Effect of Cement on Mechanical Behavior of Soil Contaminated with Monoethylene Glycol (MEG)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Cement on Mechanical Behavior of Soil Contaminated with Monoethylene Glycol (MEG)

Author(s): A. R. Estabragh, M. Khatibi, and A. A. Javadi

Publication: Materials Journal

Volume: 113

Issue: 6

Appears on pages(s): 709-717

Keywords: contaminated soil; monoethylene glycol; soil cement; strength; treatment

DOI: 10.14359/51689236

Date: 11/1/2016

Abstract:
This paper presents a study on the mechanical properties of a contaminated clay soil and its treatment by cement. One group of unconfined compression (UC) tests was performed on samples of natural soil, and soil contaminated by monoethylene glycol (MEG) with 40% concentration at different degrees of contamination (3, 6, and 9%). Another group of UC tests was conducted on the samples that were prepared as mixtures of clean or MEG-contaminated soil with different cement contents (3, 6, and 9%) at different curing times. The results show that the strength and stiffness of the soil contaminated with MEG is reduced increasingly by the degree of contamination. In addition, by adding cement to the contaminated soil, the strength of the soil is increased as a function of degree of contamination, percent of cement, and curing time.

Related References:

1. Tremblay, H.; Duchesne, J.; Locat, J.; and Leroueil, S., “Influence of the Nature of Organic Compounds on Fire Soil Stabilization with Cement,” Canadian Geotechnical Journal, V. 39, No. 3, 2002, pp. 535-546. doi: 10.1139/t02-002

2. Bahar, R.; Benazzoug, M.; and Kenai, S., “Performance of Compacted Cement Stabilized Soil,” Cement and Concrete Composites, V. 26, No. 7, 2004, pp. 811-820. doi: 10.1016/j.cemconcomp.2004.01.003

3. Basha, E. A.; Hashim, R.; Mahmud, H. B.; and Muntohar, A. S., “Stabilization of Residual Soil with Rice Husk Ash and Cement,” Construction and Building Materials, V. 19, No. 6, 2005, pp. 448-453. doi: 10.1016/j.conbuildmat.2004.08.001

4. Wiles, C., “Review of Solidification/Stabilization Technology,” Journal of Hazardous Materials, V. 14, No. 1, 1987, pp. 5-21. doi: 10.1016/0304-3894(87)87002-4

5. Barth, E. F., “An Overview of the History, Present Status and Future Directions of Solidification/Stabilization Technologies for Hazardous Waste Treatment,” Solidification/Stabilization: Mechanisms and Applications, Proceedings of the Second Symposium, Lamar University, Beaumont, TX, 1990, pp. 1-6.

6. Grabinska-Loniewska, A., “Studies on the Activated Sludge Bacteria Participating in the Biodegradation of Methanol, Formaldehyde and Ethylene Glycol: II. Utilization of Various Carbon and Nitrogen Compounds,” Acta Microbiologica Polonica. Series B: Microbiologia Applicata, V. 6, 1974, pp. 83-88.

7. Flathman, P. E.; Jerger, D. E.; and Bottomley, L. S., “Remediation of Contaminated Ground Water Using Biological Techniques,” Ground Water Monitoring Review, V. 9, No. 1, 1989, pp. 105-119. doi: 10.1111/j.1745-6592.1989.tb01126.x

8. Sills, R. D., and Blakeslee, P. A., “The Environmental Impact of Deicers in Airport Storm Water Runoff,” Chemical Deicers and the Environment, Lewis Publishers, Boca Raton, FL, 1992, pp. 323-340.

9. Lokke, H., “Leaching of Ethylene Glycol and Ethanol in Subsoils,” Water, Air, and Soil Pollution, V. 22, No. 4-5, 1984, pp. 373-387. doi: 10.1007/BF00282608

10. Dobson, S., “Ethylene Glycol: Environmental Aspects,” Concise International Chemical Assessment Document 22, Institute of Terrestrial Ecology, Natural Environment Research Council, Huntingdon, UK, 2000, pp. 1-27.

