Development of Ultra-High-Performance Concretes for Dry Cask Waste Storage Applications

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development of Ultra-High-Performance Concretes for Dry Cask Waste Storage Applications

Author(s): Brian H. Green

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 11/4/2015

Abstract:
Cementitious materials have widespread use in nuclear waste storage and disposal applications, including waste form stabilization, dry storage structures, and repository applications, and in each application, the use of cement-based materials presents unique challenges. For cement-stabilized wastes and repository applications, the transport of radionuclides through the cementitious materials is of great concern, as certain radionuclides are highly mobile in high-pH pore fluid. For intermediate-term dry storage, thermal, radiation, and environmental loading can influence degradation of the portland cement concrete structures, which in turn impacts safe storage. This session addresses the measurement and modeling of properties that will improve the understanding and prediction of the long-term structural, hydraulic, and chemical performance of cementitious materials used in nuclear waste disposal.