Phase equilibria in the system Ca4Al6O12SO4 – Ca2SiO4 – CaSO4 – H2O referring to the hydration of calcium sulfoaluminate cements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Phase equilibria in the system Ca4Al6O12SO4 – Ca2SiO4 – CaSO4 – H2O referring to the hydration of calcium sulfoaluminate cements

Author(s): Frank Winnefeld; Barbara Lothenbach

Publication: RILEM

Volume: 1

Issue:

Appears on pages(s): 10-16

Keywords: Calcium sulfoaluminate cement; Hydration; Thermodynamic modelling; Phase diagram

DOI:

Date: 4/18/2016

Abstract:
This paper presents thermodynamic calculations of the stable hydrate assemblages in calcium sulfoaluminate cements containing different amounts of ye’elemite, calcium sulfate and belite. The ternary diagrams developed in this paper can be used directly to assess the long-term composition of such calcium sulfoaluminate cements containing belite. The phase diagram was validated using experimental data from literature. The ternary diagrams developed can be used to read out directly the stable hydrate assemblage of calcium sulfoaluminate cements containing belite based on their initial composition.


International union of laboratories and experts in construction materials, systems and structures, International Partner Access