11. Fang, H. Y., Introduction to Environmental Geotechnology, CRC Press, Boca Raton, FL, 1997, 688 pp.

12. Meegoda, J. N.; Ezeldin, A. S.; Vaccari, D. A.; and Muller, R. T., “Petroleum Contaminated Soils in Highway Construction,” Infrastructure: New Materials and Methods of Repair, Proceedings of the 3rd Materials Engineering Conference, San Diego, CA, 1994, pp. 904-911.

13. Meegoda, J. N.; Chen, B.; Gunasekera, S. D.; and Pederson, P., “Compaction Characteristics of Contaminated Soils—Reuse as a Road Base Material,” Recycled Materials in Geotechnical Applications, Proceedings of the Geocongress: Geotechnical Special Publication No. 79, Boston, MA, 1998, pp. 195-209.

14. Meegoda, J. N., and Muller, R. T., “Petroleum Contaminate Soils in Highway Construction,” Recovery and Effective Reuse of Discarded and By-products for Construction of Highway Facilities, Denver, CO, 1993, pp. 4-83 to 4-95.

15. Tuncan, A.; Tuncan, M.; and Koyuncu, H., “Use of Petroleum Contaminated Drilling Wastes as Sub-base Material for Road Construction,” Waste Management & Research, V. 18, No. 5, 2000, pp. 489-505. doi: 10.1177/0734242X0001800511

16. Hassan, H. F.; Taha, R.; Al Rawas, A.; Al Shandoudi, B.; Al Gheithi, K.; and Al Barami, A. M., “Potential Uses of Petroleum-Contaminated Soil in Highway Construction,” Construction and Building Materials, V. 19, No. 8, 2005, pp. 646-652. doi: 10.1016/j.conbuildmat.2005.01.001

17. Pincus, H. J.; Meegoda, N. J.; and Ratnaweera, P., “Treatment of Oil Contaminated Soils for Identification and Classification,” Geotechnical Testing Journal, V. 18, No. 1, 1995, pp. 41-49. doi: 10.1520/GTJ10120J

18. Meegoda, N. J., and Ratnaweera, P., “Compressibility of Contaminated Fine-Grained Soils,” Geotechnical Testing Journal, V. 17, No. 1, 1994, pp. 101-112. doi: 10.1520/GTJ10078J

19. Kumar, A.; Walia, B. S.; and Bajaj, J. A., “Influence of Fly Ash, Lime, and Polyester Fibers on Compaction and Strength Properties of Expansive Soil,” Journal of Materials in Civil Engineering, ASCE, V. 19, No. 3, 2007, pp. 242-248. doi: 10.1061/(ASCE)0899-1561(2007)19:3(242)

20. Estabragh, A. R.; Namdar, P.; and Javadi, A. A., “Behavior of Cement-Stabilized Clay Reinforced with Nylon Fiber,” Geosynthetics International, V. 19, No. 1, 2012, pp. 85-92. doi: 10.1680/gein.2012.19.1.85

21. Kézdi, Á., Stabilized Earth Roads, Elsevier, 1979, 350 pp.

22. Khattak, M. J., and AlRashidi, M., “Durability and Mechanistic Characteristics of Fiber Reinforced Soil-Cement Mixtures,” International Journal of Pavement Engineering, V. 7, No. 1, 2006, pp. 53-62. doi: 10.1080/10298430500489207

23. ACI Committee 230, “State-of-the-Art Report on Soil Cement,” ACI Materials Journal, V. 87, No. 4, July-Aug. 1990, pp. 395-417.

