Title: What Do We Mean by “Setting?”

Author(s): Chang Hoon Lee and Kenneth C. Hover

Publication: Concrete International

Volume: 38

Issue: 8

Appears on pages(s): 53-59

Keywords: mortar, concrete, paste, test

DOI:

Date: 8/1/2016

Abstract:
This article provides a comparison of the stiffening behaviors of pastes, mortars, and concretes using standard tests methods and field-oriented nonstandard measures. Based on the test results, the authors determined that while the ASTM C403/C403M test provides a useful means of tracking the continuous process of stiffening, its threshold values for “initial” and “final” setting do not necessarily coincide with the times at which concrete placing, consolidation, or finishing operations must be performed.




  

Edit Module Settings to define Page Content Reviewer