Shear Strength of Circular Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer Bars and Spirals

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Circular Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer Bars and Spirals

Author(s): Ahmed H. Ali, Hamdy M. Mohamed, and Brahim Benmokrane

Publication: Structural Journal

Volume: 114

Issue: 1

Appears on pages(s): 39-49

Keywords: circular beams; fiber-reinforced polymer bars; piles; shear load; spirals

DOI: 10.14359/51689423

Date: 1/1/2017

Abstract:
Recent years have witnessed noticeable advances in incorporating shear design provisions for fiber-reinforced polymers (FRPs) into guidelines and standards. These provisions were developed based on experimental work on rectangular concrete members reinforced with FRP bars and bent FRP stirrups. In contrast, no research seems to have investigated circular concrete members reinforced with FRP bars and spirals under shear loads. This paper reports experimental data on the shear strength of concrete beams reinforced with glass FRP (GFRP) bars and spirals. A total of seven full-scale concrete beams with a total length of 3000 mm (118.11 in.) and a diameter of 500 mm (20 in.) were constructed and tested up to failure. The test parameters included the type and ratio of shear reinforcement (spiral diameter and spacing). The test specimens comprised five beams reinforced with sand-coated GFRP bars and spirals, one beam with only longitudinal GFRP bars, and a reference beam reinforced with conventional steel bars and spirals. As designed, the beams failed in shear due to GFRP spiral rupture. The experimental results were compared to current codes and design guidelines. The comparison indicates that the shear capacity of GFRP-reinforced concrete members with circular cross sections may be determined with the approaches developed for rectangular sections, provided that certain modifications are made to take into account the effective shear depth, equivalent breadth, and the mechanical properties and geometry of GFRP spirals.

Related References:

AASHTO, 2012, “AASHTO LRFD Bridge Design Guide Specifications,” sixth edition, American Association of State Highway and Transportation Officials, Washington, DC, pp. 5-63 to 5-64.

ACI Committee 318, 2014, “Building Code Requirements for Structural concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 519 pp.

ACI Committee 440, 2004, “Guide Test Methods for Fiber-Reinforced Polymers (FRPs) for Reinforcing or Strengthening Concrete Structures (ACI 440.3R-04),” American Concrete Institute, Farmington Hills, MI, 23 pp.

ACI Committee 440, 2015, “Guide for the Design and Construction of Concrete Reinforced with FRP Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 84 pp.

Ahmed, E. A.; El-Salakawy, E. F.; and Benmokrane, B., 2010, “Performance Evaluation of Glass Fiber-Reinforced Polymer Shear Reinforcement for Concrete Beams,” ACI Structural Journal, V. 107, No. 1, Jan.-Feb., pp. 53-62.

Bentz, E.; Massam, L.; and Collins, M., 2010, “Shear Strength of Large Concrete Members with FRP Reinforcement,” Journal of Composites for Construction, ASCE, V. 14, No. 6, pp. 637-646. doi: 10.1061/(ASCE)CC.1943-5614.0000108

Clarke, J. L., and Birjandi, F. K., 1993, “The Behaviour of Reinforced Concrete Circular Section in Shear,” The Structural Engineer, V. 71, No. 5, pp. 73-81.

CSA, 2012, “Design and Construction of Building Components with Fiber Reinforced Polymers (CAN/CSA-S806-12),” Canadian Standards Association, Rexdale, ON, Canada, pp. 30-33.

CSA, 2014, “Canadian Highway Bridge Design Code (CAN/CSA-S6-14),” Canadian Standards Association, Rexdale, ON, Canada, pp. 713-751.

El-Sayed, A. K., and Benmokrane, B., 2008, “Evaluation of the New Canadian Highway Bridge Design Code Shear Provisions for Concrete Beams with Fiber-Reinforced Polymer Reinforcement,” Canadian Journal of Civil Engineering, V. 35, No. 6, pp. 609-623. doi: 10.1139/L08-009

Feltham, I., 2004, “Shear in Reinforced Concrete Piles and Circular,” Journal of Structural Engineering, ASCE, V. 84, No. 11, pp. 27-31.

