371R-16 Guide for Analysis, Design, & Construction of Elevated Concrete & Composite Steel-Concrete Water Storage Tanks

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 371R-16 Guide for Analysis, Design, & Construction of Elevated Concrete & Composite Steel-Concrete Water Storage Tanks

Author(s): ACI Committee 371

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 41

Keywords: composite tanks; concrete-pedestal tanks; earthquake-resistant structures; elevated water tanks; formwork (construction).

DOI:

Date: 6/21/2016

Abstract:

This guide presents recommendations for materials, analysis, design, and construction of concrete-pedestal elevated water storage tanks, including all-concrete and composite tanks. Composite tanks consist of a steel water storage vessel supported on a cylindrical reinforced concrete pedestal.

Concrete-pedestal elevated water storage tanks are structures that present special problems not encountered in typical environmental engineering concrete structures. This guide refers to ACI 350 for design and construction of those components of the pedestal tank in contact with the stored water, and to ACI 318 for design and construction of components not in contact with the stored water. Determination of snow, wind, and seismic loads based on ASCE/SEI 7 is included. These loads conform to the requirements of national building codes that use ASCE/SEI 7 as the basis for environmental loads as well as those of local building codes. Special requirements, based on successful experience, for the unique aspects of loads, analysis, design, and construction of concrete-pedestal tanks are presented.