Influence of Stirrup Corrosion on Shear Strength of Reinforced Concrete Slender Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Stirrup Corrosion on Shear Strength of Reinforced Concrete Slender Beams

Author(s): Ahmed K. El-Sayed, Raja Rizwan Hussain, and Ahmed B. Shuraim

Publication: Structural Journal

Volume: 113

Issue: 6

Appears on pages(s): 1223-1232

Keywords: corrosion; shear strength; slender beams; stirrups

DOI: 10.14359/51689147

Date: 11/1/2016

Abstract:
The influence of stirrup corrosion on the shear strength of reinforced concrete slender beams was investigated and presented in this paper. A total of nine full-scale reinforced concrete beams were constructed and tested. The beams measured 200 mm (7.87 in.) wide, 350 mm (13.78 in.) deep, and 2800 mm (110.24 in.) long. Six beams had the embedded stirrups subjected to accelerated corrosion. The beams were tested in four-point bending under a simply supported span of 2400 mm (94.49 in.) and a shear span depth ratio of 3. The test variables included the corrosion damage level and the spacing of stirrups. The test results indicated that the corroded beams exhibited reduced shear strength in comparison to the uncorroded control beams. The reduction in shear strength became more pronounced as the corrosion level increased. The study was extended showing how to incorporate the corrosion effects into the current shear design method. The shear strength of the tested corroded beams was predicted using the proposed design procedure. Good correlation and agreement were found by comparing the predicted and experimental shear strength of the beams.

Related References:

1. Du, Y. G.; Clark, L. A.; and Chan, A., “Residual Capacity of Corroded Reinforcing Bars,” Magazine of Concrete Research, V. 57, No. 3, 2005, pp. 135-147. doi: 10.1680/macr.2005.57.3.135

2. Almusallam, A. A., “Effect of Degree of Corrosion on the Properties of Reinforcing Steel Bars,” Construction and Building Materials, V. 15, No. 8, 2001, pp. 361-368. doi: 10.1016/S0950-0618(01)00009-5

3. Lee, H. S.; Tomosawa, F.; and Noguchi, T., “Effect of Rebar Corrosion on the Structural Performance of Single Reinforced Beams,” Durability of Building Materials and Components, V. 7, C. Sjostrom, ed., E&FN Spon, London, UK, 1996, pp. 571-580.

4. Lee, H. S.; Noguchi, T.; and Tomosawa, F., “Evaluation of the Bond Properties between Concrete and Reinforcement as a Function of the Degree of Reinforcement Corrosion,” Cement and Concrete Research, V. 32, No. 8, 2002, pp. 1313-1318. doi: 10.1016/S0008-8846(02)00783-4

5. Auyeung, Y.; Balaguru, P.; and Chung, L., “Bond Behavior of Corroded Reinforcement Bars,” ACI Materials Journal, V. 97, No. 2, Mar.-Apr. 2000, pp. 214-220.

6. Amleh, L., and Mirza, S., “Corrosion Influence on Bond between Steel and Concrete,” ACI Structural Journal, V. 96, No. 3, May-June 1999, pp. 415-423.

7. Stanish, K.; Hooton, R. D.; and Pantazopoulou, S. J., “Corrosion Effects on Bond Strength in Reinforced Concrete,” ACI Structural Journal, V. 96, No. 6, Nov.-Dec. 1999, pp. 915-921.

8. Al-Sulaimani, G. J.; Kaleemullah, M.; Basunbul, I. A.; and Rasheeduzzafar, “Influence of Corrosion and Cracking on Bond Behavior and Strength of Reinforced Concrete Members,” ACI Structural Journal, V. 87, No. 2, Mar.-Apr. 1990, pp. 220-231.

9. Tastani, S. P., and Pantazopoulou, S. J., “Behavior of Corroded Bar Anchorages,” ACI Structural Journal, V. 104, No. 6, Nov.-Dec. 2007, pp. 756-766.

10. Oyado, M.; Kanakubo, T.; Sato, T.; and Yamamoto, Y., “Bending Performance of Reinforced Concrete Member Deteriorated by Corrosion,” Journal of Structure and Infrastructure Engineering: Maintenance, Management, Life-Cycle Design and Performance, V. 7, No. 1-2, 2011, pp. 121-130. doi: 10.1080/15732471003588510

11. Chung, L.; Najm, H.; and Balaguru, P., “Flexural Behavior of Concrete Slabs with Corroded Bars,” Cement and Concrete Composites, V. 30, No. 3, 2008, pp. 184-193. doi: 10.1016/j.cemconcomp.2007.08.005

12. Azad, A. K.; Ahmad, E. F.; and Azher, S. A., “Residual Strength of Corrosion-Damaged Reinforced Concrete Beams,” ACI Structural Journal, V. 104, No. 1, Jan.-Feb. 2007, pp. 40-47.

