Title: Assessment of Static Stability of Concrete Using Shear Wave Velocity Approach

Author(s): Siwar Naji, Kamal H. Khayat, and Mourad Karray

Publication: Materials Journal

Volume: 114

Issue: 1

Appears on pages(s): 105-115

Keywords: nondestructive testing; P-RAT; segregation; self-consolidating concrete; shear wave velocity; static stability

DOI: 10.14359/51689244

Date: 1/1/2017

Abstract:
Flowable concrete is prone to segregation that can adversely affect its performance. The risk of segregation should be reduced through adequate mixture proportioning and proper placement technique. The objective of this paper is to evaluate the potential segregation of concrete by monitoring changes in shear wave (S-wave) velocity using the piezoelectric ring actuator technique (P-RAT) after the initial setting time. The S-wave that can only propagate into solid phase is sensitive to differences in properties of cement paste and aggregate and can therefore reflect changes in static stability associated with changes in aggregate concentration and porosity of the cement paste. The proposed technique consists of a column measuring 450 mm (17.72 in.) in height that is equipped with three pairs of P-RAT sensors fixed at different heights to evaluate the homogeneity of S-wave velocity. Eight self-consolidating concrete (SCC) mixtures designed to have different levels of segregation resistance were used to evaluate the ability of the proposed S-wave velocity approach to evaluate segregation resistance. Static stability was also evaluated using the column segregation test determined for fresh concrete as well as coarse aggregate distribution along P-RAT column samples in the hardened state. Homogeneity of primary wave (P-wave) velocities was measured along the same concrete prismatic samples. The proposed P-RAT column approach is shown to enable the assessment of static stability of SCC. Test results indicated that a higher degree of correlation can be obtained between the segregation index deduced from the P-RAT column test at 10 and 24 hours after casting and the physical tests determined on fresh and hardened concrete. The interpretation of the distribution of S-waves is shown to be more reliable than that of the P-waves for in-place assessment of static stability of concrete.

Related References:

1. Esmaeilkhanian, B.; Khayat, K. H.; Yahia, A.; and Feys, D., “Effects of Mix Design Parameters and Rheological Properties on Dynamic Stability of Self-Consolidating Concrete,” Cement and Concrete Composites, V. 54, 2014, pp. 21-28. doi: 10.1016/j.cemconcomp.2014.03.001

2. Khayat, K. H.; Ghezal, A.; and Hadriche, M. S., “Factorial Design Model for Proportioning Self-Consolidating Concrete,” Materials and Structures, V. 32, No. 9, 1999, pp. 679-686. doi: 10.1007/BF02481706

3. Khayat, K. H., and Roussel, Y., “Testing and Performance of Fiber-Reinforced, Self- Consolidating Concrete,” Materials and Structures, V. 33, No. 6, 2000, pp. 391-397. doi: 10.1007/BF02479648

4. De Schutter, G.; Ye, G.; Audenaert, K.; Bager, D.; Baroghel-Bouny, V.; Bellmann, F.; Boel, V.; Bonen, D.; Boström, L.; Corradi, M.; Gartner, E.; Hama, Y.; Jacobsen, S.; Jansson, R.; Justnes, H.; Khayat, K. H.; Khrapko, M.; Leemann, A.; Luco, L. F.; Magarotto, R.; Nowak, A. S.; Persson, B.; Poppe, A.-M.; Qian, C.; Setzer, M. J.; and Sideris, K., “Final Report of RILEM TC 205-DSC: Durability of Self-Compacting Concrete,” Materials and Structures, V. 41, No. 2, 2008, pp. 225-233. doi: 10.1617/s11527-007-9319-9

5. Khayat, K. H., and De Schutter, G., eds., “Mechanical Properties of Self-Compacting Concrete,” State-of-the-Art Report 228-MPS on Mechanical Properties of Self-Compacting Concrete, Springer Publishers, New York, Jan. 2014, 271 pp.

6. Khayat, K. H., “Use of Viscosity-Modifying Admixture to Reduce Top-Bar Effect of Anchored Bars Cast with Fluid Concrete,” ACI Materials Journal, V. 95, No. 2, Mar.-Apr. 1998, pp. 158-167.

7. El-Chabib, H., and Nehdi, M., “Effect of Mixture Design Parameters on Segregation of Self-Consolidating Concrete,” ACI Materials Journal, V. 103, No. 5, Sept.-Oct. 2006, pp. 374-383.

