Physical and Chemical Actions of Nano-Mineral Additives on Properties of High-Volume Fly Ash Engineered Cementitious Composites

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Physical and Chemical Actions of Nano-Mineral Additives on Properties of High-Volume Fly Ash Engineered Cementitious Composites

Author(s): Y. Al-Najjar, S. Yesilmen, A. Majeed Al-Dahawi, M. Sahmaran, G. Yıldırım, M. Lachemi, and L. Amleh

Publication: Materials Journal

Volume: 113

Issue: 6

Appears on pages(s): 791-801

Keywords: chloride ion permeability; engineered cementitious composites; high-volume fly ash; hydration characteristics; mechanical properties; nanomineral additives

DOI: 10.14359/51689114

Date: 11/1/2016

Abstract:
Unlike conventional concrete, the material design process for engineered cementitious composites (ECC) involves micromechanics-based design theory, paving the way for the use of high volumes of fly ash (HVFA) as a major component. Using high volumes of fly ash (up to 85% weight fraction of cement) in ECC mixtures enables improved tensile ductility (approximately a 3% increase in long-term tensile strain) with reduced crack widths, although it also leads to significantly reduced early-age compressive and tensile strength and chloride ion resistance. However, nanomineral additives are known to improve mechanical strength and durability of HVFA systems. The study emphasizes the effects of different fly ash (FA)/cement ratios on various properties (hydration and microstructural characteristics, transport and mechanical properties) of ECC mixtures designed with different mineral additives. Experimental results confirm that although different optimum levels can be selected to favor various ECC properties, optimum weight fraction of FA is dependent on the mechanism of nanomodification (that is, type of modifier). The optimum level of fly ash weight fraction that yields the highest rate of improvement through nanomodification of ECC varies for different mechanical and transport properties.

Related References:

1. Li, V. C., “On Engineered Cementitious Composites (ECC),” Advanced Concrete Technology, V. 1, No. 3, 2003, pp. 215-230. doi: 10.3151/jact.1.215

2. Wang, S., and Li, V. C., “Engineered Cementitious Composites with High-Volume Fly Ash,” ACI Materials Journal, V. 104, No. 3, May-June 2007, pp. 233-241.

3. Yang, E. H.; Yang, Y.; and Li, V. C., “Use of High Volumes of Fly Ash to Improve ECC Mechanical Properties and Material Greenness,” ACI Materials Journal, V. 104, No. 6, Nov.-Dec. 2007, pp. 620-628.

4. Poon, C. S.; Lam, L.; and Wong, Y. L., “A Study on High Strength Concrete Prepared with Large Volumes of Low Calcium Fly Ash,” Cement and Concrete Research, V. 30, No. 3, 2000, pp. 447-455. doi: 10.1016/S0008-8846(99)00271-9

5. Hanehara, S.; Tomosawa, F.; Kobayakawa, M.; and Hwang, K., “Effects of Water/Powder Ratio, Mixing Ratio of Fly Ash, and Curing Temperature on Pozzolanic Reaction of Fly Ash in Cement Paste,” Cement and Concrete Research, V. 31, No. 1, 2001, pp. 31-39. doi: 10.1016/S0008-8846(00)00441-5

6. Zhang, Y. M.; Sun, W.; and Yan, H. D., “Hydration of High-Volume Fly Ash Cement Pastes,” Cement and Concrete Composites, V. 22, No. 6, 2000, pp. 445-452. doi: 10.1016/S0958-9465(00)00044-5

7. Zhang, M. H., and Islam, J., “Use of Nano-Silica to Reduce Setting Time and Increase Early Strength of Concretes with High Volumes of Fly Ash or Slag,” Construction and Building Materials, V. 29, 2012, pp. 573-580. doi: 10.1016/j.conbuildmat.2011.11.013

8. Kawashima, S.; Hou, P.; Corr, D. J.; and Shah, S. P., “Modification of Cement-Based Materials with Nanoparticles,” Cement and Concrete Composites, V. 36, 2013, pp. 8-15. doi: 10.1016/j.cemconcomp.2012.06.012

9. Bentz, D. P.; Sato, T.; de la Varga, I.; and Weiss, W. J., “Fine Limestone Additions to Regulate Setting in High Volume Fly Ash Mixtures,” Cement and Concrete Composites, V. 34, No. 1, 2012, pp. 11-17. doi: 10.1016/j.cemconcomp.2011.09.004

