Cyclic Shear Behavior of High-Strength Concrete Structural Walls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cyclic Shear Behavior of High-Strength Concrete Structural Walls

Author(s): Susanto Teng and Jimmy Chandra

Publication: Structural Journal

Volume: 113

Issue: 6

Appears on pages(s): 1335-1345

Keywords: boundary element; building codes; height-to-length ratio; highstrength concrete (HSC) walls; shear behavior; shear strength; web reinforcement ratio

DOI: 10.14359/51689158

Date: 11/1/2016

Abstract:
High-strength concrete (HSC) walls having compressive strength of approximately 100 MPa (14,500 psi) were tested under cyclic lateral loading to investigate their shear behavior. The parameters included were height-to-length ratio of the walls, vertical and horizontal web reinforcement ratios, and the effects of boundary elements in the form of flanges. The experimental results show that shorter walls exhibit greater shear strength than taller walls. Both vertical and horizontal web reinforcements contribute significantly to increasing the shear strength of the walls, with the horizontal web reinforcement being more effective for walls having height-to-length ratio from 1.0 to 2.0. With increase in height-to-length ratio of walls, the concrete contribution to the shear strength decreases while the web reinforcement contribution increases. The presence of flanges also significantly increases the shear strength of HSC walls. Experimental wall shear strengths from this study as well as from literature were compared with predictions from the ACI Code and Eurocode provisions. It can be seen that both ACI and Eurocode do not give consistent safety factors. The ACI method can be unsafe for low-strength concrete walls, while the Eurocode is overly conservative in almost all cases.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

2. Comite Europeen de Normalisation, “Eurocode 8: Design of Structures for Earthquake Resistance Part 1: General Rules, Seismic Actions and Rules for Buildings (EN 1998-1),” Comite Europeen de Normalisation (CEN), Brussels, Belgium, 2004, 229 pp.

3. Cardenas, A. E., and Magura, D. D., “Strength of High-Rise Shear Walls—Rectangular Cross Section,” Multistory Structures/Lateral Forces, SP-36, American Concrete Institute, Farmington Hills, MI, 1972, pp. 119-150.

4. Cardenas, A. E.; Russell, H. G.; and Corley, W. G., “Strength of Low-Rise Structural Walls,” Reinforced Concrete Structures Subjected to Wind and Earthquake Forces, SP-63, American Concrete Institute, Farmington Hills, MI, 1980, pp. 221-242.

5. Chandra, J., and Teng, S., “Shear Behaviour of High Strength Concrete Walls Subjected to Cyclic Lateral Loading,” 2015 Interim Research Report to National Research Foundation (NRF), School of Civil and Environmental Engineering, Nanyang Technological University, Singapore, 2015, 329 pp.

6. Barda, F.; Hanson, J. M.; and Corley, W. G., “Shear Strength of Low-Rise Walls with Boundary Elements,” Reinforced Concrete Structures in Seismic Zones, SP-53, American Concrete Institute, Farmington Hills, MI, 1977, pp. 149-202.

7. Corley, W. G.; Fiorato, A. E.; and Oesterle, R. G., “Structural Walls,” Significant Developments in Engineering Practice and Research, SP-72, American Concrete Institute, Farmington Hills, MI, 1981, pp. 77-132.

8. Maeda, Y., “Study on Load-Deflection Characteristics of Reinforced Concrete Shear Walls of High Strength Concrete—Part 1 Lateral Loading Test (in Japanese),” Research Institute Maeda Construction Corporation, Tokyo, Japan, 1986, pp. 97-107.

9. Okamoto, S., “Study on Reactor Building Structure using Ultra-High Strength Materials: Part 1. Bending Shear Test of RC Shear Wall—Outline (in Japanese),” Summaries of Technical Papers of Annual Meeting, Architectural Institute of Japan, Tokyo, Japan, 1990, pp. 1469-1470.

10. Mo, Y. L., and Chan, J., “Behavior of Reinforced Concrete Framed Shear Walls,” Nuclear Engineering and Design, V. 166, No. 1, 1996, pp. 55-68. doi: 10.1016/0029-5493(96)01244-7

11. Gupta, A., and Rangan, B. V., “High-Strength Concrete (HSC) Structural Walls,” ACI Structural Journal, V. 95, No. 2, Mar.-Apr. 1998, pp. 194-204.

12. Kabeyasawa, T., and Hiraishi, H., “Tests and Analyses of High-Strength Reinforced Concrete Shear Walls in Japan,” High-Strength Concrete in Seismic Regions, SP-176, American Concrete Institute, Farmington Hills, MI, 1998, pp. 281-310.

13. Farvashany, F. E.; Foster, S. J.; and Rangan, B. V., “Strength and Deformation of High-Strength Concrete Shear Walls,” ACI Structural Journal, V. 105, No. 1, Jan.-Feb. 2008, pp. 21-29.

14. Burgueno, R.; Liu, X.; and Hines, E. M., “Web Crushing Capacity of High-Strength Concrete Structural Walls: Experimental Study,” ACI Structural Journal, V. 111, No. 1, Jan.-Feb. 2014, pp. 37-48.


ALSO AVAILABLE IN:

Electronic Structural Journal