Size Effect in Torsional Strength of Plain and Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Size Effect in Torsional Strength of Plain and Reinforced Concrete

Author(s): Kedar Kirane, Konjengbam Darunkumar Singh, and Zdenek P. Bažant

Publication: Structural Journal

Volume: 113

Issue: 6

Appears on pages(s): 1253-1262

Keywords: crack band model; microplane model; reinforced concrete; size effect; torsion

DOI: 10.14359/51689149

Date: 11/1/2016

Abstract:
As shown long ago, plain and longitudinally reinforced concrete beams without stirrups exhibit a significant size effect on torsional strength, which was thought to be of a type occurring after long, stable crack growth (called Type II). This paper shows, by experimentally calibrated finite element simulations, that: 1) longitudinally reinforced concrete beams with stirrups also exhibit a significant size effect; and 2) the size effect in beams both with and without stirrups is not of Type II but Type I, characterizing failure at macrocrack initiation. In the practical size range, Type I is deterministic and terminates with a horizontal, rather than inclined, asymptote. The simulations are based on microplane model M7, which was shown to match well all the types of uniaxial, biaxial, and triaxial tests with post-peak softening in tension and compression. The model is calibrated by simulating previous torsional size effect tests of plain concrete beams and of longitudinally reinforced beams without stirrups, as well as the tests of beams with stirrups having different reinforcement ratios and different aspect ratios. The fact that all these tests are fitted closely, in terms of not only the maximum loads but also the crack patterns, lends credence to the predictions of size effect in beams with stirrups.

Related References:

1. Joint ACI-ASCE Committee 445, “Report on Torsion in Structural Concrete (ACI 445.1R-12),” American Concrete Institute, Farmington Hills, MI, 2013, 92 pp.

2. Hsu, T. T. C., “Torsion of Structural Concrete—Plain Concrete Rectangular Sections,” Torsion of Structural Concrete, SP-18, American Concrete Institute, Farmington Hills, MI, Jan. 1968, pp. 203-238.

3. Hsu, T. T. C., “Torsion of Structural Concrete—Behavior of Reinforced Concrete Rectangular Members,” Torsion of Structural Concrete, SP-18, American Concrete Institute, Farmington Hills, MI, Jan. 1968, pp. 261-306.

4. Bažant, Z. P., and Sener, S., “Size Effect in Torsional Failure of Concrete Beams,” Journal of Structural Engineering, ASCE, V. 113, No. 10, 1987, pp. 2125-2136. doi: 10.1061/(ASCE)0733-9445(1987)113:10(2125)

5. Bažant, Z. P.; Sener, S.; and Prat, P. C., “Size Effect Tests of Torsional Failure of Plain and Reinforced Concrete Beams,” Materials and Structures, V. 21, No. 6, 1988, pp. 425-430. doi: 10.1007/BF02472322

6. Hsu, T. T. C., and Mo, Y. L., “Softening of Concrete in Torsional Members—Theory and Tests,” ACI Journal Proceedings, V. 82, No. 3, May-June 1985, pp. 290-303.

7. Humphreys, R., “Torsional Properties of Prestressed Concrete,” The Structural Engineer, V. 35, No. 6, 1957, pp. 213-224.

8. Iravani, S., “Mechanical Properties of High-Performance Concrete,” ACI Materials Journal, V. 93, No. 5, Sept.-Oct. 1996, pp. 416-426.

9. McMullen, A. E., and Daniel, H. R., “Torsional Strength of Longitudinally Reinforced Concrete Beams Containing an Opening,” ACI Journal Proceedings, V. 72, No. 8, Aug. 1975, pp. 415-420.

10. McMullen, A. E., and Woodhead, H. R., “Experimental Study of Prestressed Concrete under Combined Torsion, Bending, and Shear,” PCI Journal, V. 18, No. 5, 1973, pp. 85-100. doi: 10.15554/pcij.09011973.85.100

11. Rahal, K. N., “Torsional Strength of Reinforced Concrete Beams,” Canadian Journal of Civil Engineering, V. 27, No. 3, 2000, pp. 445-453. doi: 10.1139/l99-083

12. Wang, W., and Hsu, T. T. C., “Limit Analysis of Reinforced Concrete Beams Subjected to Pure Torsion,” Journal of Structural Engineering, ASCE, V. 123, No. 1, 1997, pp. 86-94. doi: 10.1061/(ASCE)0733-9445(1997)123:1(86)

13. Zia, P., “Torsional Strength of Prestressed Concrete Members,” ACI Journal Proceedings, V. 57, No. 10, Oct. 1961, pp. 1337-1359.

14. Bažant, Z. P., and Planas, J., 1998, Fracture and Size Effect in Concrete and Other Quasibrittle Materials, CRC Press, Boca Raton, FL, 640 pp.

15. Caner, F. C., and Bažant, Z. P., “Microplane Model M7 for Plain Concrete I: Formulation,” Journal of Engineering Mechanics, ASCE, V. 139, No. 12, 2013, pp. 1714-1723. doi: 10.1061/(ASCE)EM.1943-7889.0000570

16. Bažant, Z. P.; Caner, F. C.; Carol, I.; Adley, M. D.; and Akers, S. A., “Microplane Model M4 for Concrete: I. Formulation with Work-Conjugate Deviatoric Stress,” Journal of Engineering Mechanics, ASEC, V. 126, No. 9, 2000, pp. 944-953. doi: 10.1061/(ASCE)0733-9399(2000)126:9(944)

17. Bažant, Z. P., and Oh, B. H., “Microplane Model for Progressive Fracture of Concrete and Rock,” Journal of Engineering Mechanics, ASCE, V. 111, No. 4, 1985, pp. 559-582. doi: 10.1061/(ASCE)0733-9399(1985)111:4(559)

18. Caner, F. C., and Bažant, Z. P., “Microplane Model M7 for Plain Concrete II: Calibration and Verification,” Journal of Engineering Mechanics, ASCE, V. 139, No. 12, 2013, pp. 1724-1735. doi: 10.1061/(ASCE)EM.1943-7889.0000571

19. Taylor, G. I., “Plastic Strain in Metals,” Journal of the Institute of Metals, V. 62, 1938, pp. 307-324.

20. Batdorf, S., and Budianski, B., “A Mathematical Theory of Plasticity Based on the Concept of Slip,” Technical Note 1871, National Advisory Committee for Aeronautics, Washington, DC, 1949.

21. Abaqus, ABAQUS/Explicit User’s Manual, Abaqus Version 6.11, 2011.

22. Bažant, Z. P., and Oh, B. H., “Crack Band Theory for Fracture of Concrete,” Matériaux et Constructions, V. 16, No. 3, 1983, pp. 155-177. doi: 10.1007/BF02486267

23. Bažant, Z. P., and Novák, D., “Energetic-Statistical Size Effect in Quasibrittle Failure at Crack Initiation,” ACI Materials Journal, V. 97, No. 3, May-June 2000, pp. 381-392.

24. Bažant, Z. P., and Novák, D., “Probabilistic Nonlocal Theory for Quasibrittle Fracture Initiation and Size Effect. I. Theory,” Journal of Engineering Mechanics, ASCE, V. 126, No. 2, 2000, pp. 166-174. doi: 10.1061/(ASCE)0733-9399(2000)126:2(166)


ALSO AVAILABLE IN:

Electronic Structural Journal