10. Sato, T., and Beaudoin, J. J., “Effect of Nano-CaCO3 on Hydration of Cement Containing Supplementary Cementitious Materials,” Advances in Cement Research, V. 23, No. 1, 2011, pp. 33-43. doi: 10.1680/adcr.9.00016

11. De Weerdt, K.; Haha, M. B.; Le Saout, G.; Kjellsen, K. O.; Justnes, H.; and Lothenbach, B., “Hydration Mechanisms of Ternary Portland Cements Containing Limestone Powder and Fly Ash,” Cement and Concrete Research, V. 41, No. 3, 2011, pp. 279-291. doi: 10.1016/j.cemconres.2010.11.014

12. Bentz, D. P., “Activation Energies of High-Volume Fly Ash Ternary Blends: Hydration and Setting,” Cement and Concrete Composites, V. 53, 2014, pp. 214-223. doi: 10.1016/j.cemconcomp.2014.06.018

13. Sato, T., and Diallo, F., “Seeding Effect of Nano-CaCO3 on the Hydration of Tricalcium Silicate,” Transportation Research Record: Journal of the Transportation Research Board, V. 2141, No. 1, 2010, pp. 61-67. doi: 10.3141/2141-11

14. Pera, J.; Husson, S.; and Guilhot, B., “Influence of Finely Ground Limestone on Cement Hydration,” Cement and Concrete Composites, V. 21, No. 2, 1999, pp. 99-105. doi: 10.1016/S0958-9465(98)00020-1

15. Bentz, D. P.; Ardani, A.; Barrett, T.; Jones, S. Z.; Lootens, D.; Peltz, M. A.; Sato, T.; Stutzman, P. E.; Tanesi, J.; and Weiss, W. J., “Multi-Scale Investigation of the Performance of Limestone in Concrete,” Construction and Building Materials, V. 75, 2015, pp. 1-10. doi: 10.1016/j.conbuildmat.2014.10.042

16. Matschei, T.; Lothenbach, B.; and Glasser, F. P., “The Role of Calcium Carbonate in Cement Hydration,” Cement and Concrete Research, V. 37, No. 4, 2007, pp. 551-558. doi: 10.1016/j.cemconres.2006.10.013

17. De Weerdt, K.; Kjellsen, K. O.; Sellevold, E.; and Justnes, H., “Synergy Between Fly Ash and Limestone Powder in Ternary Cements,” Cement and Concrete Composites, V. 33, No. 1, 2011, pp. 31-38. doi: 10.1016/j.cemconcomp.2010.09.006

18. Şahmaran, M.; Al-Emam, M.; Yıldırım, G.; Şimşek, Y. E.; Erdem, T. K.; and Lachemi, M., “High-Early-Strength Ductile Cementitious Composites with Characteristics of Low Early-Age Shrinkage for Repair of Infrastructures,” Materials and Structures, V. 48, No. 5, 2015, pp. 1389-1403. doi: 10.1617/s11527-013-0241-z

19. Kadri, E. H., and Duval, R., “Hydration Heat Kinetics of Concrete with Silica Fume,” Construction and Building Materials, V. 23, No. 11, 2009, pp. 3388-3392. doi: 10.1016/j.conbuildmat.2009.06.008

20. Gündoğdu, D.; Pekmezci, B. Y.; and Atahan, H. N., “Influence of Nanosilica on the Mechanical Properties of Mortars Containing Fly Ash,” International RILEM Conference on Materials Science Additions Improving Properties of Concrete (AdIPoC), 2010, pp. 345-354.

21. Ipavec, A.; Gabrovcek, R.; Vuk, T.; Kaucic, V.; Macek, J.; and Meden, A., “Carboaluminate Phases Formation During the Hydration of Calcite-Containing Portland Cement,” Journal of the American Ceramic Society, V. 94, No. 4, 2011, pp. 1238-1242. doi: 10.1111/j.1551-2916.2010.04201.x

22. Oner, A.; Akyuz, S.; and Yildiz, R., “An Experimental Study on Strength Development of Concrete Containing Fly Ash and Optimum Usage of Fly Ash in Concrete,” Cement and Concrete Research, V. 35, No. 6, 2005, pp. 1165-1171. doi: 10.1016/j.cemconres.2004.09.031

23. Yeşilmen, S.; Al-Najjar, Y.; Balav, M. H.; Şahmaran, M.; Yıldırım, G.; and Lachemi, M., “Nano-Modification to Improve the Ductility of Cementitious Composites,” Cement and Concrete Research, V. 76, 2015, pp. 170-179. doi: 10.1016/j.cemconres.2015.05.026

24. Yang, E. H.; Şahmaran, M.; Yang, Y.; and Li, V. C., “Rheological Control in the Production of Engineered Cementitious Composites,” ACI Materials Journal, V. 104, No. 4, July-Aug. 2009, pp. 257-366.

