Experimental Evaluation on Effect of Openings on Behavior of Prestressed Precast Hollow-Core Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Evaluation on Effect of Openings on Behavior of Prestressed Precast Hollow-Core Slabs

Author(s): Sameer Kumar Sarma Pachalla and S. Suriya Prakash

Publication: Structural Journal

Volume: 114

Issue: 2

Appears on pages(s): 427-436

Keywords: cutouts; finite element analysis (FEA); hollow-core slabs; openings; precast prestressed; shear span-depth ratio

DOI: 10.14359/51689155

Date: 3/1/2017

Abstract:
Prestressed precast hollow-core slabs are generally machine-cast with prestressing strands as only flexural reinforcement with no shear reinforcement. Various mechanical, electrical, and plumbing service requirements require openings to be provided in these precast slabs. Openings in hollow-core slabs can coincide with the location of strands and may lead to their curtailment. The size of these openings can vary from minimal, causing no change, to very large, causing adverse effects on the structural behavior of the slab. An experimental study was carried out to evaluate the effect of openings in hollow-core slabs. Six full-scale tests were conducted by considering shear span-depth ratio and location of openings as parameters. The strength of concrete, prestressing ratio, and size of opening was kept constant in all slabs. It was observed that the provision of openings not only reduced the cracking and ultimate strength of slabs but also altered the failure modes with change in deformation capacity. Experimental results were compared with predictions of code equations and finite element analysis (FEA) based software. A fair correlation was observed between the test results and finite element (FE) predictions. The FE modeling approach of hollow-core slabs suggested in this study can be used further for parametric studies and to develop design equations.

Related References:

ACI Committee 318, 2011, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary,” American Concrete Institute, Farmington Hills, MI, 503 pp.

Afefy, H. M., and Fawzy, T. M., 2013, “Strengthening of RC One-Way Slabs Including Cut-Out Using Different Techniques,” Engineering Structures, V. 57, pp. 23-36. doi: 10.1016/j.engstruct.2013.09.013

Al-hafiz, A. M.; Chiad, S. S.; and Farhan, M. S., 2013, “Flexural Strength of Reinforced Concrete One-Way Opened Slabs with and without Strengthening,” Australian Journal of Basic and Applied Sciences, V. 7, No. 6, pp. 642-651.

Anil, Ö.; Kaya, N.; and Arslan, O., 2013, “Strengthening of One Way RC Slab with Opening Using CFRP Strips,” Construction and Building Materials, V. 48, pp. 883-893. doi: 10.1016/j.conbuildmat.2013.07.093

ANSYS, 2012, version 14.5, ANSYS, Inc., Canonsburg, PA.

Becker, R. J., and Buettner, D. R., 1985, “Shear Tests of Extruded Hollow-Core Slabs,” PCI Journal, V. 30, No. 2, pp. 40-54.

Foubert, S., 2014, “Flexural Strengthening of Prestressed Hollow-Core Slabs Using Near-Surface Mounted (NSM) CFRP Reinforcement,” University of Manitoba, Winnipeg, MB, Canada.

Hawkins, N. M., and Ghosh, S. K., 2006, “Shear Strength of Hollow-Core Slabs,” PCI Journal, V. 51, No. 1, pp. 110-114.

Hognestad, E., 1951, “A Study of Combined Bending and Axial Load in Reinforced Concrete Members,” Bulletin Series No. 399.

Jendele, L., and Cervenka, J., 2006, “Finite Element Modelling of Reinforcement with Bond,” Computers & Structures, V. 84, No. 28, pp. 1780-1791. doi: 10.1016/j.compstruc.2006.04.010

Johnson, T., and Ghadiali, Z., 1972, “Load Distribution Test on Precast Hollow Core Slabs with Openings,” PCI Journal, V. 17, No. 5, pp. 9-19. doi: 10.15554/pcij.09011972.9.19

Kim, Y. J.; Longworth, J. M.; Wight, R. G.; and Green, M. F., 2010, “Punching Shear of Two-Way Slabs Retrofitted with Prestressed or Non-Prestressed CFRP Sheets,” Journal of Reinforced Plastics and Composites, V. 29, No. 8, pp. 1206-1223. doi: 10.1177/0731684409103143

Pajari, M., 1998, “Shear Resistance of PHC Slabs Supported on Beams. II: Analysis,” Journal of Structural Engineering, ASCE, V. 124, No. 9, pp. 1062-1073. doi: 10.1061/(ASCE)0733-9445(1998)124:9(1062)

Palmer, K. D., and Schultz, A. E., 2011, “Experimental Investigation of the Web-Shear Strength of Deep Hollow-Core Units,” PCI Journal, V. 56, No. 4, pp. 83-104. doi: 10.15554/pcij.09012011.83.104

Ramberg, W., and Osgood, W. R., 1943, “Description of Stress-Strain Curves by Three Parameters,” Technical Note No. 902, National Advisory Committee for Aeronautics.

Seliem, H. M.; Seracino, R.; Sumner, E.; and Smith, S. T., 2011, “Case Study on the Restoration of Flexural Capacity of Continuous One-Way RC Slabs with Cutouts,” Journal of Composites for Construction, ASCE, V. 15, No. 6, pp. 992-998. doi: 10.1061/(ASCE)CC.1943-5614.0000232

Tan, K. H., and Zhao, H., 2004, “Strengthening of Openings in One-Way Reinforced-Concrete Slabs Using Carbon Fiber-Reinforced Polymer Systems,” Journal of Composites for Construction, ASCE, V. 8, No. 5, pp. 393-402. doi: 10.1061/(ASCE)1090-0268(2004)8:5(393)

Vasquez, A., and Karbhari, V. M., 2003, “Fiber-Reinforced Polymer Composite Strengthening of Concrete Slabs with Cutouts,” ACI Structural Journal, V. 100, No. 5, Sept.-Oct. pp. 665-673.

Walraven, J. C., and Mercx, W. P. M., 1983, “The Bearing Capacity for Prestressed Hollow Core Slabs,” Heron, V. 28, No. 3, pp. 1-46.

Willam, K., and Warnke, E., 1975, “Constitutive Model for the Triaxial Behavior of Concrete International Association for Bridge and Structure Engineering,” Proc. Int. Association for Bridge and Structural Eng., pp. 1-30.

Yang, L., 1994, “Design of Prestressed Hollow Core Slabs with Reference to Web Shear Failure,” Journal of Structural Engineering, ASCE, V. 120, No. 9, pp. 2675-2696. doi: 10.1061/(ASCE)0733-9445(1994)120:9(2675)


ALSO AVAILABLE IN:

Electronic Structural Journal