Title: Shear-Transfer Mechanisms for Glass Fiber-Reinforced Polymer Reinforcing Bars

Author(s): Austin B. Connor and Young Hoon Kim

Publication: Structural Journal

Volume: 113

Issue: 6

Appears on pages(s): 1369-1380

Keywords: aggregate interlock; angle effect; composite reinforcement; glass fiber-reinforced polymer; shear-friction

DOI: 10.14359/51689034

Date: 11/1/2016

Abstract:
This paper proposes a shear-friction model for sand-coated glass fiber-reinforced polymer (GFRP) reinforcement. The proposed shear-friction model considers crack parameters, width, and slip, as well as the orientation angle of the reinforcing bar crossing the crack plane. A total of nine push-off tests were conducted to investigate the shear performance of two contributions: aggregate interlock and reinforcement. Main test variables include two types of reinforcement (steel and GFRP) and three different orientations (45, 90, and 135 degrees). Results indicate that width and slip along with the orientation of GFRP are critical design parameters to accurately quantify shear capacity provided by contributing mechanisms. Therefore, the performance of GFRP can be quantified as a function of crack parameters, which are larger in fiber-reinforced polymer (FRP)-reinforced systems. The proposed framework outlines the approach to develop a model to predict shear-transfer strength of FRP-reinforced concrete.

Related References:

AASHTO, 2012, “LRFD Bridge Design Specifications,” American Association of Highway and Transportation Officials, Washington, DC, 1661 pp.

ACI Committee 318, 1977, “Building Code Requirements for Reinforced Concrete (ACI 318-77),” American Concrete Institute, Farmington Hills, MI, 103 pp.

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 519 pp.

ACI Committee 440, 2015, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 85 pp.

Al-Sunna, R.; Pilakoutas, K.; Hajirasouliha, I.; and Guadagnini, M., 2012, “Deflection Behaviour of FRP Reinforced Concrete Beams and Slabs: An Experimental Investigation,” Composites. Part B, Engineering, V. 43, No. 5, pp. 2125-2134. doi: 10.1016/j.compositesb.2012.03.007

ASTM A370-13, 2013, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products,” ASTM International, West Conshohocken, PA, 48 pp.

ASTM D7205/D7205M-06(2011), 2011, “Standard Test Method for Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA, 13 pp.

Bentz, E.; Massam, L.; and Collins, M., 2010, “Shear Strength of Large Concrete Members with FRP Reinforcement,” Journal of Composites for Construction, ASCE, V. 14, No. 6, pp. 637-646. doi: 10.1061/(ASCE)CC.1943-5614.0000108

Birkeland, P. W., and Birkeland, H. W., 1966, “Connections in Precast Concrete Construction,” ACI Journal Proceedings, V. 63, No. 3, Mar., pp. 345-368.

Collins, M. P., and Mitchell, D., 1991, Prestressed Concrete Structures, Prentice Hall, Englewood Cliffs, NJ, 766 pp.

El-Sayed, A.; El-Salakawy, E.; and Benmokrane, B., 2005, “Shear Strength of One-Way Concrete Slabs Reinforced with Fiber-Reinforced Polymer Composite Bars,” Journal of Composites for Construction, ASCE, V. 9, No. 2, pp. 147-157. doi: 10.1061/(ASCE)1090-0268(2005)9:2(147)

El-Sayed, A. K., and Soudki, K., 2011, “Evaluation of Shear Design Equations of Concrete Beams with FRP Reinforcement,” Journal of Composites for Construction, ASCE, V. 15, No. 1, pp. 9-20. doi: 10.1061/(ASCE)CC.1943-5614.0000158

Elkady, M.; Tadros, M. K.; Lafferty, M.; Morcous, G.; and Gremel, D., 2015, “Precast Concrete Corbels for Insulated Wall Panels,” Concrete International, V. 37, No. 10, Oct., pp. 45-50.

Hanson, N. W., 1960, Precast-Prestressed Concrete Bridges: 2. Horizontal Shear Connections, Portland Cement Association, Skokie, IL, 25 pp.

Harries, K. A.; Zeno, G.; Shahrooz, B.; and Mattock, A. H., 2012, “Toward an Improved Understanding of Shear-Friction Behavior,” ACI Structural Journal, V. 109, No. 6, Nov.-Dec., pp. 835-844.

Hofbeck, J.; Ibrahim, I.; and Mattock, A. H., 1969, “Shear Transfer in Reinforced Concrete,” ACI Journal Proceedings, V. 66, No. 2, Feb., pp. 119-128.

Hyer, M. W., 2009, Stress Analysis of Fiber-Reinforced Composite Materials, DEStech Publications, Inc., Lancaster, PA, 710 pp.