25. Pesenti, H.; Leoni, M.; and Scardi, P., “XRD Line Profile Analysis of Calcite Powders Produced by High Energy Milling,” Zeitschrift fur Kristallographie, V. 27, No. 27, 2008, pp. 143-150. doi: 10.1524/zksu.2008.0019

26. Suryanarayana, C., “Mechanical Alloying and Milling,” Progress in Materials Science, V. 46, No. 1-2, 2001, pp. 1-184. doi: 10.1016/S0079-6425(99)00010-9

27. Railsback, L. B., “Some Fundamentals of Mineralogy and Geochemistry,” Appendix: Contextual Materials, Carbonate Materials, X-Ray Diffraction (XRD) of Aragonite and Calcite (2006) Internet Document, University of Georgia, Department of Geology, Athens, GA.

28. Balmain, J.; Hannoyer, B.; and Lopez, E., “Fourier Transform Infrared Spectroscopy (FTIR) and X-ray Diffraction Analyses of Mineral and Organic Matrix During Heating of Mother of Pearl (Nacre) from the Shell of the Mollusc Pinctada Maxima,” Journal of Biomedical Materials Research, V. 48, No. 5, 1999, pp. 749-754. doi: 10.1002/(SICI)1097-4636(1999)48:53.0.CO;2-P

29. ASTM C1202-12, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2012, 7 pp.

30. Sakai, E.; Miyahara, S.; Ohsawa, S.; Lee, S. H.; and Daimon, M., “Hydration of Fly Ash Cement,” Cement and Concrete Research, V. 35, No. 6, 2005, pp. 1135-1140. doi: 10.1016/j.cemconres.2004.09.008

31. Lorca, P.; Calabuig, R.; Benlloch, J.; Soriano, L.; and Paya, J., “Microconcrete with Partial Replacement of Portland Cement by Fly Ash and Hydrated Lime Addition,” Materials & Design, V. 64, 2014, pp. 535-541. doi: 10.1016/j.matdes.2014.08.022

32. Papadakis, V. G.; Pedersen, E. J.; and Lindgreen, H., “An AFM-SEM Investigation of the Effect of Silica Fume and Fly Ash on Cement Paste Microstructure,” Journal of Materials Science, V. 34, No. 4, 1999, pp. 683-690. doi: 10.1023/A:1004500324744

33. Ward, C. R., and French, D., “Determination of Glass Content and Estimation of Glass Composition in Fly Ash Using Quantitative X-ray Diffractometry,” Fuel, V. 85, No. 16, 2006, pp. 2268-2227. doi: 10.1016/j.fuel.2005.12.026

34. Ramachandran, V., Concrete Admixtures Handbook: Research Techniques, Standards and Specifications, second edition, William Andrew Publishing, Park Ridge, NJ, 1996, pp. 67-94.

35. Hemmings, R. T., and Berry, E. E., “On the Glass in Coal Fly Ashes: Recent Advances,” Materials Research Society Symposium Proceedings, V. 113, 1987.

36. Li, Y. X.; Chen, Y. M.; Wei, J. X.; He, X. Y.; Zhang, H. T.; and Zhang, W. S., “A Study on the Relationship Between Porosity of the Cement Paste with Mineral Additives and Compressive Strength of Mortar Based on This Paste,” Cement and Concrete Research, V. 36, No. 9, 2006, pp. 1740-1743. doi: 10.1016/j.cemconres.2004.07.007

37. Uchikawa, H.; Hanehara, S.; and Hirao, H., “Influence of Microstructure on the Physical Properties of Concrete Prepared by Substituting Mineral Powder for Part of Fine Aggregate,” Cement and Concrete Research, V. 26, No. 1, 1996, pp. 101-111. doi: 10.1016/0008-8846(95)00193-X

