Structural Testing and Dissection of Carbon Fiber- Reinforced Polymer-Repaired Bridge Girders Taken Out of Service

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Structural Testing and Dissection of Carbon Fiber- Reinforced Polymer-Repaired Bridge Girders Taken Out of Service

Author(s): Jovan Tatar, David Wagner, and H. R. (Trey) Hamilton

Publication: Structural Journal

Volume: 113

Issue: 6

Appears on pages(s): 1357-1367

Keywords: bridge; carbon fiber-reinforced polymer; corrosion; durability; load test; repair

DOI: 10.14359/51689160

Date: 11/1/2016

Abstract:
Carbon fiber-reinforced polymer (CFRP) is becoming a method of choice for repair and strengthening of many environmentally aged structures, bridges in particular. Durability of such CFRP repairs/strengthening efforts still remains uncertain. This paper presents the findings from structural and materials testing conducted on a CFRP-wrapped bridge girder that was taken out of service from the Indian River Bridge located in Melbourne, FL. The bridge girders, originally constructed in the 1960s, experienced corrosion damage during their service life in a brackish water environment. Following the repair of corrosion damage using conventional methods, repaired regions were wrapped with CFRP. Test results showed a modest increase in strength as a result of CFRP wrapping; fiber-reinforced polymer wrap, however, may have resulted in a reduction of chloride contamination following installation of the repair system. Furthermore, comparison of test results between the laboratory and field load tests indicated that AASHTO load distribution factors are conservative for this cast-in-place beam and slab bridge.

Related References:

AASHTO, 2015, “AASHTO LRFD Bridge Design Specifications,” American Association of State Highway and Transportation Officials, Washington, DC.

AASHTO T 24, 2013, “Standard Method of Test for Obtaining and Testing Drilled Cores and Sawed Beams of Concrete,” American Association of State Highway and Transportation Officials, Washington, DC, 13 pp.

AASHTO T 260, 1997, “Standard Method of Test for Sampling and Testing for Chloride Ion in Concrete and Concrete Raw Materials,” American Association of State Highway and Transportation Officials, Washington, DC, 15 pp.

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary,” American Concrete Institute, Farmington Hills, MI, 519 pp.

ACI Committee 440, 2008, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-08),” American Concrete Institute, Farmington Hills, MI, 76 pp.

Akinci, N. O.; Liu, J.; and Bowman, M. D., 2008, “Parapet Strength and Contribution to Live-Load Response for Superload Passages,” Journal of Bridge Engineering, ASCE, V. 13, No. 1, pp. 55-63. doi: 10.1061/(ASCE)1084-0702(2008)13:1(55)

ASTM D3039/D3039M-08, 2008, “Standard Test Method for Tensile Properties of Polymer Matrix Composite Materials,” ASTM International, West Conshohocken, PA, 13 pp.

ASTM A370-13, 2013, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products,” ASTM International, West Conshohocken, PA, 48 pp.

ASTM C39/C39M-15, 2015, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 7 pp.

ASTM C42/C42M-13, 2013, “Standard Test Method for Obtaining and Testing Drilled Cores and Sawed Beams of Concrete,” ASTM International, West Conshohocken, PA, 7 pp.

ASTM A615/A615M-15, 2015, “Standard Specification for Deformed and Plain Carbon-Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2015, 8 pp.

ASTM D7565/D7565M-10, 2010, “Standard Test Method for Determining Tensile Properties of Fiber Reinforced Polymer Matrix Composites Used for Strengthening of Civil Structures,” ASTM International, West Conshohocken, PA, 5 pp.

Belarbi, A., and Hsu, T. C., 1994, “Constitutive Laws of Concrete in Tension and Reinforcing Bars Stiffened by Concrete,” ACI Structural Journal, V. 91, No. 4, July-Aug., pp. 465-474.

Binns, R., and Mygind, H., 1949, “The Use of Electrical Resistance Strain Gauges and the Effect of Aggregate Size on Gauge Length in Connexion with the Testing of Concrete,” Magazine of Concrete Research, V. 1, No. 1, pp. 35-39.

Collins, M. P., and Mitchell, D., 1991, Prestressed Concrete Structures, Prentice-Hall, Englewood Cliffs, NJ, 766 pp.

Conner, S., and Huo, X. S., 2006, “Influence of Parapets and Aspect Ratio on Live-Load Distribution,” Journal of Bridge Engineering, ASCE, V. 11, No. 2, pp. 188-196. doi: 10.1061/(ASCE)1084-0702(2006)11:2(188)

Consolazio, G. R.; Fung, J.; and Ansley, M., 2004, “M-f-P Diagrams for Concrete Sections Under Biaxial Flexure and Axial Compression,” ACI Structural Journal, V. 101, No. 1, Jan.-Feb., pp. 114-123.

Cromwell, J. R.; Harries, K. A.; and Shahrooz, B. M., 2011, “Environmental Durability of Externally Bonded FRP Materials Intended for Repair of Concrete Structures,” Construction & Building Materials, V. 25, No. 5, pp. 2528-2539. doi: 10.1016/j.conbuildmat.2010.11.096

Eamon, C. D., and Nowak, A. S., 2002, “Effects of Edge-Stiffening Elements and Diaphragms on Bridge Resistance and Load Distribution,” Journal of Bridge Engineering, ASCE, V. 7, No. 5, pp. 258-266. doi: 10.1061/(ASCE)1084-0702(2002)7:5(258)

Hamilton, H. R., and Potter, W., 2010, “In Situ Load Test of Concrete Bridge Girders Repaired With CFRP Bonded Reinforcement,” 13th International Conference—Structural Faults and Repair 2010, E.C.S. Publications, Edinburgh, UK.

Masters, J. E., and Ifju, P. G., 1997, “Strain Gage Selection Criteria for Textile Composite Materials,” Journal of Composites, Technology and Research, V. 19, No. 3, pp. 152-167. doi: 10.1520/CTR10026J

NCHRP Report 655, 2010, “Recommended Guide Specification for the Design of Externally Bonded FRP Systems for Repair and Strengthening of Concrete Bridge Elements,” National Cooperative Highway Research Program, Transportation Research Board, Washington, DC.

Pessiki, S.; Harries, K. A.; Kestner, J. T.; Sause, R.; and Ricles, J. M., 2001, “Axial Behavior of Reinforced Concrete Columns Confined with FRP Jackets,” Journal of Composites for Construction, ASCE, V. 5, No. 4, pp. 237-245. doi: 10.1061/(ASCE)1090-0268(2001)5:4(237)

RILEM CPC-18, 1994, “Measurement of Hardened Concrete Carbonation Depth,” RILEM Recommendations for the Testing and Use of Constructions Materials, RILEM, Paris, France, pp. 56-58.

Tatar, J., and Hamilton, H. R., 2016, “Bond Durability Factor for Externally Bonded CFRP Systems in Concrete Structures,” Journal of Composites for Construction, ASCE, V. 20, No. 1, p. 04015027 doi: 10.1061/(ASCE)CC.1943-5614.0000587

Yang, X.; Nanni, A.; Haug, S.; and Sun, C. L., 2002, “Strength and Modulus Degradation of Carbon Fiber-Reinforced Polymer Laminates from Fiber Misalignment,” Journal of Materials in Civil Engineering, ASCE, V. 14, No. 4, pp. 320-326. doi: 10.1061/(ASCE)0899-1561(2002)14:4(320)


ALSO AVAILABLE IN:

Electronic Structural Journal