8. Khayat, K. H., and Mitchell, D., “Self-Consolidating Concrete for Precast, Prestressed Concrete Bridge Elements,” National Cooperative Highway Research Program (NCHRP) Report 628, Transportation Research Board, Washington, DC, 2009, 99 pp.

9. Assaad, J.; Khayat, K. H.; and Daczko, J., “Evaluation of Static Stability of Self-Consolidating Concrete,” ACI Materials Journal, V. 101, No. 3, May-June 2004, pp. 207-215.

10. Khayat, K. H.; Manai, K.; and Trudel, A., “In-Situ Mechanical Properties of Wall Elements Cast Using Self-Consolidating Concrete,” ACI Materials Journal, V. 94, No. 6, Nov.-Dec. 1997, pp. 491-500.

11. Picka, J. D.; Jaiswal, S. S.; Igusa, T.; Karr, A. F.; and Shah, S. P., “Quantitative Description of Coarse Aggregate Volume Fraction Gradients,” Cement, Concrete and Aggregates, V. 22, No. 2, 2000, pp. 133-141. doi: 10.1520/CCA10473J

12. Khayat, K. H.; Pavate, T. V.; Assaad, J.; and Jolicoeur, C., “Analysis of Variations in Electrical Conductivity to Assess Stability of Cement-Based Materials,” ACI Materials Journal, V. 100, No. 4, July-Aug. 2003, pp. 302-310.

13. Khayat, K. H.; Vanhove, Y.; Pavate, T. V.; and Jolicoeur, C., “Multi-Electrode Conductivity Method to Evaluate Static Stability of Flowable and Self-Consolidating Concrete,” ACI Materials Journal, V. 104, No. 4, July-Aug. 2007, pp. 424-433.

14. Keske, S. D.; Schindler, A. K.; and Barnes, R. W., “Assessment of Stability Test Methods for Self-Consolidating Concrete,” ACI Materials Journal, V. 110, No. 4, July-Aug. 2011, pp. 385-393.

15. Soshiroda, T.; Voraputhaporn, K.; and Nozaki, Y., “Early-Stage Inspection of Concrete Quality in Structures by Combined Nondestructive Method,” Materials and Structures, V. 39, No. 2, 2007, pp. 149-160. doi: 10.1617/s11527-005-9007-6

16. Zhu, J.; Kee, S.; Han, D.; and Tsai, Y., “Effects of Air Voids on Ultrasonic Wave Propagation in Early Age Cement Pastes,” Cement and Concrete Research, V. 41, No. 8, 2011, pp. 872-881. doi: 10.1016/j.cemconres.2011.04.005

17. Gamal El Dean, D., “Development of a New Piezoelectric Pulse Testing Device and Soil Characterization Using Shear Waves,” doctoral thesis, Université de Sherbrooke, Sherbrooke, QC, Canada, 2007, 282 pp.

18. Ethier, Y., “La Mesure en Laboratoire de la Vitesse de Propagation des Ondes de Cisaillement,” doctoral thesis, Université de Sherbrooke, Sherbrooke, QC, Canada, 2009, 320 pp.

19. Ben Romdhan, M.; Hussien, M. N.; and Karray, M., “The Use of Piezoelectric Ring-Actuator Technique in Shear Wave Velocity Measurement of Granular Media,” GeoRegina, No. 307, 2014.

20. Karray, M.; Ben Romdhan, M.; Hussien, M. N.; and Éthier, Y., “Measuring Shear Wave Velocity of Granular Material Using the Piezoelectric Ring Actuator Technique (P-RAT),” Canadian Geotechnical Journal, V. 52, No. 9, 2015, pp. 1302-1317. doi: 10.1139/cgj-2014-0306

21. Soliman, N. A.; Khayat, K. H.; Karray, M.; and Omran, A. F., “Piezoelectric Ring Actuator Technique for Monitoring Early-Age Properties of Cement-Based Materials,” Cement and Concrete Composites, V. 63, 2015, pp. 84-95. doi: 10.1016/j.cemconcomp.2015.09.001

22. Bungey, J. H., “The Validity of Ultrasonic Pulse Velocity Testing of In-Place Concrete for Strength,” NDT&E International, V. 13, No. 6, 1980, pp. 296-300. doi: 10.1016/0308-9126(80)90021-8


ALSO AVAILABLE IN:

Electronic Materials Journal