Fico, R.; Prota, A.; and Manfredi, G., 2008, “Assessment of Eurocode-Like Design Equations for the Shear Capacity of FRP RC Members,” Composite Engineering: Part B, V. 39, No. 5, pp. 792-806. doi: 10.1016/j.compositesb.2007.10.007

Jensen, U. G.; Hoang, L. C.; Joergensen, H. B.; and Fabrin, L. S., 2010, “Shear Strength of Heavily Reinforced Concrete Members with Circular Cross-Section,” Journal of Engineering Structures, V. 32, No. 3, pp. 617-626. doi: 10.1016/j.engstruct.2009.11.008

JSCE, 1997, “Recommendation for Design and Construction of Concrete Structures Using Continuous Fiber Reinforcing Materials,” Japan Society of Civil Engineering, Tokyo, Japan, pp. 18-23.

Khalifa, J. U., and Collins, M. P., 1981, “Circular Reinforced Concrete Members Subjected to Shear,” Publication 81-08, Department of Civil Engineering, University of Toronto, ON, Canada, Dec., 103 pp.

Kim, J., and Mander, J., 2005, “Theoretical Shear Strength of Concrete Columns due to Transverse Steel,” Journal of Structural Engineering, ASCE, V. 131, No. 1, pp. 197-199. doi: 10.1061/(ASCE)0733-9445(2005)131:1(197)

MacGregor, J. G., and Wight, J. K., 2005, Reinforced Concrete: Mechanics and Design, fourth edition, Prentice-Hall, Upper Saddle River, NJ.

Merta, I., 2007, “Shear Strength Model of Reinforced Concrete Circular Cross-Section Members,” Structural Engineering, Mechanics and Computing 3, A. Zingoni, ed., Section 22, pp. 1297-1302.

Mohamed, H. M., and Benmokrane, B., 2014, “Design and Performance of Reinforced Concrete Water Chlorination Tank Totally Reinforced with GFRP Bars: Case Study,” Journal of Composites for Construction, ASCE, V. 18, No. 1, p. 05013001 doi: 10.1061/(ASCE)CC.1943-5614.0000429

Orr, J. J.; Darby, A. P.; Ibell, T. J.; Denton, S. R.; and Shave, J. D., 2010, “Shear Design of Circular Concrete Sections Using the Eurocode 2 Truss Model,” The Structural Engineer, V. 88, No. 23-24, pp. 26-33.

Priestley, M.; Verma, R.; and Xiao, Y., 1996, “Seismic Shear Strength of Reinforced Concrete Columns,” Journal of Structural Engineering, ASCE, V. 122, No. 4, pp. 464-467. doi: 10.1061/(ASCE)0733-9445(1996)122:4(464)

Razaqpur, A., and Spadea, S., 2015, “Shear Strength of FRP Reinforced Concrete Members with Stirrups,” Journal of Composites for Construction, ASCE, V. 19, No. 1, p. 04014025 doi: 10.1061/(ASCE)CC.1943-5614.0000483

Shehata, E.; Morphy, R.; and Rizkalla, S., 2000, “Fibre Reinforced Polymer Shear Reinforcement for Concrete Members: Behaviour and Design Guidelines,” Canadian Journal of Civil Engineering, V. 27, No. 5, pp. 859-872. doi: 10.1139/l00-004

Turmo, J.; Ramos, G.; and Aparicio, A. C., 2009, “Shear Truss Analogy for Concrete Members of Solid and Hollow Circular Cross Section,” Journal of Engineering Structures, V. 31, No. 2, pp. 455-465. doi: 10.1016/j.engstruct.2008.09.002


ALSO AVAILABLE IN:

Electronic Structural Journal