24. Singh, S. K.; Srivastava, R. K.; and John, S., “Studies on Soil Contamination due to Used Motor Oil and Its Remediation,” Canadian Geotechnical Journal, V. 46, No. 9, 2009, pp. 1077-1083. doi: 10.1139/T09-047

25. Al-Rawas, A. A.; Hago, A.; and Al-Sarmi, H., “Effect of Lime, Cement and Sarooj (Artificial Pozzolan) on the Swelling Potential of an Expansive Soil from Oman,” Building and Environment, V. 40, No. 5, 2005, pp. 681-687. doi: 10.1016/j.buildenv.2004.08.028

26. Al-Sanad, H.; Eid, W. K.; and Ismael, N. F., “Geotechnical Properties of Oil-Contaminated Kuwaiti Sand,” Journal of Geotechnical Engineering, ASCE, V. 121, No. 5, 1995, pp. 407-412. doi: 10.1061/(ASCE)0733-9410(1995)121:5(407)

27. Croft, J. B., “The Influence of Soil Mineralogical Composition on Cement Stabilization,” Geotechnique, V. 17, No. 2, 1967, pp. 119-135. doi: 10.1680/geot.1967.17.2.119

28. Shen, C. K., and Mitchell, J. K., “Behaviour of Soil-Cement in Repeated Compression and Flexure,” Highway Research, V. 128, 1966, pp. 68-100.

29. Mitchell, J. K., and Soga, K., Fundamentals of Soil Behavior, John Wiley & Sons Inc., New York, 2005, 529 pp.

30. Craig, R. F., Soil Mechanics, fourth edition, Chapman and Hall, UK, 1987, 402 pp.

31. Fukue, M.; Minato, T.; Horibe, H.; and Taya, N., “The Micro-structures of Clay Given by Resistivity Measurements,” Engineering Geology, V. 54, No. 1-2, 1999, pp. 43-53. doi: 10.1016/S0013-7952(99)00060-5

32. van Olphen, H., “Internal Mutual Flocculation in Clay Suspensions,” Journal of Colloid and Interface Science, V. 19, No. 4, 1964, pp. 313-322. doi: 10.1016/0095-8522(64)90033-9

33. Kaya, A., and Durukan, S., “Utilization of Bentonite Embedded Zeolite as Clay Liner,” Applied Clay Science, V. 25, No. 1-2, 2004, pp. 83-91. doi: 10.1016/j.clay.2003.07.002

34. Bowders, J. J. Jr., and Daniel, D. E., “Hydraulic Conductivity of Compacted Clay to Dilute Organic Chemicals,” Journal of Geotechnical Engineering, ASCE, V. 113, No. 12, 1987, pp. 1432-1448. doi: 10.1061/(ASCE)0733-9410(1987)113:12(1432)

35. Moore, C. A., and Mitchell, J. K., “Electromagnetic Forces and Soil Strength,” Geotechnique, V. 24, No. 4, 1974, pp. 627-640. doi: 10.1680/geot.1974.24.4.627

36. Sridharan, A., and Rao, G., “Mechanisms Controlling Volume Change of Saturated Clays and the Role of the Effective Stress Concept,” Geotechnique, V. 29, No. 3, 1973, pp. 359-382. doi: 10.1680/geot.1973.23.3.359

37. Sridharan, A., and Rao, G., “Shear Strength Behaviour of Saturated Clays and Role of the Effective Stress Concept,” Geotechnique, V. 2, No. 2, 1979, pp. 177-193. doi: 10.1680/geot.1979.29.2.177

38. Ratnaweera, P., and Meegoda, J. N., “Shear Strength and Stress-Strain Behaviour of Contaminated Soils,” Geotechnical Testing Journal, V. 29, 2005, pp. 1-8.

39. Proctor, R. R., “Fundamental Principles of Soil Compaction,” Engineering News-Record, V. 11, 1933, pp. 245-248.

40. Sherif, M. A., and Burrous, C. M., “Temperature Effects on the Unconfined Shear Strength of Saturated Cohesive Soil,” Highway Research Board Special Report No. 103, 1969, pp. 267-272.

41. Mindess, S., and Young, F. J., Concrete, Prentice Hall, Englewood Cliffs, NJ, 1981, 644 pp.

42. Williamson, S., and Cortes, D. D., “Dimensional Analysis of Soil-Cement Mixture Performance,” Géotechnique Letters, V. 4, No. 1, pp. 33-38.


ALSO AVAILABLE IN:

Electronic Materials Journal