Keller, T., 2001, “Recent All-Composite and Hybrid Fibre-Reinforced Polymer Bridges and Buildings,” Progress in Structural Engineering and Materials, V. 3, No. 2, pp. 132-140. doi: 10.1002/pse.66

Kim, Y. H.; Hueste, M. B. D.; Trejo, D.; and Cline, D. B. H., 2010, “Shear Characteristics and Design for High-Strength Self-Consolidating Concrete,” Journal of Structural Engineering, ASCE, V. 136, No. 8, pp. 989-1000. doi: 10.1061/(ASCE)ST.1943-541X.0000194

Loov, R. E., and Patnaik, A. K., 1994, “Horizontal Shear Strength of Composite Concrete Beams with a Rough Interface,” PCI Journal, V. 39, No. 1, pp. 48-69. doi: 10.15554/pcij.01011994.48.69

Lucas, W.; Oehlers, D. J.; Mohamed Ali, M. S.; and Griffith, M., 2012, “The FRP Reinforced Shear-Friction Mechanism,” Advances in Structural Engineering, V. 15, No. 4, pp. 615-624. doi: 10.1260/1369-4332.15.4.615

Mast, R., 1968, “Auxillary Reinforcement in Concrete Connections,” Journal of the Structural Division, ASCE, V. 94, No. 6, pp. 1485-1504.

Mattock, A., 1974, “Shear Transfer in Concrete having Reinforcement at an Angle to the Shear Plane,” Shear in Reinforced Concrete, SP-42, American Concrete Institute, Farmington Hills, MI, pp. 14-42.

Mattock, A., 2001, “Shear Friction and High-Strength Concrete,” ACI Structural Journal, V. 98, No. 1, Jan.-Feb., pp. 50-59.

Mattock, A. H., 2013, “Toward an Improved Understanding of Shear-Friction Behavior—Discussion,” ACI Structural Journal, V. 110, No. 5, Sept.-Oct., pp. 890-891.

Mattock, A. H.; Chen, K.; and Soongswang, K., 1976a, “The Behavior of Reinforced Concrete Corbels,” PCI Journal, V. 21, No. 2, pp. 52-77. doi: 10.15554/pcij.03011976.52.77

Mattock, A. H., and Hawkins, N. M., 1972, “Shear Transfer in Reinforced Concrete,” PCI Journal, V. 17, No. 2, pp. 55-75. doi: 10.15554/pcij.03011972.55.75

Mattock, A. H.; Johal, L.; and Chow, H., 1975, “Shear Transfer in Reinforced Concrete with Moment or Tension Acting Across the Shear Plane,” PCI Journal, V. 20, No. 4, pp. 76-93. doi: 10.15554/pcij.07011975.76.93

Mattock, A. H.; Li, W.; and Wang, T., 1976b, “Shear Transfer in Lightweight Reinforced Concrete,” PCI Journal, V. 21, No. 1, pp. 20-39. doi: 10.15554/pcij.01011976.20.39

Mohamed Ali, M. S.; Oehlers, D. J.; Griffith, M. C.; and Seracino, R., 2008, “Interfacial Stress Transfer of Near Surface-Mounted FRP-to-Concrete Joints,” Engineering Structures, V. 30, No. 7, pp. 1861-1868. doi: 10.1016/j.engstruct.2007.12.006

Nanni, A., 1993, “Flexural Behavior and Design of RC Members Using FRP Reinforcement,” Journal of Structural Engineering, ASCE, V. 119, No. 11, pp. 3344-3359. doi: 10.1061/(ASCE)0733-9445(1993)119:11(3344)

Oehlers, D. J.; Liu, I. S. T.; Seracino, R.; and Mohamed Ali, M. S., 2004, “Prestress Model for Shear Deformation Debonding of FRP- and Steel-Plated RC Beams,” Magazine of Concrete Research, V. 56, No. 8, pp. 475-486. doi: 10.1680/macr.2004.56.8.475

Oehlers, D. J.; Muhamad, R.; and Mohamed Ali, M. S., 2013, “Serviceability Flexural Ductility of FRP RC Beams: A Discrete Rotation Approach,” Construction and Building Materials, V. 49, pp. 974-984. doi: 10.1016/j.conbuildmat.2012.10.001

Park, R., and Paulay, T., 1975, Reinforced Concrete Structures, John Wiley & Sons, Inc., New York, 769 pp.

Razaqpur, A., and Spadea, S., 2014, “Shear Strength of FRP Reinforced Concrete Members with Stirrups,” Journal of Composites for Construction, ASCE, V. 19, No. 1, pp. 1-15.

Reinhardt, H. W., and Walraven, J. C., 1982, “Cracks in Concrete Subject to Shear,” Journal of the Structural Division, ASCE, V. 108, No. 1, pp. 207-224.

Sneed, L. H., and Ramirez, J. A., 2014, “Influence of Cracking on Behavior and Shear Strength of Reinforced Concrete Beams,” ACI Structural Journal, V. 111, No. 1, Jan.-Feb., pp. 157-166.

Walraven, J., 1981, “Fundamental Analysis of Aggregate Interlock,” Journal of the Structural Division, ASCE, V. 107, No. 11, pp. 2245-2270.

Walraven, J.; Frenay, J.; and Pruijssers, A., 1987, “Influence of Concrete Strength and Load History on the Shear Friction Capacity of Concrete Members,” PCI Journal, V. 32, No. 1, pp. 66-84. doi: 10.15554/pcij.01011987.66.84

Walraven, J. C., and Reinhardt, H. W., 1981, “Theory and Experiments on the Mechanical Behaviour of Cracks in Plain and Reinforced Concrete Subjected to Shear Loading,” Heron, V. 26, pp. 1-68.

Wight, J. K., and MacGregor, J. G., 2011, Reinforced Concrete: Mechanics and Design, Pearson Education, Upper Saddle River, NJ, 1157 pp.