38. Mindess, S., and Young, J., Concrete, Prentice Hall, Englewood Cliffs, NJ, 1981.

39. Şahmaran, M., and Li, V. C., “Durability Properties of Micro-Cracked ECC Containing High Volumes Fly Ash,” Cement and Concrete Research, V. 39, No. 11, 2009, pp. 1033-1043. doi: 10.1016/j.cemconres.2009.07.009

40. Shaikh, F. U. A.; Supit, S. W. M.; and Sarker, P. K., “A Study on the Effect of Nano Silica on Compressive Strength of High Volume Fly Ash Mortars and Concretes,” Materials & Design, V. 60, 2014, pp. 433-442. doi: 10.1016/j.matdes.2014.04.025

41. Tanesi, J.; Bentz, D.; and Ardani, A., “Enhancing High Volume Fly Ash Concretes Using Fine Limestone Powder,” Dallas, TX, 2013.

42. Kayali, O., and Ahmed, M. S., “Assessment of High Volume Replacement Fly Ash Concrete—Concept of Performance Index,” Construction and Building Materials, V. 39, 2013, pp. 71-76. doi: 10.1016/j.conbuildmat.2012.05.009

43. Siddique, R., “Performance Characteristics of High-Volume Class F Fly Ash Concrete,” Cement and Concrete Research, V. 34, No. 3, 2004, pp. 487-493. doi: 10.1016/j.cemconres.2003.09.002

44. De la Varga, I.; Castro, J.; Bentz, D.; and Weiss, J., “Application of Internal Curing for Mixtures Containing High Volumes of Fly Ash,” Cement and Concrete Composites, V. 34, No. 9, 2012, pp. 1001-1008. doi: 10.1016/j.cemconcomp.2012.06.008

45. Mehta, P. K., and Monteiro, P. J., Concrete: Microstructure, Properties and Material, third edition, McGraw Hill, New York, 2006.

46. Zhu, Y.; Zhang, Z.; Yang, Y.; and Yao, Y., “Measurement and Correlation of Ductility and Compressive Strength for Engineered Cementitious Composites (ECC) Produced by Binary and Ternary Systems of Binder Materials: Fly ash, Slag, Silica Fume and Cement,” Construction and Building Materials, V. 68, 2014, pp. 192-198. doi: 10.1016/j.conbuildmat.2014.06.080

47. Bentur, A., “Role of Interfaces in Controlling Durability of Fiber-Reinforced Cements,” Journal of Materials in Civil Engineering, ASCE, V. 12, No. 1, 2000, pp. 2-7. doi: 10.1061/(ASCE)0899-1561(2000)12:1(2)

48. Glavind, M., “Evaluation of the Compressive Behavior of Fiber Reinforced High Strength Concrete,” Technical University of Denmark, Department of Structural Engineering, Lyngby, Denmark, 1992.

49. Wang, S., and Li, V. C., “Polyvinyl Alcohol Fiber Reinforced Engineered Cementitious Composites: Material Design and Performances,” Proceedings of International RILEM Workshop on HPFRCC in Structural Applications, 2006.

50. Chan, Y. W., and Li, V. C., “Age Effect on the Characteristics of Fibre/Cement Interfacial Properties,” Journal of Materials Science, V. 32, No. 19, 1997, pp. 5287-5292. doi: 10.1023/A:1018658626152

51. Xu, A., and Sarkar, S. L., “Microstructural Development in High-Volume Fly-Ash Cement System,” Journal of Materials in Civil Engineering, ASCE, V. 6, No. 1, 1994, pp. 117-136. doi: 10.1061/(ASCE)0899-1561(1994)6:1(117)

52. Escalante-Garcia, J. I., and Sharp, J. H., “The Chemical Composition and Microstructure of Hydration Products in Blended Cements,” Cement and Concrete Composites, V. 26, No. 8, 2004, pp. 967-976. doi: 10.1016/j.cemconcomp.2004.02.036

53. Helmuth, R. A.; Whiting, D. A.; Dubovoy, V. S.; Tang, F. J.; and Love, H., “Performance of Blended Cements Made with Controlled Particle Size Distributions,” ASTM Special Technical Publication, V. 897, 1986, pp. 106-127.


ALSO AVAILABLE IN: