface. Both the hardening and softening functions are based on the continuous plastic volumetric strain. The softening function parameter is defined in terms of the plastic volumetric strain at the inflection point of the softening curve. A new flow rule is proposed that is dependent on the plastic dilation rate. Both a constant or nonconstant plastic dilation rate can be used. In this paper, only a constant plastic dilation rate is examined. The accuracy of the proposed approach is validated through comparisons with a number of available experimental results in uniaxial, biaxial, and triaxial loading.

Related References:

1. Papanikolaou, V. K., and Kappos, A. J., “Confinement-Sensitive Plasticity Constitutive Model for Concrete in Triaxial Compression,” International Journal of Solids and Structures, V. 44, No. 21, 2007, pp. 7021-7048. doi: 10.1016/j.ijsolstr.2007.03.022

2. Bao, J.; Long, X.; Tan, K. H.; and Lee, C. K., “A New Generalized Drucker-Prager Flow Rule for Concrete under Compression,” Engineering Structures, V. 56, 2013, pp. 2076-2082. doi: 10.1016/j.engstruct.2013.08.025

3. Attard, M., and Setunge, S., “Stress-Strain Relationship of Confined and Unconfined Concrete,” ACI Materials Journal, V. 93, No. 5, Sept.-Oct. 1996, pp. 432-442.

4. Menetrey, P., and Willam, K., “Triaxial Failure Criterion for Concrete and its Generalization,” ACI Structural Journal, V. 92, No. 3, May-June 1995, pp. 311-318.

5. Červenka, J., and Papanikolaou, V. K., “Three Dimensional Combined Fracture–Plastic Material Model for Concrete,” International Journal of Plasticity, V. 24, No. 12, 2008, pp. 2192-2220. doi: 10.1016/j.ijplas.2008.01.004

6. Richart, F.; Brandtzæg, A.; and Brown R., “A Study of the Failure of Concrete under Combined Compressive Stresses,” University of Illinois Bulletin No. 185, 1928.

7. Jamet, P.; Millard, A.; and Nahas, G., “Triaxial Behaviour of Micro-Concrete Complete Stress-Strain Curves for Confining Pressures Ranging from 0 to 100 MPa,” RILEM-CEB International Conference Concrete under Multiaxial Conditions, V. 1. 1984, pp. 133-140.

8. Smith, S. H.; Willam, K. J.; Gerstle, K. H.; and Sture, S., “Concrete Over the Top, or: Is There Life After Peak?” ACI Materials Journal, V. 86, No. 5, Sept.-Oct. 1989, pp. 491-497.

9. Imran, I., and Pantazopoulou, S., “Experimental Study of Plain Concrete under Triaxial Stress,” ACI Materials Journal, V. 93, No. 6, Nov.-Dec. 1996, pp. 589-601.

10. Ansari, F., and Li, Q., “High-Strength Concrete Subjected to Triaxial Compression,” ACI Materials Journal, V. 95, No. 6, Nov.-Dec. 1998, pp. 747-755.

11. Samani, A., and Attard, M., “A Stress-Strain Model for Uniaxial and Confined Concrete under Compression,” Engineering Structures, V. 41, Aug., 2012, pp. 335-349. doi: 10.1016/j.engstruct.2012.03.027

12. Kupfer, H.; Hilsdorf, H. K.; and Rusch, H., “Behavior of Concrete under Biaxial Stresses,” ACI Journal Proceedings, V. 66, No. 8, Aug. 1969, pp. 656-666.

13. Tasuji, M. E., “Stress-Strain Response and Fracture of Concrete in Biaxial Loading,” ACI Journal Proceedings, V. 75, No. 7, July 1978, pp. 306-312.

14. Lee, S.-K.; Song, Y.-C.; and Han, S.-H., “Biaxial Behavior of Plain Concrete of Nuclear Containment Building,” Nuclear Engineering and Design, V. 227, No. 2, 2004, pp. 143-153. doi: 10.1016/j.nucengdes.2003.09.001

15. He, Z., and Song, Y., “Failure Mode and Constitutive Model of Plain High-Strength High-Performance Concrete under Biaxial Compression after Exposure to High Temperatures,” Guti Lixue Xuebao, V. 21, No. 2, 2008, pp. 149-159.

16. Lokuge, W.; Sanjayan, J.; and Setunge, S., “Stress-Strain Model for Laterally Confined Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 17, No. 6, 2005, pp. 607-616. doi: 10.1061/(ASCE)0899-1561(2005)17:6(607)

17. Samani, A. K., and Attard, M. M., “Lateral Strain Model for Concrete under Compression,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr. 2014, pp. 441-452.

18. Carrazedo, R.; Mirmiran, A.; and de Hanai, J. B., “Plasticity Based Stress-Strain Model for Concrete Confinement,” Engineering Structures, V. 48, 2013, pp. 645-657. doi: 10.1016/j.engstruct.2012.12.014

19. Macari, E. J.; Weihe, S.; and Arduino, P., “Implicit Integration of Elastoplastic Constitutive Models for Frictional Materials with Highly Nonlinear Hardening Functions,” Mechanics of Cohesive-Frictional Materials, V. 2, No. 1, 1997, pp. 1-29. doi: 10.1002/(SICI)1099-1484(199701)2:13.0.CO;2-P

20. Dahl, K. K. B., “Uniaxial Stress-Strain Curves for Normal and High Strength Concrete,” Afdelingen for Bærende Konstruktioner, Danmarks Tekniske Højskole, 1992.

21. Xie, J.; Elwi, A.; and MacGregor, J., “Mechanical Properties of Three High-Strength Concretes Containing Silica Fume,” ACI Materials Journal, V. 92, No. 2, Mar.-Apr. 1995, pp. 135-145.

22. Candappa, D.; Sanjayan, J.; and Setunge, S., “Complete Triaxial Stress-Strain Curves of High-Strength Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 13, No. 3, 2001, pp. 209.-215. doi: 10.1061/(ASCE)0899-1561(2001)13:3(209)


ALSO AVAILABLE IN:

Electronic Structural Journal