13. Du, Y.; Clark, L. A.; and Chan, A. H., “Impact of Reinforcement Corrosion on Ductile Behavior of Reinforced Concrete Beams,” ACI Structural Journal, V. 104, No. 3, May-June 2007, pp. 285-293.

14. Ballim, Y., and Reid, J. C., “Reinforcement Corrosion and the Deflection of RC Beams––An Experimental Critique of Current Test Methods,” Cement and Concrete Composites, V. 25, No. 6, 2003, pp. 625-632. doi: 10.1016/S0958-9465(02)00076-8

15. Yoon, S.; Wang, K.; Weiss, W. J.; and Shah, S. P., “Interaction between Loading, Corrosion, and Serviceability of Reinforced Concrete,” ACI Materials Journal, V. 97, No. 6, Nov.-Dec. 2000, pp. 637-644.

16. Magnat, P. S., and Elgarf, M. S., “Flexural Strength of Concrete Beams with Corroding Reinforcement,” ACI Structural Journal, V. 96, No. 1, Jan.-Feb. 1999, pp. 149-159.

17. Almusallam, A. A.; Al-Gahtani, A. S.; Aziz, A. R.; Dakhil, F. H.; and Rasheeduzzafar, “Effect of Reinforcement Corrosion on Flexural Behavior of Concrete Slabs,” Journal of Materials in Civil Engineering, ASCE, V. 8, No. 3, 1996, pp. 123-127. doi: 10.1061/(ASCE)0899-1561(1996)8:3(123)

18. Cabrera, J. G., “Deterioration of Concrete due to Reinforcement Steel Corrosion,” Cement and Concrete Composites, V. 18, No. 1, 1996, pp. 47-59. doi: 10.1016/0958-9465(95)00043-7

19. Xia, J.; Jin, W.; and Li, L., “Shear Performance of Reinforced Concrete Beams with Corroded Stirrups in Chloride Environment,” Journal of Corrosion Science, V. 53, No. 5, 2011, pp. 1794-1805. doi: 10.1016/j.corsci.2011.01.058

20. Suffern, C.; El-Sayed, A. K.; and Soudki, K., “Shear Strength of Disturbed Regions with Corroded Stirrups in Reinforced Concrete Beams,” Canadian Journal of Civil Engineering, V. 37, No. 8, 2010, pp. 1045-1056. doi: 10.1139/L10-031

21. Higgins, C., and Farrow, W. C., “Tests of Reinforced Concrete Beams with Corrosion Damaged Stirrups,” ACI Structural Journal, V. 103, No. 1, Jan.-Feb. 2006, pp. 133-141.

22. Tastani, S. P., and Pantazopoulou, S. J., “Recovery οf Seismic Resistance in Corrosion-Damaged Reinforced Concrete through FRP Jacketing.” International Journal of Materials and Product Technology, V. 23, No. 3/4, 2005, pp. 389-415.

23. Zsutty, T., “Shear Strength Prediction for Separate Categories of Simple Beam Tests,” ACI Structural Journal, V. 68, No. 2, Mar.-Apr. 1971, pp. 138-143.

24. Zsutty, T., “Beam Shear Strength Prediction by Analysis of Existing Data,” ACI Journal Proceedings, V. 65, No. 11, Nov. 1968, pp. 943-951.

25. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

26. ASTM G1-03(2011), “Standard Practice for Preparing, Cleaning and Evaluating Corrosion Test Specimens,” ASTM International, West Conshohocken, PA, 2011, 9 pp.

27. Khan, I.; François, R.; and Castel, A., “Experimental and Analytical Study of Corroded Shear-Critical Reinforced Concrete Beams,” Materials and Structures Journal, V. 47, No. 9, 2014, pp. 1467-1481. doi: 10.1617/s11527-013-0129-y

28. Vidal, T.; Castel, A.; and François, R., “Analyzing Crack Width to Predict Corrosion in Reinforced Concrete,” Cement and Concrete Research, V. 34, No. 1, 2004, pp. 165-174. doi: 10.1016/S0008-8846(03)00246-1

29. Higgins, C.; Farrow, W. C.; Potisuk, T.; Miller, T. H.; Yim, S. C.; Holocomb, G. R.; Cramer, S. D.; Covino, B. S.; Bullard, S. J.; Ziomek-Moroz, M.; and Matthes, S. A., “Shear Capacity Assessment of Corrosion Damaged Reinforced Concrete Beams,” Final Report SPR 326, Oregon Department of Transportation, Salem, OR, 2003, pp. 62-64.


ALSO AVAILABLE IN:

Electronic Structural Journal