The New NY Bridge Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The New NY Bridge Construction

Author(s): Brian P. Cresenzi

Publication: Concrete International

Volume: 38

Issue: 9

Appears on pages(s): 29-34

Keywords: quality, oversight, placement, sample

DOI: 10.14359/51689266

Date: 9/1/2016

Abstract:
The existing Tappan Zee Bridge across the Hudson River between Westchester and Rockland Counties in New York State is being replaced with the New NY Bridge. A central requirement of the project is to achieve a 100-year service life without major rehabilitation. Cast-in-place concrete is a major material in the new bridge and will be in severe exposure conditions. The article discusses concrete production and concrete quality organization, as well as oversight testing and evaluation.

Related References:

1. “Code of Federal Regulations, Title 23: Highways, Part 637—Construction Inspection and Approval, Subpart B—Quality Assurance Procedures for Construction,” U.S. Government Printing Office, Washington, DC (www.ecfr.gov/cgi-bin/text-idx?rgn=div5&node=23:1.0.1.7.25).

2. “Construction Quality Assurance for Design-Build Highway Projects,” FHWA-HRT-12-039, Federal Highway Administration, McLean, VA, 2012, 8 pp.

3. “Materials Method 9.2—Field Inspection of Portland Cement Concrete,” New York State Department of Transportation, Albany, NY, 2012.

4. “Concrete, Mortar and Cement-Based Repair Materials: Chloride Migration Coefficient from Non-Steady-State Migration Experiments (NT Build 492),” Approved 1999-11, Nordtest, Taastrup, Denmark, 8 pp.

5. ASTM C457/C457M-11, “Standard Test Method for Microscopical Determination of Parameters of the Air-Void System in Hardened Concrete,” ASTM International, West Conshohocken, PA, 2011.

6. ASTM C1218/C1218M-99(2008), “Standard Test Method for Water-Soluble Chloride in Mortar and Concrete,” ASTM International, West Conshohocken, PA, 2008.

7. ASTM C231/C231M-10, “Standard Test Method for Air Content of Freshly Mixed Concrete by the Pressure Method,” ASTM International, West Conshohocken, PA, 2010.

8. ASTM C143/C143M-10a, “Standard Test Method for Slump of Hydraulic-Cement Concrete,” ASTM International, West Conshohocken, PA, 2010.

9. ASTM C138/C138M-10b, “Standard Test Method for Density (Unit Weight), Yield, and Air Content (Gravimetric) of Concrete,” ASTM International, West Conshohocken, PA, 2010.

10. ASTM C1064/C1064M-11, “Standard Test Method for Temperature of Freshly Mixed Hydraulic-Cement Concrete,” ASTM International, West Conshohocken, PA, 2011.

11. ASTM C39/C39M-12, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2012.