Title: Temperature Control for the Gomal Zam RCC Arch-Gravity Dam

Author(s): Chongjiang Du

Publication: Concrete International

Volume: 38

Issue: 11

Appears on pages(s): 31-36

Keywords: thermal, mixture, aggregate, pipe

DOI:

Date: 11/1/2016

Abstract:
An arch-gravity roller-compacted concrete (RCC) dam on the Gomal River, Pakistan, was built from 2008 to 2012. Temperature control measures were required during construction to prevent thermal cracking of RCC in hot weather. The article provides detailed descriptions of these measures, specifically the precooling of aggregates and mixing water and post-cooling of the placed RCC.




  